| Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature |
LOU Feng1, LIU Ke1( ), LIU Jinxue2, DONG Hanwu3, LI Shubo1, DU Wenbo1 |
1.Faculty of Materials and Manufacturing, Beijing University of Technology, Beijing 100124, China 2.Zhengzhou Light Alloy Institute Co. Ltd., Zhengzhou 450041, China 3.Key Laboratory of Advanced Forming of Metallic Materials, Chongqing Academy of Sciece and Technology, Chongqing 401123, China |
|
Cite this article:
LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature. Acta Metall Sin, 2023, 59(11): 1439-1447.
|
|
|
Abstract As lightweight requirements rise in transportation, aerospace, and other industries, magnesium alloys have a great application prospect. However, the low formability capabilities of magnesium alloys lead to a severe limit in applications. At present, there are many reports on the influences of texture and second phases on the formability of magnesium alloys at room temperature. Nevertheless, the dominant factors affecting the formability performance of magnesium alloys at room temperature are not clear. In this study, the development of the microstructures and texture of Mg-xZn-0.5Er (x = 0.5, 2.0, 3.0, 4.0, mass fraction, %) alloy sheets were studied, and the impact of the texture and second phases on the formability of these sheets were also investigated. The findings showed that the increase in Zn addition led to an early and complete dynamic recrystallization (DRX) in Mg-Zn-Er alloys sheets, and these recrystallized grains would expand significantly during subsequent hot rolling processes. These recrystallized grains with a large size were typically elongated and then helped to create a strong basal texture. Thus, it was discovered that the microstructures of these sheets were typically made up of equiaxed and elongated grains. The formability performance of these sheets was strongly related to the size of the second phases and the texture. The formability of the sheets containing microscopic second phases mainly depended on the basal texture, while the formability of the sheets which contained coarse second phases was mostly influenced by the second phases and basal texture. Particularly, when the component of the coarse second was larger, the formability would get more inferior due to the predominant role of the second phase at room temperature.
|
|
Received: 13 December 2021
|
|
|
| Fund: National Key Research and Development Program of China(2021YFB3701100);Scientific Re-search Institution Performance Incentive and Guidance Special Project of Chongqing(cstc2021jxjl50004);Scientific Re-search Institution Performance Incentive and Guidance Special Project of Chongqing(cstc2021jxjl50004) |
Corresponding Authors:
LIU Ke, associate professor, Tel: (010)67392423, E-mail: lk@bjut.edu.cn
|
| 1 |
You S H, Huang Y D, Kainer K U, et al. Recent research and developments on wrought magnesium alloys [J]. J. Magn. Alloy., 2017, 5: 239
doi: 10.1016/j.jma.2017.09.001
|
| 2 |
Liu X W, Liu Y, Jin B, et al. Microstructure evolution and mechanical properties of a SMATed Mg alloy under in situ SEM tensile testing [J]. J. Mater. Sci. Technol., 2017, 33: 224
doi: 10.1016/j.jmst.2016.11.012
|
| 3 |
Zhang J, Joshi S P. Phenomenological crystal plasticity modeling and detailed micromechanical investigations of pure magnesium [J]. J. Mech. Phys. Solids, 2012, 60: 945
doi: 10.1016/j.jmps.2012.01.005
|
| 4 |
Sabat R K, Brahme A P, Mishra R K, et al. Ductility enhancement in Mg-0.2%Ce alloys [J]. Acta Mater., 2018, 161: 246
doi: 10.1016/j.actamat.2018.09.023
|
| 5 |
Ding W J, Jin L, Wu W X, et al. Texture and texture optimization of wrought Mg alloy [J]. Chin. J. Nonferrous Met., 2011, 21: 2371
|
|
丁文江, 靳 丽, 吴文祥 等. 变形镁合金中的织构及其优化设计 [J]. 中国有色金属学报, 2011, 21: 2371
|
| 6 |
Huang X S, Suzuki K, Chino Y, et al. Influence of aluminum content on the texture and sheet formability of AM series magnesium alloys [J]. Mater. Sci. Eng., 2015, A633: 144
|
| 7 |
Nakata T, Xu C, Ohashi H, et al. New Mg-Al based alloy sheet with good room-temperature stretch formability and tensile properties [J]. Scr. Mater., 2020, 180: 16
doi: 10.1016/j.scriptamat.2020.01.015
|
| 8 |
Wang Q H, Shen Y Q, Jiang B, et al. A good balance between ductility and stretch formability of dilute Mg-Sn-Y sheet at room temperature [J]. Mater. Sci. Eng., 2018, A736: 404
|
| 9 |
Bian M Z, Huang X S, Mabuchi M, et al. Compositional optimization of Mg-Zn-Sc sheet alloys for enhanced room temperature stretch formability [J]. J. Alloys Compd., 2020, 818: 152891
doi: 10.1016/j.jallcom.2019.152891
|
| 10 |
Luo Z P, Zhang S Q, Tang Y L, et al. Thermodynamics of Mg-Zn-RE system solutions forming stable quasicrystals [J]. Scr. Metall. Mater., 1994, 30: 393
doi: 10.1016/0956-716X(94)90592-4
|
| 11 |
Xu D K, Tang W N, Liu L, et al. Effect of W-phase on the mechanical properties of as-cast Mg-Zn-Y-Zr alloys [J]. J. Alloys Compd., 2008, 461: 248
doi: 10.1016/j.jallcom.2007.07.096
|
| 12 |
Kawamura Y, Hayashi K, Inoue A, et al. Rapidly solidified powder metallurgy Mg97Zn1Y2 alloys with excellent tensile yield strength above 600 MPa [J]. Mater. Trans., 2001, 42: 1172
doi: 10.2320/matertrans.42.1172
|
| 13 |
Al-Samman T. Modification of texture and microstructure of magnesium alloy extrusions by particle-stimulated recrystallization [J]. Mater. Sci. Eng., 2013, A560: 561
|
| 14 |
Wang Q F, Du W B, Liu K, et al. Microstructure, texture and mechanical properties of as-extruded Mg-Zn-Er alloys [J]. Mater. Sci. Eng., 2013, A581: 31
|
| 15 |
Meng Y Z, Yu J M, Liu K, et al. The evolution of long-period stacking ordered phase and its effect on dynamic recrystallization in Mg-Gd-Y-Zn-Zr alloy processed by repetitive upsetting-extrusion [J]. J. Alloys Compd., 2020, 828: 154454.
doi: 10.1016/j.jallcom.2020.154454
|
| 16 |
Humphreys F J. Recrystallization mechanisms in two-phase alloys [J]. Met. Sci., 1979, 13: 136
doi: 10.1179/msc.1979.13.3-4.136
|
| 17 |
Lou F, Liu K, Lui J X, et al. Microstructure and formability at room temperature of as-annealing Mg-xZn-0.5Er alloy sheets [J]. Chin. J. Nonferrous Met., 2022, 32: 365
|
|
娄 峰, 刘 轲, 刘金学 等. 退火态Mg-xZn-0.5Er合金板材组织及室温成形性能 [J]. 中国有色金属学报, 2022, 32: 365
|
| 18 |
Kaibyshev R. Dynamic recrystallization in magnesium alloys [A]. Advances in Wrought Magnesium Alloys [M]. Cambridge, UK: Woodhead Publishing, 2012: 186
|
| 19 |
Fatemi-Varzaneh S M, Zarei-Hanzaki A, Beladi H. Dynamic recrystallization in AZ31 magnesium alloy [J]. Mater. Sci. Eng., 2007, A456: 52
|
| 20 |
Al-Samman T, Gottstein G. Dynamic recrystallization during high temperature deformation of magnesium [J]. Mater. Sci. Eng., 2008, A490: 411
|
| 21 |
Vaughan M W, Nasim W, Dogan E, et al. Interplay between the effects of deformation mechanisms and dynamic recrystallization on the failure of Mg-3Al-1Zn [J]. Acta Mater., 2019, 168: 448
doi: 10.1016/j.actamat.2019.02.010
|
| 22 |
Chino Y, Huang X S, Suzuki K, et al. Influence of Zn concentration on stretch formability at room temperature of Mg-Zn-Ce alloy [J]. Mater. Sci. Eng., 2010, A528: 566
|
| 23 |
Liu K, Lou F, Fu J J, et al. Microstructure and corrosion behaviors of as-rolled Mg-Zn-Er alloy sheets [J]. Trans. Nonferrous Met. Soc. China, 2022, 32: 1881
doi: 10.1016/S1003-6326(22)65915-6
|
| 24 |
Liu K, Sun C C, Wang Z H, et al. Microstructure, texture and mechanical properties of Mg-Zn-Er alloys containing I-phase and W-phase simultaneously [J]. J. Alloys Compd., 2016, 665: 76
doi: 10.1016/j.jallcom.2015.10.262
|
| 25 |
Qin D H, Wang M J, Sun C Y, et al. Interaction between texture evolution and dynamic recrystallization of extruded AZ80 magnesium alloy during hot deformation [J]. Mater. Sci. Eng., 2020, A788: 139537
|
| 26 |
Suh B C, Kim J H, Hwang J H, et al. Twinning-mediated formability in Mg alloys [J]. Sci. Rep., 2016, 6: 22364
doi: 10.1038/srep22364
|
| 27 |
Robson J D, Henry D T, Davis B. Particle effects on recrystallization in magnesium-manganese alloys: Particle-stimulated nucleation [J]. Acta Mater., 2009, 57: 2739
doi: 10.1016/j.actamat.2009.02.032
|
| 28 |
Robson J D, Henry D T, Davis B. Particle effects on recrystallization in magnesium-manganese alloys: Particle pinning [J]. Mater. Sci. Eng., 2011, A528: 4239
|
| 29 |
Liu P, Jiang H T, Duan X G, et al. Effects of yttrium (Y) and cerium (Ce) on microstructure and stretch formability of hot rolled Mg-1.5Zn magnesium sheet at room temperature [J]. J. Mater Eng., 2014, (12): 1
|
|
刘 鹏, 江海涛, 段晓鸽 等. 稀土元素Y和Ce对热轧Mg-1.5Zn镁合金组织和室温成形性能的影响 [J]. 材料工程, 2014, (12): 1
|
| 30 |
Cai Z X, Tang D, Jiang H T, et al. Influence of Gd concentration on texture and stretch formability of rolled Mg-Zn-Gd alloys at room temperature [J]. Rare Met. Mater. Eng., 2013, 42: 2073
|
|
蔡正旭, 唐 荻, 江海涛 等. 不同Gd含量对变形Mg-Zn-Gd合金织构和室温成形性能的影响 [J]. 稀有金属材料与工程, 2013, 42: 2073
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|