| CRYSTAL STRUCTURE AND MAGNETIC PROPERTIES OF Y_2Fe_(17-x)Mn_x |
| YIN Xiaoying;WANG Yingang;TANG Ning;YANG Fuming(State Key Laboratory of Magnetism; Institute of Physics; Chinese Academy of Sciences; Beijing 100080)(Chinese People's Public Security University; Beijing 100038) |
|
Cite this article:
YIN Xiaoying;WANG Yingang;TANG Ning;YANG Fuming(State Key Laboratory of Magnetism; Institute of Physics; Chinese Academy of Sciences; Beijing 100080)(Chinese People's Public Security University; Beijing 100038). CRYSTAL STRUCTURE AND MAGNETIC PROPERTIES OF Y_2Fe_(17-x)Mn_x. Acta Metall Sin, 1997, 33(5): 539-542.
|
|
|
Abstract X-ray diffraction has proved that the structure of Y2Fe17-xMnx(x≤6.0) compounds is same as Y2Fe17. The study on the lattice constants, Curie temperature and magnetization of the Y2Fe17-xMnx compounds has shown that the lattice constants do not increase continuously with increasing Mn content and have a minimum at x=2.0. The Curie temperature increases from 328 K (x=0.0) to 342 K (x=0.3), and then decreases with increasing Mn content. The saturation magnetization decreases with increasing Mn content.
|
|
Received: 18 May 1997
|
1 Chafik El Idrissi B,Venturini G,Malaman B Fruchart D.J Less-Common Met, 1991;175:143 2 Jacobs J H,Buschow K H J,Zhou Z F,Liu J P,Li X,De Boer F R.J Magn Magn Mater,1992;104:1275 3 de Boer F R,Zhong X P,Buschow K H J,Jacobs T H,J Magn Magn Mater,1990;90-91:25 4 Franse J J M,Radwanski R J.Handbook of Magnetic Material.Vol.7,Amsterdam:ElsevierScience,1993:384 5 Li Hongshuo,Coey J M D.Handbook of Magnetic Material.Vol.6,Amsterdam:Elsevier Science,1991:73 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|