| TEXTURES AND DEFORMATION MECHANISMS OF AZ31 MAGNESIUM ALLOYS UNDER SPECIAL PROCESSING TECHNOLOGIES |
| WANG Lina1;YANG Ping1; XIA Weijun2;CHEN Zhenhua2;CHEN Ding2; LI Xiao1; MENG Li1 |
1 School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing 100083
2 School of Materials Science and Engineering; Hunan University; Changsha 410082 |
|
Cite this article:
WANG Lina YANG Ping XIA Weijun CHEN Zhenhua CHEN Ding LI Xiao MENG Li. TEXTURES AND DEFORMATION MECHANISMS OF AZ31 MAGNESIUM ALLOYS UNDER SPECIAL PROCESSING TECHNOLOGIES. Acta Metall Sin, 2009, 45(1): 58-62.
|
|
|
Abstract The modifications of basal texture in AZ31 magnesium alloys processed by asymmetrical rolling and equal channel angular rolling (ECAR) are investigated. Deformation mechanisms are determined by microstructure observation and macro- and micro-texture measurements. Results show that during asymmetrical rolling the basal texture is gradually rotated around TD (transverse direction) by basal slip activated by shear strain on the rolling plane, whereas the prism texture is induced by tension twinning activated by shearing parallel to the plane separating the two channels during ECAR. So both the special processing techniques may improve the plasticity of magnesium alloy. The effects of rolling reduction and annealing on textures are also studied and discussed.
|
|
Received: 17 April 2008
|
|
|
| Fund: Supported by National Natural Science Foundation of China (No.50571009) and State Key Laboratory\par
for Advanced Metals and Materials of University of Science and Technology Beijing (No.2007AMM006) |
| [1] Mukai T, Yamanoi M,Watanabe H, Higashi K. Scr Mater, 2001; 45: 89
[2] Yoshida Y, Cisar L, Kamado S, Kojima Y. Mater Trans, 2003; 44: 468
[3] Kim H K, Kim W J. Mater Sci Eng, 2004; A385: 300
[4] Kim W J, Hong S I, Kim Y S, Min S H, Jeong H T, Lee J D. Acta Mater, 2003; 51: 3293
[5] Liu X, Chen Z H, Xia W J, Cheng Y Q, Yang Z W. Hot Work Technol, 2006; 35(20): 22
(刘兴, 陈振华, 夏伟军, 程永奇, 杨忠旺. 热加工工艺, 2006; 35(20): 22)
[6] Kim S H, You B S, Yim C D, Seo Y M. Mater Lett, 2005; 59: 3876
[7] Ji Y H, Park J J, Kim W J. Mater Sci Eng, 2007; A454–455: 570
[8] Watanabe H, Mukai T, Ishikawa K. J Mater Process Technol, 2007; 182: 644
[9] Cheng Y Q, Chen Z H, Xia W J, Fu D F. Chin J Nonferrous Met, 2005; 15: 1369
(程永奇, 陈振华, 夏伟军, 傅定发. 中国有色金属学报, 2005; 15: 1369)
[10] Cheng Y Q, Chen Z H, Xia W J. Mater Charact, 2006; 58: 617
[11] Cheng Y Q, Chen Z H, Xia W J, Zhou T. J Mater Process Technol, 2006; 184: 97
[12] Yang P, Meng L, Xie Q G, Cui F E. Mater Sci Forum, 2007; 546–549: 297
[13] Meng L, Yang P, Xie Q G, Mao W M. Mater Trans, 2008; 49: 710 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|