Please wait a minute...
Acta Metall Sin  1997, Vol. 33 Issue (10): 1085-1093    DOI:
Current Issue | Archive | Adv Search |
HIGH ORDER SUB-REGULAR SOLUTION MODEL AND ITS APPLICATIONS IN THE CALCULATION OF COMPONENT ACTIVITIES OF MnO-SiO_2-Al_2O_3-CaO MOLTEN SLAG
ZHANG Xiaobing;JIANG Guochang;XU Kuangdi (Shanghai University; ShanghaiEnhanced Lab of Ferrometallurgy; Shanghai 200072)
Cite this article: 

ZHANG Xiaobing;JIANG Guochang;XU Kuangdi (Shanghai University; ShanghaiEnhanced Lab of Ferrometallurgy; Shanghai 200072). HIGH ORDER SUB-REGULAR SOLUTION MODEL AND ITS APPLICATIONS IN THE CALCULATION OF COMPONENT ACTIVITIES OF MnO-SiO_2-Al_2O_3-CaO MOLTEN SLAG. Acta Metall Sin, 1997, 33(10): 1085-1093.

Download:  PDF(709KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  a high order sub-regular solution modeI for predicting the component activities in a homogeneous region of a quaternary system was developed in the Shanghai Enhanced Lab of Ferrometallurgy, which is designated as SELF-SReM4. It is composed of some polynomials of excess mole free energies versus content variable. a group of parameters is included in the polynomials. along with the reliable known thermodynamic properties associating the homogeneous region the parameters can be evaluated. and then the component activities in that region are possible to be predicated. This paper is devoted to illustrate the applications of SELF-SReM4 for molten slag of MnO-SiO2-al2O3-CaO and its sub-ternary systems. The evaluated results were very close to those of slag-metal equilibrium experiments and the Chipman's and Pelton's results.
Key words:  SELF-SReM4 model      MnO-SiO_2-Al_2O_3-CaO system      calculation of component activity     
Received:  18 October 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I10/1085

1 Masson V R. 2nd Intern Confon Melten Fluxes and Slags, Lake Tahoe, 1984; 3
2 万谷郎,日野光兀,铁钢,1988, 74;1701
3 Pelton a D, Blander M. 2nd Intern Con fon Melten Fluxes and Slagr, Lake Tahoe, 1984;281
4 Kriksson G, Pelton a D. Metall Trans. 1993, 24B:795
5 Gaye H, Welfringer J. 2nd Intern Confon Melten Fluxes and Slagr, Lake Tahoe, 1984;357
6 Gaye H, Riboud P V, Welfringer J. 5th Int. Iron SteeI Congr, Washington D.C., 1996: 631
7 Hillert M, Jansson B, Sundman B, J agren Met Trans, 1985; 16a:261
8 Jiang Guo Chang, Zhang Xiao Bing, Xu Kuang Di. acla Metall Sin, 1992, 5B:476
9 Zhang Xiao Bing. Ph.D. Thesis, Shanghai University, 1996:24
10 S.Ban-Ya, M.Hino. Chemical Properties of Melten Slags, ISIJ, 1991; 17
11 abraham K P, Davies M W, Richardson F D. J Iron Steel Inst, 1960, 196:82
12 Sharma R a, Richardson F D. Trans MeI Soc aIME, 1965, 233:1586
l3 Rein R H, Chipman J. Trans Met Soc aIME, 1965, 233; 415
14 Sharma R a, Richardson F D. J Iron Steel Inst, 1961, 198:386
15 Risbud S H, Pask J a. J am Ceramic Society, 1977, 60, 418
16 Mehta S R, Richardson F D. J Iron Steel Inst, 1965, 203:524
17 Warren G F, Jochens P R, Howat D D. INFaCON, 1974: 175
18 Ding W, Olsen S E. Metall Trans, 1996; 27B:5
No related articles found!