The mesomechanical analysis of the deformation of copper with continuous columnar crystals
ZOU Fenglei; GAO Kewei; ZHU Qifang; XIEJianxin
Cite this article: 

ZOU Fenglei; GAO Kewei; ZHU Qifang; XIEJianxin. The mesomechanical analysis of the deformation of copper with continuous columnar crystals. Acta Metall Sin, 2008, 44(3): 297-301 .

Download:  PDF(1158KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The pure copper bar with continuous columnar crystals, which had excellent plastic workability and conductivity, was fabricated by continuous unidirectional solidification process with vacuum melting and argon protecting. This paper investigates the copper bar’s plastic deformation behavior through mesomechanical analysis with the device developed by General Research Institute for Nonferrous Metals. It was found that during the deformation, different crystals had different slip systems because of different crystal orientation, and the nucleation of a sub-grain was observed. Grain boundary played an important role in the deformation, which is the reason for excellent plastic workability.
Key words:  mesomechanical analysis      continuous columnar crystals      bicrystals deformation      sub-grains      slip-system      
Received:  03 July 2007     
ZTFLH:  TG146.1  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I3/297

[1]Zhang H,Xie J X,Wang Z D,Wang H.Mater Mech,2004; 28(2):31 (张鸿,谢建新,王自东,王浩.机械工程材料,2004;28(2):31)
[2]Li B,Wang X,Guo J C,Fan X H,Yan W.J Xi'an Inst Technol,2005;25:579 (李炳,王鑫,郭俊仓,范新会,严文.西安工业学院学报,2005;25:579)
[3]Wu T K,Liu W.J Tsinghua Univ (Nat Sci),2005;45: 792 (吴廷坤,刘伟.清华大学学报(自然科学版),2005;45:792)
[4]Huang X X,Cai D Y,Liu Q,Yao M.Chin J Nonferrous Met,2001;11:110 (黄晓旭,蔡大勇,刘庆,姚枚.中国有色金属学报,2001;11:110)
[5]Li H Y,Yah W,Chen J,Fan X H,Wang X Y.J Xi'an Inst Technol,2006;26:64 (李红英,严文,陈建,范新会,王雪艳.西安工业学院学报,2006;26:64)
[6]uang X.Scr Mater,1998;38:1697
[7]Wang Z G,Zhang Z F,Li X.W,Jia W P,Li S X.Mater Sci Eng,2001;A319:63
[8]Li X W,Wang Z G,Li S X.Chin J Mater Res,2000;12: 36 (李小武,王中光,李守新,材料研究学报,2000;12:36)
[9]Makarov P V.Theor Appl Fract Mech,2000;33:23
[10]Panin V,Kolubaev A,Tarasov S,Popov V.Wear,2002; 249:860
[11]Miravete A,Bielsa J M,Chiminelli A,Cuartero J,Serrano S,Tolosana N.Compos Sci Technol,2006;66:2954
[12]LI Y,Li S X,Li G Y.Acta Metall Sin,2002:38:819 (李勇,李守新,李广义.金属学报,2002;38:819)
[13]Yang J X.Fundamental of Metalline Plastic Deformation. Beijng:Metallurgical Industry Press,1988:179 (杨觉先.金属塑性变形物理基础.北京:冶金工业出版社,1988:179)
[14]Huang X X,Cai D Y,Yao M,Liu Q,Hansen N.Chin J Nonferrous Met,2001;11:31 (黄晓旭,蔡大勇,姚枚,刘庆,Hansen N.中国有色金属学报,2001;11:31)
[15]Chen M A,Li H Z,Li X Q,Liu C M.Mater Sci Eng, 2007;A452:454
[16]Xiao J M,Zhu F W.Study of Material Energy.Shanghai: Shanghai Science & Technology Press,1999:336,400 (肖纪美、朱逢吾.材料能量学.上海:上海科学技术出版社,1999:336,400)
[17]Zheng Z Q.Fundamental of Material Sciences.Changsha: Zhongnan University Press,2005:353 (郑子樵.材料科学基础.长沙:中南大学出版社,2005:353)
[18]Morinage T,Translated by Jin X Z.Copper and Copper Alloy.Beijing:National Defence Industry Press,1963 (森永卓一著,金宪真译.铜及铜合金.北京:国防工业出版社,1963:77)
[1] . Effects of Overlapping Process on Grain Orientation and Microstructure of  Nickel-Based Single Crystal Superalloy DD491Fabricated by Selective Laser Melting[J]. 金属学报, 0, (): 0-0.
[2] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[3] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[4] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[5] LU Yuhua, WANG Haizhou, LI Dongling, FU Rui, LI Fulin, SHI Hui. A Quantitative and Statistical Method of γ' Precipitates in Superalloy Based on the High-Throughput Field Emission Scanning Eelectron Microscope[J]. 金属学报, 2023, 59(7): 841-854.
[6] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[7] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[8] . Effects of Cu Content on the Microstructure and Tensile Property of K4061 Superalloy[J]. 金属学报, 0, (): 0-0.
[9] . Osteogenic and Antibacterial Metal-Polyphenol Drug-Loaded Coating on Biodegradable Zinc for Orthopedic Implants Application[J]. 金属学报, 0, (): 0-0.
[10] CAO Shuting, ZHANG Shaohua, ZHANG Jian. Combustion Behavior of GH4061 Alloy in High Pressure and Oxygen-Enriched Atmosphere[J]. 金属学报, 2023, 59(4): 547-555.
[11] ZHU Guoliang, KONG Decheng, ZHOU Wenzhe, HE Jian, DONG Anping, SHU Da, SUN Baode. Research Progress on the Crack Formation Mechanism and Cracking-Free Design of γ' Phase Strengthened Nickel-Based Superalloys Fabricated by Selective Laser Melting[J]. 金属学报, 2023, 59(1): 16-30.
[12] . Effects of Cryorolling on Properties and Precipitation Behavior of a High-Strength and High-Conductivity Cu-1Cr-0.2Zr-0.25Nb Alloy[J]. 金属学报, 0, (): 0-0.
[13] SONG Qingzhong, QIAN Kun, SHU Lei, CHEN Bo, MA Yingche, LIU Kui. Interfacial Reaction Between Nickel-Based Superalloy K417G and Oxide Refractories[J]. 金属学报, 2022, 58(7): 868-882.
[14] SHEN Gang, ZHANG Wentai, ZHOU Chao, JI Huanzhong, LUO En, ZHANG Haijun, WAN Guojiang. Mechanical Properties and Degradation Behavior of Hot-Extruded Zn-2Cu-0.5Zr Alloy[J]. 金属学报, 2022, 58(6): 781-791.
[15] GAO Yubi, DING Yutian, LI Haifeng, DONG Hongbiao, ZHANG Ruiyao, LI Jun, LUO Quanshun. Effect of Deformation Rate on the Elastic-Plastic Deformation Behavior of GH3625 Alloy[J]. 金属学报, 2022, 58(5): 695-708.
No Suggested Reading articles found!