| MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Mg–12Zn–4Al–0.3Mn ALLOY CONTAINING Sr AND Ca |
| WAN Xiaofeng1; SUN Yangshan1; 2; XUE Feng1; 2; BAI Jing1; 2; TAO Weijian3 |
1. School of Materials Science and Engineering; Southeast University; Nanjing 211189
2. Jiangsu Key Laboratory for Advanced Metallic Materials; Nanjing 211189
3. Jiangsu Engineering Research Center for Magnesium Alloys; Nanjing 211224 |
|
Cite this article:
WAN Xiaofeng; SUN Yangshan; XUE Feng; BAI Jing; TAO Weijian. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Mg–12Zn–4Al–0.3Mn ALLOY CONTAINING Sr AND Ca. Acta Metall Sin, 2009, 45(5): 585-591.
|
|
|
Abstract Magnesium alloys have emerged as potentially good candidates for numerous applications, especially in automotive industry. Although the commonly used magnesium alloys, such as AZ91 and AM60 based on Mg–Al system have excellent castability, good room temperature mechanical properties and low cost, the application of these alloys has been limited to temperatures below 120℃ because of their poor heat resistance, especially creep property at elevated temperatures. Recent development reported that magnesium alloys with high zinc and low aluminum concentrations (Mg–Zn–Al based alloys) exhibit better creep properties than Mg–Al based alloys at temperatures above 150 ℃ and small amounts of alkaline–earth element (Sr and Ca) additions to the Mg–Zn–Al ternary alloys lead to further improvement of their mechanical properties. The purpose of the present paper is to describe the effects of calcium and strontium additions on the microstructure and mechanical properties of Mg–12Zn–4Al–0.3Mn based alloy. The results indicate that the as–cast microstructure of Mg–12Zn–4Al–0.3Mn alloy consists of the α–Mg matrix and a quasicrystalline Q phase at grain boundaries. Small amounts of Sr addition to the master alloy result in the transition of metastable Q phase to the equilibrium Mg32(Al, Zn)49 phase and the formation of binary eutectic phase Mg51Zn20. Another lamellar eutectic phase Al2Mg5Zn2 is observed in the as–cast microstructure when Ca combined with Sr is added to the base alloy, and its volume fraction increases with increase of Ca addition. The single addition of Sr causes the increase of tensile strength, but decrease of creep resistance at elevated temperatures. However, the creep properties are significantly improved if Sr is added in combination with Ca to the master alloy due to the formation of ternary eutectic phase Al2Mg5Zn2, which shows the high thermal stability at elevated temperatures. The alloy with composition of Mg–12Zn–4Al–0.2Sr–0.4Ca–0.3Mn exibits good creep resistance at 175℃and 70 MPa.
|
|
Received: 06 May 2008
|
|
|
| Fund: Supported by National Key Basic Technology R&D Program of China (No.2006BAE04B07) and Special Program for the Commercialization of Key Science and Technology Achievements Financed by Jiangsu Science and Technology Department (No.BA2005004) |
| [1] Luo A, Pekguleryuz M O. J Mater Sci, 1994; 29: 5259
[2] Li P J, Zeng D B, Guo X T. Chin Rare Earths, 2002; 23(2): 63
(李培杰, 曾大本, 郭旭涛. 稀土, 2002; 23(2): 63)
[3] Luo A A. Int Mater Rev, 2004; 49: 13
[4] Zeng R C, Ke W, Xu Y B, Han E H, Zhu Z Y. Acta MetallSin, 2001; 37: 673
(曾荣昌, 柯伟, 徐永波, 韩恩厚, 朱自勇. 金属学报, 2001; 37: 673)
[5] Zhang Z, Couture A, Luo A. Scr Mater, 1998; 39: 45
[6] Zhang J, Guo Z X, Pan F S, Li Z S, Luo X D. Mater Sci Eng, 2007; A456: 43
[7] Zhang Z, Tremblay R. Canad Metall Quart, 2000; 39: 503
[8] Zhang Z, Tremblay R, Dub´e D. Mater Sci Eng, 2004; A385: 286
[9] Liu C M, Zhu X R, Zhou H T. Magnesium Phase Diagram. Changsha: Central South University Press, 2006:256
(刘楚明, 朱秀荣, 周海涛. 镁合金相图集. 长沙: 中南大学出版社, 2006: 256)
[10] Higashi I, Shiotani N, Uda M, Mizoguchi T, Katoh H. J Solid State Chem, 1981; 36: 225
[11] Bergman G, Waugh J L T, Pauling L. Acta Crystal–Logr, 1957; 10: 254
[12] Bourgeois L, Muddle B C, Nie J F. Acta Mater, 2001; 49: 2701
[13] Sun Y S, Zhang W M, Min X G. Acta Metall, 2001; 14: 330
[14] Vogel M, Kraft O, Dehm G, Arzt E. Scr Mater, 2001; 45: 517
[15] Takeuchi T, Murasaki S, Matsumuro A, Mizutani U. J Non–Cryst Solids, 1993; 914: 156
[16] Niikura A, Tsai A, Nishiyama N, Inoue A, Masumoto T. Mater Sci Eng, 1994; A1387: 181
[17] Petrov D V, Petzow G, Effenberg G. Aluminum–Magnesium–Zinc Ternary Alloys: A Comprehensive Compendium of Evaluated Constitutional Data and Phase Diagrams. Weinheim: VCM, 1993: 57
[18] Henley C L, Elser V. Philos Mag, 1986; 53B: 59
[19] Wang S Q, Ye H Q. Philos Mag, 1991; 64B: 551
[20] Wei L Y, Dunlop G L, Westengen H. Metall Mater Trans, 1995; 26A: 1947 |