| Effect of homogenizing treatment on microstructures and properties of AZ91 alloy |
| 北京科技大学材料科学与工程学院 |
|
Cite this article:
. Effect of homogenizing treatment on microstructures and properties of AZ91 alloy. Acta Metall Sin, 2006, 42(10): 1014-1018 .
|
|
|
Abstract There are reticular coarse Mg17Al12 and component segregation generated during solidification on grain boundary of AZ91 magnesium alloy as cast, which deteriorate the mechanical properties and the workability of ingots severely. In order to improve the workability, homogenizing treatment is researched. The homogenizing temperature is 350, 380, 420, 450℃ and the holding time is 5, 10, 15, 24h. After homogenizing treatment, the Mg17Al12 phase is scattered on the α-Mg matrix as fine grains, and dendritic segregation is eliminated almost. It is concluded from the mechanical properties test that the tensile strength of the AZ91 on the condition of as-cast, homogenized at 380℃15h and 420℃5h is about 163MPa, 243MPa and 246MPa, while the elongation is about 3.2%, 11.2% and 10%.
|
|
Received: 13 December 2005
|
|
|
[1]Agfion E,Bronfin B.Mater Sci Forum,2000;350-351:19 [2]Cahn R W,Haasen P,Kramer E J.Materials Science and Technology.New York:VCH Publishers Inc,1996 [3]Mordike B L,Ebert T.Mater Sci Eng,2001;A302:37 [4]Dahle A K,Lee Y C,Nave M D,Schaffer P L,StJohn D H.J Light Met,2001;(1):61 [5]Yan Y Q,Zhang T J,Zhou L,Deng J.Rare Met,2004;23:220 [6]LüY Z Wang Q D,Ding W J.Mater Lett,2000;44:265 [7]Zhang Y Z,Zhang K,Cui D J,Wu X P,Fan J Z,Cui B,Zheng Y X,Lei J.Foundry,2000;49(12):74(张永忠,张奎,崔代金,吴绪平,樊建中,崔波,郑宇新,雷健.铸造,2000;49(12):74) [8]Huang G S,Wang L Y,Huang G J,Pan F S.J Chongqing Univ(Nat Sci),2004;27(11):18(黄光胜,汪凌云,黄光杰,潘复生.重庆大学学报(自然科学版),2004;27(11):18) [9]Peng J,Zhang D F,Yang C M,Ding P D.J Mater Eng,2004;(8):32(彭建,张丁非,杨椿楣,丁培道.材料工程,2004;(8):32) [10]Xie J X,Liu X F,Wang Z X,Jin J B.China Pat,CN200510126459.7,2005-12-12(谢建新,刘雪峰,王智祥,金军兵.中国发明专利,CN200510126459.7,2005-12-12) [11]Liu Z,Zhang K,Zeng X Q.Theoretical Basis and Applications of Magnesium-Base Alloys.Beijing:China Machine Press, 2902(刘正,张奎,曾小勤.镁基轻质合金理论基础及其应用.北京:机械工业出版社,2002) [12]Cho S S,Chun B S,Won C W.J Mater Sci,1999; 34:4311 [13]Duly D,Brechet Y.Acta Metall Mater,1994;42:3035 [14]Duly D,Simon J P,Brechet Y.Acta Metall Mater,1995;43:101m |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|