Please wait a minute...
Acta Metall Sin  2008, Vol. 44 Issue (6): 675-680     DOI:
Research Articles Current Issue | Archive | Adv Search |
EFFECTS OF ANNEALING TEMPERATURE ON THE MICROSTRUCTURES AND PROPERTIES OF COPPER CLADDING ALUMINUM WIRES BY COLD HYDROSTATIC EXTRUSION
;;;
北京科技大学材料科学与工程学院
Cite this article: 

;. EFFECTS OF ANNEALING TEMPERATURE ON THE MICROSTRUCTURES AND PROPERTIES OF COPPER CLADDING ALUMINUM WIRES BY COLD HYDROSTATIC EXTRUSION. Acta Metall Sin, 2008, 44(6): 675-680 .

Download:  PDF(2489KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effects of annealing temperature on the microstructures and properties of copper cladding aluminum wires fabricated by cold hydrostatic extrusion were investigated, and the influence mechanism was discussed based on the different interface fracture modes. The experimental results show that the appropriate annealing temperature is 350℃ for as-extruded wires. At a annealing temperature below 200℃, a recovery process is dominant in copper sheath and the mechanical properties partly recovered. The recrystallization of copper proceeded sufficiently at 350℃, the tensile strength reaches a minimum and the elongation gets its maximum. The growth of copper grains occurred during annealing at 400℃, which decreases the elongation of the alloy. With the annealing temperature increased, the interface strength of the Cu/Al bimetal wires increased to a maximum value and then decreased, the interface fracture location transformed from Al-side to the Cu/Al interface and at the same time the fracture mode transformed from ductile to brittle.
Key words:  hydrostatic extrusion      copper cladding aluminum wire      annealing temperature      microstructure      mechanical      
Received:  09 November 2007     
ZTFLH:  TG146.4  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I6/675

[1]Kang C G,Jung Y J,Kwon H C.J Mater Process Technol, 2002;124:49
[2]Xu R C,Tang D,Ren X P,Wang X H,Wen Y H.Rare Met,2007;26:230
[3]Braunovi■ M,Aleksandrov N.Proc 38th IEEE Holm Conf of Electrical Contacts,Philadelphia,USA,18 21 Oct., 1992:25
[4]Chen S D,Ke F J,Zhou M,Bai Y L.Acta Mater,2007: 55:3169
[5]Lee W B,Bang K S,Jung S B.J Alloys Compd,2005; 390:212
[6]Lee J E,Bae D H,Chung W S,Kim K H,Cho Y R.,J Mater Process Technol,2007;187-188:546
[7]Heness G,Wuhrer R,Yeung W Y.Mater Sci En9 A,Avail- able Online at www.sciencedirect.com,16 May,2007,in Press
[8]Moreno D,Garrett J,Embury J D.Intermetallics,1999; 7:1001
[9]Hang C J,Wang C Q,Mayer M,Tian Y H,Zhou Y,Wang H H.Microelectron Reliab,2008;48:416
[10]Chen C Y,Chcn H L,Hwang W S.Mater Trans,2006; 47:1232
[11]Shen L.Master Degree Dissertation,Kunming University of Science and Technology,2002 (沈黎.硕士学位论文,昆明理工大学,2002)
[12]Shackelford J F,Alexander W.Materials Science and En- gineering Handbook. Boca Raton,FL:CRC Press LLC, 2001:1
[13]Ying D Y,Zhang D L.J Alloys Compd,2000;311:275
[14]Tomida S,Nakata K,Saji S.Surf Coat Technol,2001; 142-144:585
[15]Ouyang J,Yarrapareddy E,Kovacevic R.J Mater Process Technol,2006;172:110
[16]Pcng X K,Wuhrer R,Heness G,Yeung W Y.J Mater Sci, 1999;34:2029
[1] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[2] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[3] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[4] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[5] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[6] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[7] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[8] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[9] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[10] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[11] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[12] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[13] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[14] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[15] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
No Suggested Reading articles found!