COMPUTER MODEL OF DISTRIBUTION BEHAVIOR OF ACCESSORY ELEMENTS IN COPPER SMELTING
TAN Pengfu;ZHANG Chuanfu(Central South University of Technology; Changsha 410083)
Cite this article: 

TAN Pengfu;ZHANG Chuanfu(Central South University of Technology; Changsha 410083). COMPUTER MODEL OF DISTRIBUTION BEHAVIOR OF ACCESSORY ELEMENTS IN COPPER SMELTING. Acta Metall Sin, 1997, 33(10): 1094-1100.

Download:  PDF(521KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By using computer-aided techniques of equilibrium calculations for multicomponent and multiphase systems, a computer model has been developed to simulate distribution behavior of Ni, Co, Sn, Pb, Zn, as, Sb,Bi, au and ag in copper smelting. The predicted results by the present computer model are compared with the known commerical data from Gui Xi Smelter in China and Horne Smelter in Canada. The agreements between the computer prediction and the commercial data are excellent, so that the present computer model can be used to monitor and optimize the actual industrial operations of copper smelting and control the distribution behavior of accessory elements in copper smelting.
Key words:  copper      smelting      accessory element      computer model     
Received:  18 October 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I10/1094

1 Itagaki K, Yazawa a. In:Sohn H Y, ed., advances in Sulfide Smelting. Utah: americal Institute ofMining, Metallurgical and Petroleum Engineers, 1983:119
2 Chaubal P C. MetalI Trans, 1989; 20B(12):39
3 Shimpo R, Ogawa O, Goto S. Metall Trans, 1993, 24a(8):1882
4 Shimpo R, Watanabe Y, Goto S. In. Sohn H Y, ed., advances in Sulfide Smelting. Utah:americalInstitute of Mining, Metallurgical and Petroleum Engineers, 1983; 295
5 Nagamori N, Mackey P J. Metall Trans, 1978; 9B:567
6 Nagamori M, Errington W J, Mackey P J. MetalI Trans. 1994; 25B(12):839
7 Seo K W, Sohn H Y. Metall Trans. 1991; 22B(12):791
8 Yazawa a, Nakazawa S, Takeda Y. In:Sohn H Y, ed., advances in Sulfide Smelting. Utah:americal Institute of Mining, Metallurgical and Petroleum Engineers, 1983; 90
9 Sinha S N, Nagamori M. Metall Trans. 1982, 13B(9). 461
10 Sinha S N, Sohn H Y, Nagamori M. Metall Trans. 1984; 15B(9):595
11 Sinha S N, Sohn H Y, Nagamori M. Metall Trans. 1985; 16B(31):53
12 Takeda Y, Ishinata S, Yazawa a. Trans Jpn Inst Met, 1983; 24(7):518
13 Mackey P J. Can Metall Q, 1982, 21(3). 221
14 Grimsey E J, Liu X L. Metall Trans, 1995; 26B(4): 229
15 Jalkanen H K, Holppa L E K.In:Sohn H Y,ed,advances in Sulfide Smelting.Utah: americal Institute of Mining,Metallurgical and Petroleum Engineers,1983:277
16Nagamori M, Mackey P J. Metall Trans, 1978; 9B(6): 255
17王震华,有色冶金设计与研究.1993;14(4):18
[1] CHEN Kaixuan, LI Zongxuan, WANG Zidong, Demange Gilles, CHEN Xiaohua, ZHANG Jiawei, WU Xuehua, Zapolsky Helena. Morphological Evolution of Fe-Rich Precipitates in a Cu-2.0Fe Alloy During Isothermal Treatment[J]. 金属学报, 2023, 59(12): 1665-1674.
[2] ZHAO Naiqin, GUO Siyuan, ZHANG Xiang, HE Chunnian, SHI Chunsheng. Progress on Graphene/Copper Composites Focusing on Reinforcement Configuration Design: A Review[J]. 金属学报, 2021, 57(9): 1087-1106.
[3] PENG Wuqingliang, LI Qiang, CHANG Yongqin, WANG Wanjing, CHEN Zhen, XIE Chunyi, WANG Jichao, GENG Xiang, HUANG Lingming, ZHOU Haishan, LUO Guangnan. A Review on the Development of the Heat Sink of the Fusion Reactor Divertor[J]. 金属学报, 2021, 57(7): 831-844.
[4] HUANG Songpeng, PENG Can, CAO Gongwang, WANG Zhenyao. Corrosion Behavior of Copper-Nickel Alloys Protected by BTA in Simulated Urban Atmosphere[J]. 金属学报, 2021, 57(3): 317-326.
[5] ZHANG Yong, LI Xinxu, WEI Kang, WEI Jianhuan, WANG Tao, JIA Chonglin, LI Zhao, MA Zongqing. Element Segregation in GH4169 Superalloy Large-Scale Ingot and Billet Manufactured by Triple-Melting[J]. 金属学报, 2020, 56(8): 1123-1132.
[6] Jianqiang REN, Shuhua LIANG, Yihui JIANG, Xiang DU. Research on the Microstructure and Properties of In Situ (TiB2-TiB)/Cu Composites[J]. 金属学报, 2019, 55(1): 126-132.
[7] Pengyue ZHAO, Yongbo GUO, Qingshun BAI, Feihu ZHANG. Research of Surface Defects of Polycrystalline Copper Nanoindentation Based on Microstructures[J]. 金属学报, 2018, 54(7): 1051-1058.
[8] Tingting ZHAO, Zhixin KANG, Xiayu MA. Fabricating Superhydrophobic Copper Meshes by One-Step Electrodeposition Method and Its Anti-Corrosion and Oil-Water Separation Abilities[J]. 金属学报, 2018, 54(1): 109-117.
[9] Tingbiao GUO, Qi LI, Chen WANG, Feng ZHANG, Zhi JIA. Deformation Characteristics and Mechanical Properties of Single Crystal Copper During Equal Channel Angular Pressing by Route A[J]. 金属学报, 2017, 53(8): 991-1000.
[10] Wei FU,Xiaoguo SONG,Long LONG,Jianhang CHAI,Jicai FENG,Guodong WANG. INTERFACIAL MICROSTRUCTURE AND MECHANI-CAL PROPERTIES OF INDIRECT BRAZED GRAPHITE/COPPER JOINT[J]. 金属学报, 2016, 52(6): 734-740.
[11] Zhisheng WANG, Xiang CHEN, Yanxiang LI, Huawei ZHANG, Yuan LIU. EFFECTS OF B ON HIGH TEMPERATURE MECHA-NICAL PROPERTIES AND THERMAL FATIGUE BEHAVIOR OF COPPER DIE-CASTING DIE STEEL[J]. 金属学报, 2015, 51(5): 519-526.
[12] ZHUO Weijia, LIU Yuan, LI Yanxiang. EFFECT OF WITHDRAWING RATE ON PORE MORPHOLOGY OF LOTUS-TYPE POROUS COPPER PRODUCED BY SINGLE-MOLD GASAR TECHNIQUE[J]. 金属学报, 2014, 50(8): 921-929.
[13] JIANG Yanbin, LIU Xinhua, WANG Chunyang, MO Yongda, XIE Jianxin. INFLUENCE OF INDUCTION HEATING CONTINUOUS ANNEALING ON RECRYSTALLIZATION AND INTER- FACIAL INTERMETALLIC COMPOUND OF COPPER-CLAD ALUMINUM WIRE[J]. 金属学报, 2014, 50(4): 479-488.
[14] WANG Changgang, DONG Junhua, KE Wei, LI Xiaofang. INVESTIGATION ON PITTING CORROSION BEHAVIOR OF COPPER IN THE MIXED SOLUTION OF HCO3-, SO42- AND Cl-[J]. 金属学报, 2013, 49(2): 207-213.
[15] SUN Feilong, LI Xiaogang, LU Lin, WAN Hongxia, DU Cuiwei, LIU Zhiyong. CORROSION BEHAVIOR OF COPPER ALLOYS IN DEEP OCEAN ENVIRONMENT OF SOUTH CHINA SEA[J]. 金属学报, 2013, 49(10): 1211-1218.
No Suggested Reading articles found!