| MARTENSITE TRANSFORMATION IN TiNi ALLOY UNDER COUPLING TEMPERATURE AND HIGH MAGNETIC FIELD USING LANDAU THEORY MODEL |
| ZHENG Bin; ZHOU Wei; WANG Yinong; QI Min |
| School of Materials Science and Engineering; Dalian University of Technology; Dalian 116024 |
|
Cite this article:
ZHENG Bin ZHOU Wei WANG Yinong QI Min. MARTENSITE TRANSFORMATION IN TiNi ALLOY UNDER COUPLING TEMPERATURE AND HIGH MAGNETIC FIELD USING LANDAU THEORY MODEL. Acta Metall Sin, 2009, 45(1): 37-42.
|
|
|
Abstract The martensitic transformation behavior under coupling temperature and high magnetic field in TiNi paramagnetic shape memory alloy was studied by using the modified Landau model. In order to introduce the effect of high magnetic field, the Fermi surface total density of state (DOS) of TiNi alloy under different phase--transformed shear strain (order parameter) was calculated by using the first--principles calculations, then the relationship between magnetic susceptibility and shear strain was carried out. The calculation results from the modified Landau model involving the effect of magnetic free energy indicated that the martensitic transformation temperatures (Ms and T0) suddenly increase. It can be mainly contributed to the parabola increasing of martensitic transformation driving force under coupling temperature and high magnetic field. Also, it is found that the oriented growth of martensitic variants occurs under coupling temperature and high magnetic field due to the increased difference of free energy between variants, which is consistent with the TEM observation that some vertical two--variants are present in TiNi alloy under 5 T magnetic field.
|
|
Received: 10 March 2008
|
|
|
| Fund: Supported by National Natural Science Foundation of China (Nos.50531020 and 50471067) |
| [1] Humbeeck J V. Mater Sci Eng, 1999; A273–275: 134
[2] Duerig T, Pelton A, St¨ockel D. Mater Sci Eng, 1999; A273–275: 149
[3] Less M R, Bourgault D, Braithwaite D. Physica, 1999; 191C: 414
[4] Beaugnon E, Touriner R. Nature, 1991; 349: 470
[5] Farrell D E, Chandrasekhar B S, DeGuire M R, Fang M M, Kogan V G, Clem J R, Finnemore D K. Phys Rev, 1987; 36B: 4025
[6] Satyanarayan K R, Eliasz W, Miodownik A P. Acta Metall, 1968; 16: 877
[7] Kakeshita T, Shimizu K, Funada S, Date M. Acta Metall, 1985; 33: 1381
[8] Joo H D, Kim S U, Shin N S, Koo Y M. Mater Lett, 2000; 43: 225
[9] Tickle R, James R D, Wuttig M, Kokorin V V, Shield T. IEEE Trans Magn, 1999; 35: 4301
[10] Guo S H, Zhang Y H, Li J L, Qi Y, Wang X L. Acta Metall Sin, 2004; 40: 972
(郭世海, 张羊换, 李健靓, 祁焱, 王新林. 金属学报, 2004; 40: 972)
[11] Liu X P, Wang Y N, Qi M, Yang D Z. Chin J Nonferrous Met, 2006; 16: 2005
(刘晓鹏, 王轶农, 齐 民, 杨大智. 中国有色金属学报, 2006; 16: 2005)
[12] Falk F. Acta Metall, 1980; 28: 1773
[13] Wang F E, Buehler W J, Pickart S J. J Appl Phys, 1965; 36: 3232
[14] Perdew J P, Wang Y. Phys Rev, 1992; 45B: 13244
[15] Otsuka K, Ren X. Prog Mater Sci, 2005; 50: 511
[16] Kudoh Y, Tokonami M, Miyazaki S, Otsuka K. Acta Metall, 1985; 33: 2049
[17] Madangopal K. Acta Mater, 1997; 45: 5347 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|