| STRUCTURE AND MAGNETIC PROPERTIES OF QUASI-TERNARY TbMn_(6-x)Co_xSn_6 COMPOUNDS |
| WANG Yingung;CHEN Changpin;WANG Qidong(Zhejiang University; Hangzhou 310027); TANG Ning;YANG Fuming (State Key Laboratory of Magnetism; Institute of Physics; Chinese Academy of Sciences; Beijing 100080) |
|
Cite this article:
WANG Yingung;CHEN Changpin;WANG Qidong(Zhejiang University; Hangzhou 310027); TANG Ning;YANG Fuming (State Key Laboratory of Magnetism; Institute of Physics; Chinese Academy of Sciences; Beijing 100080). STRUCTURE AND MAGNETIC PROPERTIES OF QUASI-TERNARY TbMn_(6-x)Co_xSn_6 COMPOUNDS. Acta Metall Sin, 1997, 33(5): 543-547.
|
|
|
Abstract Structure and magnetic properties of quasi-ternary TbMn6-xCoxSn6 compounds with x=0.0, 0.3, 0.6, 0.9, 1.2 and 1.5 have been studied. The structure of TbMn6-xCoxSn6 compounds has not been changed on Co substitution. The substitution of Co for Mn in TbMn6Sn6 results in a monotonous decrease in the lattice constants and the unit-cell volume. The ordering temperature decreases monotonously with increasing Co content. The reorientation temperature decreases with increasing Co content and the reorientation of easy axis magnetization of TbMn6Sn6 disappeared at x=0.6. When x exceeding 0.9 a compensation temperature was observed in the thermal magnetization curve and the compensation temperature increases with increasing Co content. The saturation magnetization at 4.5 K decreases to a minimum at x=0.6 and then increases again.
|
|
Received: 18 May 1997
|
1Venturini G,Chafik E1 Idrissi B,Malaman B.J Magn Magn Mater,1991;94:35 2Chafik E1 Idrissi B,Venturini G,Malaman B,Fruchart D.J Less-Common Met,1991;175:143 3Venturini G,Welter R, Malaman B.J Alloys Compounds,1992;185:99 4Weitzer F,Leithe-Jasper A,Hiebl K,Rogl P,Qi Qinian,Coey J M D.J Appl Phys,1993;73:8447 5Wang Yingang,Yang Fuming,Chen Changpin,Tang Ning,Wang Jianli,Han Xiufeng,PanHongge,Hu Jifan,Zhou Kaiwen,Zhao Ruwen,Wang Qidong.J Phys:Condens Matter,1996;8:1851 6Colpa J H P,Brabers J H V J.Physica B,1994;203:29 7Jacobs T H,Buschow K H J,Zhou G F,Li X,de Boer F R. J Magn Magn Mater,1992;116:220 8 Nguyen H D.Phys Stat Sol(b),1993;176: K29 |