Fabricating Superhydrophobic Copper Meshes by One-Step Electrodeposition Method and Its Anti-Corrosion and Oil-Water Separation Abilities
Tingting ZHAO, Zhixin KANG(), Xiayu MA
Guangdong Key Laboratory for Advanced Metallic Materials Processing, National Engineering Research Center of Near-Net-Shape Forming for Metallic Materials, School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou 510640, China
Cite this article:
Tingting ZHAO, Zhixin KANG, Xiayu MA. Fabricating Superhydrophobic Copper Meshes by One-Step Electrodeposition Method and Its Anti-Corrosion and Oil-Water Separation Abilities. Acta Metall Sin, 2018, 54(1): 109-117.
Special wettability includes superhydrophobic, superhydrophilic, superoleophobic and superoleophilic etc. The superhydrophobic surfaces are governed by the surface chemistry and unique micro/nanostructures. Up to now, numerous methods have been reported in constructing superhydrophobic surfaces including chemical vapor deposition, chemical etching, hydrothermal, sol-gel and so on. Preparing superhydrophobic films on metal surfaces is an effective way to improve the anti-corrosion property of metal substrates. In addition, superhydrophobic films can be used to oil-water separation. In this work, a one-step electrodeposition was applied to prepare superhydrophobic surfaces on copper meshes. The morphology, wettability and chemical composition of the prepared films were characterized by SEM, optical contact angle meter, EDS, FTIR and XPS. The results showed that the surface on copper meshes obtained at 30 V with 10 min was uniformly covered by microcells aggregated by nanosheets. The surfaces of the copper meshes were composed of copper myristate (Cu[CH3(CH2)12COO]2) and reach the maximum contact angle of 156.2° with the rolling angle as low as 1°. The potentiodynamic polarization curves were utilized to analyze the corrosion resistance, which demonstrated that corrosion current densities of the superhydrophobic film was 4.77×10-9 A/cm2, decreased by more than 3 orders of magnitude, and the corrosion potential was 0.036 V more positive compared with the copper substrate. Moreover,the oil-water separation tests showed that the separation efficiency of the film after reused for 5 times maintained above 95%, exhibiting excellent oil-water property and recycle capability.
Fund: Supported by Natural Science Foundation of Guangdong Province (No.2015A030313219) and Science and Technology Research Program of Guangzhou (No.201510010155)
Fig.1 Schematic of the fabrication of a superhydrophobic film on Cu meshes
Fig.2 Low (a~e) and high (f~j) magnified surface SEM images of the as-prepared films obtained with different electrodeposition time at 30 V (a, f) 1 min (b, g) 4 min (c, h) 7 min (d, i) 10 min (e, j) 15 min
Fig.3 Water contact angles and sliding angles of the as-prepared films obtained with different electrodeposition time at 30 V
Fig.4 Low (a~e) and high (f~j) magnified surface SEM images of the films obtained at different electrodeposition voltages for 10 min (a, f) 10 V (b, g) 20 V (c, h) 30 V (d, i) 40 V (e, j) 50 V
Fig.5 Water conatact angles and sliding angles of the as-prepared films obtained azat different electrodeposition voltages for 10 min
Fig.6 Images of water contact angle (a) and slide angle (b) at 30 V for 10 min
Fig.7 EDS of the superhydrophobic film
Fig.8 FTIR spectra of the superhydrophobic film and myristic acid
Fig.9 XPS survey spectrum (a), C1s (b) and O1s (c) of the superhydrophobic flim at 30 V for 10 min
Fig.10 Schematic of the electrodeposition principle
Fig.11 Potentiodynamic polarization curves of the Cu mesh and the superhydrophobic film in 3.5%NaCl solution (icorr — corrosion current density)
Fig.12 Photographs before (a) and after (b) the oilwater separation process
[1]
Liu Y, Zhang K T, Yao W G, et al.A facile electrodeposition process for the fabrication of superhydrophobic and superoleophilic copper mesh for efficient oil-water separation[J]. Ind. Eng. Chem. Res., 2016, 55: 2704
[2]
Neinhuis C, Barthlott W.Characterization and distribution of water-repellent, self-cleaning plant surfaces[J]. Ann. Bot., 1997, 79: 667
[3]
Barthlott W, Neinhuis C.Purity of the sacred lotus, or escape from contamination in biological surfaces[J]. Planta, 1997, 202: 1
[4]
Liu Q, Chen D X, Kang Z X.One-step electrodeposition process to fabricate corrosion-resistant superhydrophobic surface on magnesium alloy[J]. ACS Appl. Mater. Interfaces, 2015, 7: 1859
[5]
Kang Z X, Guo M J.Fabrication of superhydrophobic Ti surface by thermal oxidation and its anticorrosion property[J]. Acta Metall. Sin., 2013, 49: 629(康志新, 郭明杰. 热氧化法制备超疏水Ti表面及其耐腐蚀性[J]. 金属学报, 2013, 49: 629)
[6]
Liu C S, Su F H, Liang J Z, et al.Facile fabrication of superhydrophobic cerium coating with micro-nano flower-like structure and excellent corrosion resistance[J]. Surf. Coat. Technol., 2014, 258: 580
[7]
Wenzel R N.Resistance of solid surfaces to wetting by water[J]. Ind. Eng. Chem., 1936, 28: 988
[8]
Yan L, Li J, Li W J, et al.A photo-induced ZnO coated mesh for on-demand oil/water separation based on switchable wettability[J]. Mater. Lett., 2016, 163: 247
[9]
Luo Z Y, Chen K X, Wang J H, et al.Hierarchical nanoparticle-induced superhydrophilic and under-water superoleophobic Cu foam with ultrahigh water permeability for effective oil/water separation[J]. J. Mater. Chem., 2016, 4A: 10566
[10]
Wang F J, Lei S, Xu Y, et al.Green approach to the fabrication of superhydrophobic mesh surface for oil/water separation[J]. ChemPhysChem, 2015, 16: 2237
[11]
Kong L H, Chen X H, Yu L G, et al.Superhydrophobic cuprous oxide nanostructures on phosphor-copper meshes and their oil-water separation and oil spill cleanup[J]. ACS Appl. Mater. Interfaces, 2015, 7: 2616
[12]
Shinde S L, Nanda K K.Facile synthesis of large area porous Cu2O as super hydrophobic yellow-red phosphors[J]. RSC Adv., 2012, 2: 3647
[13]
Yin S H, Wu D X, Yang J, et al.Fabrication and surface characterization of biomimic superhydrophobic copper surface by solution-immersion and self-assembly[J]. Appl. Surf. Sci., 2011, 257: 8481
[14]
Fan Y H, Chen Z J, Liang J, et al.Preparation of superhydrophobic films on copper substrate for corrosion protection[J]. Surf. Coat. Technol., 2014, 244: 1
[15]
Ou J F, Hu W H, Liu S, et al.Superoleophobic textured copper surfaces fabricated by chemical etching/oxidation and surface fluorination[J]. ACS Appl. Mater. Interfaces, 2013, 5: 10035
[16]
Qing Y Q, Yang C N, Zhao Q Q, et al.Simple fabrication of superhydrophobic/superoleophobic surfaces on copper substrate by two-step method[J]. J. Alloys Compd., 2017, 695: 1878
[17]
Lv Y.Electrodeposited patterning organic luminescent films and their applications for display devices [D]. Changchun: Jilin University, 2013(吕营. 电沉积图案化有机发光薄膜及其在显示器件中的应用 [D]. 长春: 吉林大学, 2013)
[18]
Hong B.Study on texture and internal stress of electrodeposited copper film [D]. Shanghai: Shanghai Jiao Tong University, 2008(洪波. 电沉积铜薄膜中织构与内应力的研究 [D]. 上海: 上海交通大学, 2008)
[19]
She Z X, Li Q, Wang Z W, et al.Highly anticorrosion, selfcleaning superhydrophobic Ni- Co surface fabricated on AZ91D magnesium alloy[J]. Surf. Coat. Technol., 2014, 251: 7
[20]
Zhang X F, Chen R J, Hu J M.Superhydrophobic surface constructed on electrodeposited silica films by two-step method for corrosion protection of mild steel[J]. Corros. Sci., 2016, 104: 336
[21]
Chen Z, Hao L M, Chen C L.A fast electrodeposition method for fabrication of lanthanum superhydrophobic surface with hierarchical micro-nanostructures[J]. Colloids Surf., 2012, 401A: 1
[22]
Xi J M, Feng L, Jiang L.A general approach for fabrication of superhydrophobic and superamphiphobic surfaces[J]. Appl. Phys. Lett., 2008, 92: 053102
[23]
Cassie A B D, Baxter S. Wettability of porous surfaces[J]. Trans. Faraday. Soc., 1944, 40: 546
[24]
Chen Z, Hao L M, Chen C L.Simultaneous fabrication of superhydrophobic coatings on cathodic and anodic copper surfaces with Micro/nano- structures[J]. ECS Electrochem. Lett., 2012, 1: D21
[25]
Wang S, Feng L, Jiang L.One-step solution-immersion process for the fabrication of stable bionic superhydrophobic surfaces[J]. Adv. Mater., 2006, 18: 767
[26]
Zhao T T, Kang Z X.Simultaneously fabricating multifunctional superhydrophobic/superoleophilic coatings by one-step electrodeposition method on cathodic and anodic magnesium surfaces[J]. J. Electrochem. Soc., 2016, 163: D628
[27]
Chen Z, Hao L M, Chen A Q, et al.A rapid one-step process for fabrication of superhydrophobic surface by electrodeposition method[J]. Electrochim. Acta, 2012, 59: 168
[28]
Crick C R, Gibbins J A, Parkin I P.Superhydrophobic polymer-coated copper-mesh; membranes for highly efficient oil-water separation[J]. J. Mater. Chem., 2013, 1A: 5943