| COMPUTER MODEL OF DISTRIBUTION BEHAVIOR OF ACCESSORY ELEMENTS IN COPPER SMELTING |
| TAN Pengfu;ZHANG Chuanfu(Central South University of Technology; Changsha 410083) |
|
Cite this article:
TAN Pengfu;ZHANG Chuanfu(Central South University of Technology; Changsha 410083). COMPUTER MODEL OF DISTRIBUTION BEHAVIOR OF ACCESSORY ELEMENTS IN COPPER SMELTING. Acta Metall Sin, 1997, 33(10): 1094-1100.
|
|
|
Abstract By using computer-aided techniques of equilibrium calculations for multicomponent and multiphase systems, a computer model has been developed to simulate distribution behavior of Ni, Co, Sn, Pb, Zn, as, Sb,Bi, au and ag in copper smelting. The predicted results by the present computer model are compared with the known commerical data from Gui Xi Smelter in China and Horne Smelter in Canada. The agreements between the computer prediction and the commercial data are excellent, so that the present computer model can be used to monitor and optimize the actual industrial operations of copper smelting and control the distribution behavior of accessory elements in copper smelting.
|
|
Received: 18 October 1997
|
1 Itagaki K, Yazawa a. In:Sohn H Y, ed., advances in Sulfide Smelting. Utah: americal Institute ofMining, Metallurgical and Petroleum Engineers, 1983:119 2 Chaubal P C. MetalI Trans, 1989; 20B(12):39 3 Shimpo R, Ogawa O, Goto S. Metall Trans, 1993, 24a(8):1882 4 Shimpo R, Watanabe Y, Goto S. In. Sohn H Y, ed., advances in Sulfide Smelting. Utah:americalInstitute of Mining, Metallurgical and Petroleum Engineers, 1983; 295 5 Nagamori N, Mackey P J. Metall Trans, 1978; 9B:567 6 Nagamori M, Errington W J, Mackey P J. MetalI Trans. 1994; 25B(12):839 7 Seo K W, Sohn H Y. Metall Trans. 1991; 22B(12):791 8 Yazawa a, Nakazawa S, Takeda Y. In:Sohn H Y, ed., advances in Sulfide Smelting. Utah:americal Institute of Mining, Metallurgical and Petroleum Engineers, 1983; 90 9 Sinha S N, Nagamori M. Metall Trans. 1982, 13B(9). 461 10 Sinha S N, Sohn H Y, Nagamori M. Metall Trans. 1984; 15B(9):595 11 Sinha S N, Sohn H Y, Nagamori M. Metall Trans. 1985; 16B(31):53 12 Takeda Y, Ishinata S, Yazawa a. Trans Jpn Inst Met, 1983; 24(7):518 13 Mackey P J. Can Metall Q, 1982, 21(3). 221 14 Grimsey E J, Liu X L. Metall Trans, 1995; 26B(4): 229 15 Jalkanen H K, Holppa L E K.In:Sohn H Y,ed,advances in Sulfide Smelting.Utah: americal Institute of Mining,Metallurgical and Petroleum Engineers,1983:277 16Nagamori M, Mackey P J. Metall Trans, 1978; 9B(6): 255 17王震华,有色冶金设计与研究.1993;14(4):18 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|