IMPROVEMENT ON THE MODIFIED MAXIMUM ENTROPY METHOD FOR TEXTURE ANALYSIS BY PARTICLE SWARM OPTIMIZATION
WANG Dapeng1; WANG Dazhi2; WU Baolin1; ZUO Liang3; WANG Fu3; LIANG Zhide3
1 School of Materials Science and Engineering; Shenyang Institute of Aeronautical Engineering; Shenyang 110136
2 College of Information Science and Engineering; Northeastern University; Shenyang 110004
3 School of Materials and Metallurgy; Northeastern University; Shenyang 110004
Cite this article: 

WANG Dapeng WANG Dazhi WU Baolin ZUO Liang WANG Fu LIANG Zhide. IMPROVEMENT ON THE MODIFIED MAXIMUM ENTROPY METHOD FOR TEXTURE ANALYSIS BY PARTICLE SWARM OPTIMIZATION. Acta Metall Sin, 2009, 45(1): 63-66.

Download:  PDF(556KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The particle swarm optimization (PSO) was successfully applied for the modified maximum entropy method (MMEM) of the quantitative texture analysis. Using two incomplete pole figures or only one incomplete pole figure, the complete orientation distributions of pure copper samples can been obtained. Such an improvement has been verified to keep the merits of primary MMEM, i.e., the complete orientation distribution function (ODF) of samples can be calculated using lesser experimental data, furthermore, the difficulty to choose a set of purposely initial solutions has also been overcome when solving the nonlinear equation, which makes the MMEM more versatile and practicable.

Key words:  particle swarm optimization      texture      orientation distribution function      modified maximum entropy method     
Received:  23 April 2008     
ZTFLH: 

TG335.19

 
Fund: 

Supported by National Natural Science Foundation of China (No.50771067) and Doctorate Research Project of Shenyang Institute of Aeronautical Engineering (No.BY2009-2953)

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2009/V45/I1/63

[1] Liang Z D. Acta Metall Sin, 1997; 33: 133
(梁志德. 金属学报, 1997; 33: 133)
[2] Wang F, Xu J Z, Liang Z D. Textures Microstruct, 1992; 19: 55
[3] Kennedy J, Eberhart R. Proc IEEE Int Conf Neural Networks. Piscataway, NJ: IEEE Service Center, 1995: 1942
[4] Tang J G, Zhang X M, Deng Y L, Xuan Y, Chen Z Y. Mater Sci Forum, 2007; 546: 1009
[5] Wang D Z, Wang D P, Wang D W, Zuo L, Wang F, Liang Z D. Acta Metall Sin, 2008; 44: 183
(王大志, 王大鹏, 汪定伟, 左良, 王福, 梁志德. 金属学报, 2008; 44: 183)
[6] Wang Y D, Xu J Z, Liang Z D. Textures Microstruct, 1998; 26–27: 103
[7] Jiang J X,Wang F, Liu Y S, Liang Z D. In: Liang Z D, Zuo L, Chu Y Y, eds., Proc 11th Int Conf Textures of Materials, Part 1, Beijing: International Academic Publishers, 1996: 112
[8] Shi Y, Eberhart R. IEEE Int Conf Evolutionary Computation, Piscataway, NJ: IEEE Service Center, 1998: 69
[9] Trelea I. Inf Process Lett, 2003; 85: 317
[10] Liang Z D, Xu J Z, Wang F. Three Dimensional Orientation Analysis of Textured Materials–ODF Analysis. Shenyang: Northeastern University of Technology Press, 1986: 116
(梁志德, 徐家祯, 王福. 织构材料的三维取向分析术---ODF分析. 沈阳: 东北工学院出版社, 1986: 116)

[1] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[2] LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature[J]. 金属学报, 2023, 59(11): 1439-1447.
[3] JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge. Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. 金属学报, 2022, 58(12): 1545-1556.
[4] YANG Ping, WANG Jinhua, MA Dandan, PANG Shufang, CUI Feng'e. Influences of Composition on the Transformation-Controlled {100} Textures in High Silicon Electrical Steels Prepared by Mn-Removal Vacuum Annealing[J]. 金属学报, 2022, 58(10): 1261-1270.
[5] DING Ning, WANG Yunfeng, LIU Ke, ZHU Xunming, LI Shubo, DU Wenbo. Microstructure, Texture, and Mechanical Properties of Mg-8Gd-1Er-0.5Zr Alloy by Multi-Directional Forging at High Strain Rate[J]. 金属学报, 2021, 57(8): 1000-1008.
[6] YAN Mengqi, CHEN Liquan, YANG Ping, HUANG Lijun, TONG Jianbo, LI Huanfeng, GUO Pengda. Effect of Hot Deformation Parameters on the Evolution of Microstructure and Texture of β Phase in TC18 Titanium Alloy[J]. 金属学报, 2021, 57(7): 880-890.
[7] ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang. Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys[J]. 金属学报, 2021, 57(11): 1396-1415.
[8] XU Zhanyi, SHA Yuhui, ZHANG Fang, ZHANG Huabing, LI Guobao, CHU Shuangjie, ZUO Liang. Orientation Selection Behavior During Secondary Recrystallization in Grain-Oriented Silicon Steel[J]. 金属学报, 2020, 56(8): 1067-1074.
[9] YU Lei,LUO Haiwen. Effect of Partial Recrystallization Annealing on Magnetic Properties and Mechanical Properties of Non-Oriented Silicon Steel[J]. 金属学报, 2020, 56(3): 291-300.
[10] CHENG Chao,CHEN Zhiyong,QIN Xushan,LIU Jianrong,WANG Qingjiang. Microstructure, Texture and Mechanical Property ofTA32 Titanium Alloy Thick Plate[J]. 金属学报, 2020, 56(2): 193-202.
[11] DU Zijie, LI Wenyuan, LIU Jianrong, SUO Hongbo, WANG Qingjiang. Study on the Uniformity of Structure and Mechanical Properties of TC4-DT Alloy Deposited by CMT Process[J]. 金属学报, 2020, 56(12): 1667-1680.
[12] Xin LI,Yuecheng DONG,Zhenhua DAN,Hui CHANG,Zhigang FANG,Yanhua GUO. Corrosion Behavior of Ultrafine Grained Pure Ti Processed by Equal Channel Angular Pressing[J]. 金属学报, 2019, 55(8): 967-975.
[13] Liping DENG,Kaixuan CUI,Bingshu WANG,Hongliang XIANG,Qiang LI. Microstructure and Texture Evolution of AZ31 Mg Alloy Processed by Multi-Pass Compressing Under Room Temperature[J]. 金属学报, 2019, 55(8): 976-986.
[14] Zheng LIU,Jianrong LIU,Zibo ZHAO,Lei WANG,Qingjiang WANG,Rui YANG. Microstructure and Tensile Property of TC4 Alloy Produced via Electron Beam Rapid Manufacturing[J]. 金属学报, 2019, 55(6): 692-700.
[15] Houlong LIU,Mingyu MA,Lingling LIU,Liangliang WEI,Liqing CHEN. Effect of Hot Band Annealing Processes on Texture and Formability of 19Cr2Mo1W Ferritic Stainless Steel[J]. 金属学报, 2019, 55(5): 566-574.
No Suggested Reading articles found!