| A general crystallographic model of fcc/bcc(bct) martensitic nucleation and growth in steels |
| YANG Jinbo; YANG Zhigang; QIU Dong; ZHANG Wenzheng; ZHANG Chi; BAI Bingzhe; FANG Hongsheng |
| Department of Materials Science and Engineering; Tsinghua University; Beijing 100084 |
|
Cite this article:
YANG Jinbo; YANG Zhigang; QIU Dong; ZHANG Wenzheng; ZHANG Chi; BAI Bingzhe; FANG Hongsheng. A general crystallographic model of fcc/bcc(bct) martensitic nucleation and growth in steels. Acta Metall Sin, 2005, 41(3): 225-230 .
|
|
|
Abstract The crystallography of fcc/bcc(bct) martensite transformation,
including nucleation and
growth, has been discussed from the viewpoint of invariant-line
and O-lattice theory. The
formation of martensite is accomplished by the immigration of
well-defined glissile interface
(121)fcc type and its misfit dislocations can produce the lattice
invariant deformation (LID) on the
basis of phenomenal theory of martensitic crystallography (PTMC),
however, LID is retarded
slightly after the migration of interphase (121)fcc,
i.e.a thin plate-like zone exists without LID in
martensite near the well-defined interface.
When the temperature reduces to the Ms point, the lattice parameter of austenite matrix is √3/2 times that of
the martensite without LID. This critical
condition for spontaneous transformation
agrees with that the stack fault energy in matrix is less
than zero according to Olson and Cohen's nucleation model.
|
|
Received: 25 May 2004
|
|
|
[1] Cohen M, Olson G B, Clapp P C. In: Owen W S, Cohen M, Wayman C M, eds., Proc Int Conf on Martensitic Transformations, ICOMAT 79, Cambridge, Mass: MIT Press, 1979: 1 [2] Christian J W. Mater Sci Eng, 1990; A127: 215 [3] Aaronson H I, Hall M G. Metall Mater Trans, 1994; 25A: 1797 [4] Olson G B, Cohen M. Metall Trans, 1976; 7A: 1905 [5] Olson G B, Cohen M. Metall Trans, 1976; 7A: 1915 [6] Bogers A J, Burgers W G. Acta Metall, 1964; 12: 255 [7] Roytburd A L, Khachaturyan A G. Phys Met Metall, 1970; 30: 68 [8] Kurdjumov G V, Khachaturyan A G. Acta Metall, 1975; 23: 1077 [9] Wechsler M S, Lieberman D S, Read T A. Trans AIME, 1953; 197: 1503 [10] Bowles J S, Mackenzie J K. Acta Metall, 1954; 2: 129 [11] Dahmen U, Westmacott K H. In: Aaronson H I, et al, eds., Proc Int Conf on Solid-Solid Phase Transformation, Warrendale, Pa: The Metallurgical Society of AIME, 1981: 433 [12] Dahmen U. Acta Metall, 1982; 30: 63 [13] Luo C P, Weatherly G C. Acta Metall, 1987; 35: 1963 [14] Zhang W Z, Purdy G R. Philos Mag, 1993; 68A: 291 [15] Zhang W Z, Weatherly G C. Acta Mater, 1998; 46: 1837 [16] Qiu D, Zhang W Z. Philos Mag, 2003; 83: 3093 [17] Frank F C. Acta Metall, 1953; 1: 15 [18] Srinivasan G R, Wayman C M. Acta Metall, 1968; 16: 621 [19] Hirth J P, Spanos G, Hall M G, Aaronson H I. Acta Mater, 1998; 46: 857 [20] Liu X, Zhong F, Zhang J X, Zhang M X, Kang M K, Guo Z Q. Phys Rev, 1995; 52B: 9970 [21] Ridley N, Stuart H, Zwell L. TMS AIME, 1969; 245: 1834 [22] Wayman C M. Introduction to the Crystallography of Martensitic Transformations. New York: The MacMil-lan Co., 1964: 146 [23] Greninger A B, Troiano A R. Trans AIME, 1940; 140: 307 [24] Greninger A B, Troiano A R. Trans AIME, 1949; 185: 590 [25] Otte H M, Read T A. Trans AIME, 1957; 209: 412 [26] Johnson K A, Wayman C M. Acta Crystallogr, 1963; 16: 480 [27] Read R P. Acta Metall, 1962; 10: 865 [28] Moritani T, Miyajima N, Furuhara T, Maki T. Scr Mater, 2002; 47: 193 |