| IMPROVEMENT ON THE MODIFIED MAXIMUM ENTROPY METHOD FOR TEXTURE ANALYSIS BY PARTICLE SWARM OPTIMIZATION |
| WANG Dapeng1; WANG Dazhi2; WU Baolin1; ZUO Liang3; WANG Fu3; LIANG Zhide3 |
1 School of Materials Science and Engineering; Shenyang Institute of Aeronautical Engineering; Shenyang 110136
2 College of Information Science and Engineering; Northeastern University; Shenyang 110004
3 School of Materials and Metallurgy; Northeastern University; Shenyang 110004 |
|
Cite this article:
WANG Dapeng WANG Dazhi WU Baolin ZUO Liang WANG Fu LIANG Zhide. IMPROVEMENT ON THE MODIFIED MAXIMUM ENTROPY METHOD FOR TEXTURE ANALYSIS BY PARTICLE SWARM OPTIMIZATION. Acta Metall Sin, 2009, 45(1): 63-66.
|
|
|
Abstract The particle swarm optimization (PSO) was successfully applied for the modified maximum entropy method (MMEM) of the quantitative texture analysis. Using two incomplete pole figures or only one incomplete pole figure, the complete orientation distributions of pure copper samples can been obtained. Such an improvement has been verified to keep the merits of primary MMEM, i.e., the complete orientation distribution function (ODF) of samples can be calculated using lesser experimental data, furthermore, the difficulty to choose a set of purposely initial solutions has also been overcome when solving the nonlinear equation, which makes the MMEM more versatile and practicable.
|
|
Received: 23 April 2008
|
|
|
| Fund: Supported by National Natural Science Foundation of China (No.50771067) and Doctorate Research Project of Shenyang Institute of Aeronautical Engineering (No.BY2009-2953) |
| [1] Liang Z D. Acta Metall Sin, 1997; 33: 133
(梁志德. 金属学报, 1997; 33: 133)
[2] Wang F, Xu J Z, Liang Z D. Textures Microstruct, 1992; 19: 55
[3] Kennedy J, Eberhart R. Proc IEEE Int Conf Neural Networks. Piscataway, NJ: IEEE Service Center, 1995: 1942
[4] Tang J G, Zhang X M, Deng Y L, Xuan Y, Chen Z Y. Mater Sci Forum, 2007; 546: 1009
[5] Wang D Z, Wang D P, Wang D W, Zuo L, Wang F, Liang Z D. Acta Metall Sin, 2008; 44: 183
(王大志, 王大鹏, 汪定伟, 左良, 王福, 梁志德. 金属学报, 2008; 44: 183)
[6] Wang Y D, Xu J Z, Liang Z D. Textures Microstruct, 1998; 26–27: 103
[7] Jiang J X,Wang F, Liu Y S, Liang Z D. In: Liang Z D, Zuo L, Chu Y Y, eds., Proc 11th Int Conf Textures of Materials, Part 1, Beijing: International Academic Publishers, 1996: 112
[8] Shi Y, Eberhart R. IEEE Int Conf Evolutionary Computation, Piscataway, NJ: IEEE Service Center, 1998: 69
[9] Trelea I. Inf Process Lett, 2003; 85: 317
[10] Liang Z D, Xu J Z, Wang F. Three Dimensional Orientation Analysis of Textured Materials–ODF Analysis. Shenyang: Northeastern University of Technology Press, 1986: 116
(梁志德, 徐家祯, 王福. 织构材料的三维取向分析术---ODF分析. 沈阳: 东北工学院出版社, 1986: 116) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|