| The mesomechanical analysis of the deformation of copper with continuous columnar crystals |
| ZOU Fenglei; GAO Kewei; ZHU Qifang; XIEJianxin |
|
Cite this article:
ZOU Fenglei; GAO Kewei; ZHU Qifang; XIEJianxin. The mesomechanical analysis of the deformation of copper with continuous columnar crystals. Acta Metall Sin, 2008, 44(3): 297-301 .
|
|
|
Abstract The pure copper bar with continuous columnar crystals, which had excellent plastic workability and conductivity, was fabricated by continuous unidirectional solidification process with vacuum melting and argon protecting. This paper investigates the copper bar’s plastic deformation behavior through mesomechanical analysis with the device developed by General Research Institute for Nonferrous Metals. It was found that during the deformation, different crystals had different slip systems because of different crystal orientation, and the nucleation of a sub-grain was observed. Grain boundary played an important role in the deformation, which is the reason for excellent plastic workability.
|
|
Received: 03 July 2007
|
|
|
[1]Zhang H,Xie J X,Wang Z D,Wang H.Mater Mech,2004; 28(2):31 (张鸿,谢建新,王自东,王浩.机械工程材料,2004;28(2):31) [2]Li B,Wang X,Guo J C,Fan X H,Yan W.J Xi'an Inst Technol,2005;25:579 (李炳,王鑫,郭俊仓,范新会,严文.西安工业学院学报,2005;25:579) [3]Wu T K,Liu W.J Tsinghua Univ (Nat Sci),2005;45: 792 (吴廷坤,刘伟.清华大学学报(自然科学版),2005;45:792) [4]Huang X X,Cai D Y,Liu Q,Yao M.Chin J Nonferrous Met,2001;11:110 (黄晓旭,蔡大勇,刘庆,姚枚.中国有色金属学报,2001;11:110) [5]Li H Y,Yah W,Chen J,Fan X H,Wang X Y.J Xi'an Inst Technol,2006;26:64 (李红英,严文,陈建,范新会,王雪艳.西安工业学院学报,2006;26:64) [6]uang X.Scr Mater,1998;38:1697 [7]Wang Z G,Zhang Z F,Li X.W,Jia W P,Li S X.Mater Sci Eng,2001;A319:63 [8]Li X W,Wang Z G,Li S X.Chin J Mater Res,2000;12: 36 (李小武,王中光,李守新,材料研究学报,2000;12:36) [9]Makarov P V.Theor Appl Fract Mech,2000;33:23 [10]Panin V,Kolubaev A,Tarasov S,Popov V.Wear,2002; 249:860 [11]Miravete A,Bielsa J M,Chiminelli A,Cuartero J,Serrano S,Tolosana N.Compos Sci Technol,2006;66:2954 [12]LI Y,Li S X,Li G Y.Acta Metall Sin,2002:38:819 (李勇,李守新,李广义.金属学报,2002;38:819) [13]Yang J X.Fundamental of Metalline Plastic Deformation. Beijng:Metallurgical Industry Press,1988:179 (杨觉先.金属塑性变形物理基础.北京:冶金工业出版社,1988:179) [14]Huang X X,Cai D Y,Yao M,Liu Q,Hansen N.Chin J Nonferrous Met,2001;11:31 (黄晓旭,蔡大勇,姚枚,刘庆,Hansen N.中国有色金属学报,2001;11:31) [15]Chen M A,Li H Z,Li X Q,Liu C M.Mater Sci Eng, 2007;A452:454 [16]Xiao J M,Zhu F W.Study of Material Energy.Shanghai: Shanghai Science & Technology Press,1999:336,400 (肖纪美、朱逢吾.材料能量学.上海:上海科学技术出版社,1999:336,400) [17]Zheng Z Q.Fundamental of Material Sciences.Changsha: Zhongnan University Press,2005:353 (郑子樵.材料科学基础.长沙:中南大学出版社,2005:353) [18]Morinage T,Translated by Jin X Z.Copper and Copper Alloy.Beijing:National Defence Industry Press,1963 (森永卓一著,金宪真译.铜及铜合金.北京:国防工业出版社,1963:77) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|