| LOW CYCLE FATIGUE BEHAVIOR OF A DZX40M DIRECTIONALLY SOLIDIFIED Co-BASED SUPERALLOY──Ⅰ.Fatigue and Its Mechanism at Room Temperature |
| LU Zheng; ZHOU Huihua; XU Yongbo; HU Zhuannqi (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015) |
|
Cite this article:
LU Zheng; ZHOU Huihua; XU Yongbo; HU Zhuannqi (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). LOW CYCLE FATIGUE BEHAVIOR OF A DZX40M DIRECTIONALLY SOLIDIFIED Co-BASED SUPERALLOY──Ⅰ.Fatigue and Its Mechanism at Room Temperature. Acta Metall Sin, 1997, 33(12): 1239-1245.
|
|
|
Abstract Low cycle fatigue behavior of a DZX40M directionally solidified Co-based superalloy has been investigated at room temperature in air under different total strain amplitudes ranging from 2.5 × 10(-3) to 6.0 × 10(-3). The results show that the cyclic hardening of the alloy appears at the first few cycles in the initial hardening stage, and then the saturation stage which is the major part of the whole fatigue life begins. Examination by TEM indicates that the initial hardening of the alloy is caused by the pile-up of the stacking faults at the intersection of stacking fault, while the saturation of the alloy during low cycle fatigue is arising from the transition of the stacking fault on the (111) to the closely spaced stacking fault ribbon on the (111).
|
|
|
1Thomas S, William H. The Superalloys. New York: Wlley, 1972: 45 2Davin A. Cobalt, 1974; 21: 32 3Howie A,Whelan M J.Proc R Soc London,1962:A267:206 4Gevers R, Art A, Amelinckx S. Phys Status Solidi, 1963; 3: 1563 5郭可信,叶恒强,吴玉琨,电子衍射图在晶体学中的应用,北京:科学出版社,1983:408 6Rajan K. Scr Metall, 1983; 17: 101 7Cohen J,B,Weertman J.Acta Metall,1963;11:996 |