| Study on the SiC-TaSi2/MoSi2 Multilayer Oxidation Protective Coating for Carbon/Carbon composites |
| HOU Dangshe; LI Kezhi; LI Hejun; FU Qiangang; WEI Jian; HE Yonggang |
|
Cite this article:
HOU Dangshe; LI Kezhi; LI Hejun; FU Qiangang; WEI Jian; HE Yonggang. Study on the SiC-TaSi2/MoSi2 Multilayer Oxidation Protective Coating for Carbon/Carbon composites. Acta Metall Sin, 2008, 44(3): 331-335 .
|
|
|
Abstract A SiC-TaSi2/MoSi2 multilayer oxidation protective coating for carbon/carbon (C/C) composites was prepared by pack cementation. Effects of the content of Ta and Mo in the second-step pack powders on the microstructure and high temperature anti-oxidation property of the multi-coating were studied by XRD, SEM, EDS and isothermal oxidation test. The results show that the multi-coating prepared at the mol ratio of 1:1 of Ta and Mo has a thicker, denser structure than those at the mol ratios of 0:1, 1:3, 3:1 and 1:0, on which the stable and dense glassy SiO2 film could be formed during oxidation test. After 326h oxidation in air at 1500℃ and thermal cycling between 1500℃ and room temperature for 23 times, the weight loss of the coated specimen was only 0.97%, implying that the multi-coating prepared at the mol ratio of 1:1 of Ta and Mo has excellent oxidation protective ability and thermal shock resistance.
|
|
Received: 23 July 2007
|
|
|
[1]Sun G L,Li H J,Qi L H,Wang Z W,Hu Z B,Chen Q. Acta Metall Sin,2006;42:1046 (孙国岭,李贺军,齐乐华,王兆伟,胡志彪,陈强.金属学报,2006;42:1046) [2]Buckley J D.Ceram Bull,1988;67:364 [3]Masao K,Shin K,Kuniyuki K,Nobutaka U,Yoshinari K. Energy Convers Manage,2001;42:1977 [4]Fang H T,Yin Z D,Zhu J C,Jeon J H,Hahn Y D.Carbon, 2001;39:2035 [5]Zhu Y C,Ohtani S,Sato Y,Iwamoto N.Carbon,2000; 38:501 [6]Zeng X R,Li H J,Yang Z.J Chin Ceram Soc,1999; 27:8 (曾燮榕,李贺军,杨峥.硅酸盐学报,1999;27(1):8) [7]Soojin P,Minkang S.Carbon,2001;39:1229 [8]Nihara K,Suzulki Y.Mater Sci Eng,1999;A261:6 [9]Petrovic J J.Mrs Bull,1993;18(7):35 [10]Ma Q,Yan B J,Kang M K,Yang Y Q.Rare Met Mater Eng,1999;28:10 (马勤,阎秉钧,康沫狂,杨延清.稀有金属材料与工程,1999;28:10) [11]Boettinger W J,Perepezko J H,Frankwicz P S.Mater Sci Eng,1992;A155:33 [12]Nakano T,Azuma M,Umakoshi Y.Intermetallics,1998; 6:715 [13]Wei F G,Kimura Y,Mishima Y.Intermetallics,2001;9: 661 [14]Hou D S,Li K Z,Li H J,Fu Q G,Wei J,Zhang Y L.J Mater Sci Technol,2007;23:559 [15]Huang J F,Zeng X R,Li H J,Xiong X B,Fu Y W.Carbon, 2004;42:1517 [16]Yanigihara K,Maruyama T,Nagata K.Intermetallics, 1993;3:243 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|