| Effects of Cold Deformation on Microstructure And Mechanical Behavior of a High Nitrogen Austenitic Stainless Steel |
| WANG Songtao; YANG Ke; SHAN Yiyin;LI Laifeng |
| Technical Institute of Physics and Chemistry; Chinese Academy of Sciences |
|
Cite this article:
WANG Songtao; YANG Ke; SHAN Yiyin; LI Laifeng. Effects of Cold Deformation on Microstructure And Mechanical Behavior of a High Nitrogen Austenitic Stainless Steel. Acta Metall Sin, 2007, 43(7): 713-718 .
|
|
|
|
|
Received: 01 February 2007
|
|
|
[1]Kamachi M U,Raj B,In:Kamachi M U,Raj B eds.,High Nitrogen Steels and Stainless Steels.New Delhi:Narosa Publishing House,2004:8 [2]Simmons J W.Mater Sci Eng,1996;A207:159 [3]Sailer G,Aigner H.In:Speidel M O,Kowanda C,Diener M eds.,HNS-2003 Conf Proc,Zurich:vdf Hochschulver- lag,2003:341 [4]Bernauer J N,Saller G.Trans Ind Inst Met,2002;55:193 [5]Stein G,Menzel J,In:Speidel M O,Uggowitzer P J eds., Ergebnisseder Werkstoff-Forschung,Band 4:Stickstof- flegierte Stahle,Zurich:Thubal-Kain,1991:33 [6]Wang S T,Yang K,Shan Y Y,Li L F.Acta Metall Sin, 2007;43:171 (王松涛,杨柯,单以银,李来风.金属学报.2007;43:171) [7]Liu S X,Liu X M,Wang W M.Iron Steel,2005;40(11): 67 (刘树勋,刘宪民,王维明.钢铁,2005;40(11):67) [8]Llewellyn D T.Mater Sci Technol,1997;13:389 [9]Simmons J W.Acta Mater,1997;45:2467 [10]Mullner P,Solenthaler C,Uggowitzer P,Speidel M O. Mater Sci Eng,1993;A164:164 [11]Soussan A,Degallaix S,Magnin T.Mater Sci Eng,1991; A142:169 [12]Voce E.J lnst Met,1948;74:537 [13]Swift H W.Mech J.Phys Solids,1952;1:1 [14]Ludwigson D C.Metall Trans,1971;2:2825 [15]Gavriljuk V G,Stein G,Berns H.Steel Res,2003;74:444 [16]WeiβS,Dudzinski W,Tikhovskiy I.In:Akdut N,Cooman B C,Foct J.eds.,HNS-2004 Conf Proc,Bad Harzburg: GRIPS media,2004:239 [17]Simmons J W.Acta Mater,1997;45:2467 [18]Mullner P,Solenthaler C,Uggowitzer P,Speidel M O. Mater Sci Eng,1993;A164:164 [19]Gavriljuk V G,Berns H.High Nitrogen Steels.New York: Springer-Verlag,1999:162 [20]Sailer G,Spiradek-Hahn K,Scheu C,Clemens H.Mater Sci Eng,2006;A427:246 [21]Mannan S L,Samuel K G,Rodriguez P.Scr Metall,1982; 16:255 [22]Speidel M O.In:Kamachi M U,Raj Beds.,High Nitrogen Steels and Stainless Steels,New Delhi:Narosa Publishing House,2004:243 [23]Taillard R,Foct J.In:Foct J,Hendry A eds.,HNS-88 Conf Proc,London:The Institute of Metals,1989:387 [24]Gavriljuk V,Petrov Y,Shanina B.Scr Mater,2006;55(6): 537 [25]Stoltz R E,Vander Sande J B.Metall Trans,1980;11A: 1033 [26]Balachandran G.In:Kamachi M U,Raj Beds.,High Nitrogen Steels and Stainless Steels,New Delhi:Narosa Publishing House,2004:74 [27]Vijayalakshmi M,Shankar P,Sudha C.In:Kamachi M U,Raj Beds.,High Nitrogen Steels and Stainless Steels, New Delhi:Narosa Publishing House,2004:125 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|