| COMBUSTION REACTION OF Ni_(20)Ti_(50)C_(30) DURING MECHANICAL ALLOYING |
| YE Lilei; HUANG Jianyu; LIU Zhiguang; QUAN Mingxiu(State Key Laboratory of RSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015) (Manuscript received 1995-06-13; in revised form 1995-09-26) |
|
Cite this article:
YE Lilei; HUANG Jianyu; LIU Zhiguang; QUAN Mingxiu(State Key Laboratory of RSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015) (Manuscript received 1995-06-13; in revised form 1995-09-26). COMBUSTION REACTION OF Ni_(20)Ti_(50)C_(30) DURING MECHANICAL ALLOYING. Acta Metall Sin, 1996, 32(4): 429-432.
|
|
|
Abstract The combustion reaction was observed during mechanical alloying Ni_(20)Ti_(50)C_(30), and the agglomerates and powders coexisted in final product. With the analysis of X-ray diffraction (XRD) and the observation of scanning electron microscope (SEM), it is indicated that melting occurred in the combustion reaction. The product is composed of TiC phase and NiTi compound. It is regarded that the initial TiC is produced by the heavy collision of balls during milling, and then the large heat released from the TiC formation induces the latter reactions. Correspondent: YE Lilei,(Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110015)
|
|
Received: 18 April 1996
|
| 1MaE,PaganJ,CranfordG,AtzmonM.JMaterRes,1993;8:18362WangKY,HeAQ,WangJT.MetallTrans,1993;24A:2253KruegerBR,MutzAH,VreelandTJr.MetallTrans,1992;23A:554ZhangS.MunirZA.JMaterSci,1991;26:36855YeLL,LiuZG,HuangJY,QuanMX.MaterLett,1995;25:1176AtzmonM.PhysRevLett,1990;64:4877SmithellsCJ.MetalsReferenceBook,5thed.,London:Butterworth,1976:3268MunirZA.CeramBull,1988:67:342F |