Investigation of In Situ 1150 ℃ High Temperature Deformation Behavior and Fracture Mechanism of a Second Generation Single Crystal Superalloy
Jinyao MA1,Jin WANG1,Yunsong ZHAO3,Jian ZHANG3,Yuefei ZHANG1(),Jixue LI2,Ze ZHANG2
1. Institute of Microstructure and Property of Advanced Materials, Beijing University of Technology, Beijing 100124, China
2. School of Materials Science and Engineering, Zhejiang University, Hangzhou 310027, China
3. Key Laboratory of Advanced High Temperature Structural Materials, AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China
Cite this article: 

Jinyao MA,Jin WANG,Yunsong ZHAO,Jian ZHANG,Yuefei ZHANG,Jixue LI,Ze ZHANG. Investigation of In Situ 1150 ℃ High Temperature Deformation Behavior and Fracture Mechanism of a Second Generation Single Crystal Superalloy. Acta Metall Sin, 2019, 55(8): 987-996.

Download:  HTML  PDF(26817KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Single-crystal superalloy is the key material of turbine blade and hot end parts in aerospace field. The second generation nickel-based single crystal superalloy has been widely used because of its low cost and excellent high temperature properties. At present, the research on microstructure of superalloys at high temperature mainly depends on SEM and TEM observation after heating and loading experiment. However, such kind of work lacks real-time characterization capabilities. Carrying out in situ experiments has an important significance for understanding the real time deformation behavior and microstructure evolution of superalloys. Therefore, the development of an in situ high temperature (above 1000 ℃) mechanical testing equipment for SEM faces huge challenges. In this work, high temperature tensile experiment at 1150 ℃ of a second generation single crystal nickel-based superalloy were carried out by means of a self-developed in situ heating tensile platform which can used in SEM. A high quality experimental data and serial SEM images were obtained in the course of tensile testing at 1150 ℃. The analysis of force-displacement curve shows that the yield strength and fracture strength of the specimen are 580 and 620 MPa, respectively. The sequential SEM images during this research confirm that there is no obvious shape and size change for γ and γ′ during the elastic deformation, and microstructure changing during plastic stage is mainly due to γ phase widening which is parallel to the stress axis. The results show that the original micro-voids of samples are the weakness in high temperature tensile test at 1150 ℃, the fracture direction is almost perpendicular to the stress axis, the crack propagated by passing the γ′ phase and through in the γ phase, and ultimately, temperature and stress induced adjacent holes connection leading to the sample fracture.

Key words:  nickel-based single crystal superalloy      in situ SEM      high temperature tensile      microstructure      crack     
Received:  16 January 2019     
ZTFLH:  TG132.3  
Fund: Supported by Foundation:National Key Scientific Instrument and Equipment Development Project(No.11327901)

URL: 

https://www.ams.org.cn/EN/10.11900/0412.1961.2019.00013     OR     https://www.ams.org.cn/EN/Y2019/V55/I8/987

Fig.1  Dimension of in situ SEM heating tensile specimen (unit: mm)
Fig.2  Heating and tensile platform combined with SEM (a) and schematic of heating tensile stage (b)
Fig.3  Over field image of stretch gauge segment (a), composed of γ/γ' microstructure (b), micro pores and small amounts of eutectic structure and inclusion shedding caused holes (c), EDS surface distribution of the rectangular area in Fig.3b (d) (σ—relative standard deviation, w—mass fraction)
Fig.4  Temperature vs voltage curves at samples, force and displacement sensors (Inset shows the local magnification of curves)
Fig.5  Microstructure of nickel-based single crystal superalloy during heating process at 750 ℃ (a), 950 ℃ (b), 1050 ℃ (c), 1150 ℃ (d) and CCD images of in situ tensile stage (e~h) separately corresponding to Figs.5a~d
Fig.6  In situ tensile force-displacement curve of nickel-based single crystal superalloy sample at 1150 ℃
Fig.7  In situ observation of micro hole initiation and sample deformation process under different loading conditions
Fig.8  Evolution process of micro hole on sample surface during tensile yield stage at 1150 ℃ and 620 MPa
Fig.9  SEM images of microstructure at about 500 μm away from fracture surface (a) and near fracture location (b) of nickel-based single crystal superalloy
Fig.10  Crack propagation of nickel-based single crystal superalloy at 600 MPa (a), morphology at 580 MPa corresponding to region I (b), carbides in porous cavities in region II (c), morphology evolution of Fig.10a at 530 MPa (d), and crack propagation between micropores at 500 MPa at different magnification (e, f)
Fig.11  Fractograph of the specimen after high temperature tension at 1150 ℃ (a), regions A and B corresponding to crack source and crack propagation zone respectively, and boxes 1 and 2 in area B showing the microspores (b), and dimples and cleavage plane characteristics of areas I (c) and II (d) on cross section
[1] Guo J T. Materials Science and Engineering for Superalloys (Book 1) [M]. Beijing: Science Press, 2008: 182
[1] (郭建亭. 高温合金材料学(上册) [M]. 北京: 科学出版社, 2008: 182)
[2] Chen R Z. Development status of single crystal superalloys [J]. J. Mater. Eng., 1995, (8): 3
[2] (陈荣章. 单晶高温合金发展现状 [J]. 材料工程, 1995, (8): 3)
[3] Yu J, Li J R, Shi Z X, et al. Tensile behavior and deformation mechanism of single crystal superalloy DD6 at 760 ℃ and 1070 ℃ [J]. J. Aeronaut. Mater., 2015, 35(5): 13
[3] (喻 健, 李嘉荣, 史振学等. DD6单晶高温合金760 ℃和1070 ℃拉伸行为与变形机制 [J]. 航空材料学报, 2015, 35(5): 13)
[4] Li J R, Jin H P, Liu S. Stress rupture properties and microstructures of the second generation single crystal superalloy DD6 after long term aging at 980 ℃ [J]. Rare Met. Mater. Eng., 2007, 36: 1784
[5] Roebuck B, Cox D, Reed R. The temperature dependence of γ′ volume fraction in a Ni-based single crystal superalloy from resistivity measurements [J]. Scr. Mater., 2001, 44: 917
[6] Tang Y, Ming H, Xiong J, et al. Evolution of superdislocation structures during tertiary creep of a nickel-based single-crystal superalloy at high temperature and low stress [J]. Acta Mater., 2017, 126: 336
[7] Al-Jarba K A, Fuchs G E. Effect of carbon additions on the as-cast microstructure and defect formation of a single crystal Ni-based superalloy [J]. Mater. Sci. Eng., 2004, A373: 255
[8] Li T R, Liu G H, Xu M, et al. Microstructures and high temperature tensile properties of Ti-43Al-4Nb-1.5Mo alloy in the canned forging and heat treatment process [J]. Acta Metall. Sin., 2017, 53: 1055
[8] (李天瑞, 刘国怀, 徐 莽等. Ti-43Al-4Nb-1.5Mo合金包套锻造与热处理过程的微观组织及高温拉伸性能 [J]. 金属学报, 2017, 53: 1055)
[9] Zhang S C, Li X D, Yu H C, et al. Low cycle fatigue of single crystal nickel-based superalloy DD6 at 1100 ℃ [J]. J. Aeronaut. Mater., 2018, 38(1): 95
[9] (张仕朝, 李旭东, 于慧臣等. DD6合金1100℃低周疲劳行为 [J]. 航空材料学报, 2018, 38(1): 95)
[10] Baik S I, Rawlings M J S, Dunand D C. Effect of hafnium micro-addition on precipitate microstructure and creep properties of a Fe-Ni-Al-Cr-Ti ferritic superalloy [J]. Acta Mater., 2018, 153: 126.
[11] Chen J Y, Zhao B, Feng Q, et al. Effects of Ru and Cr on γ/γ' microstructural evolution of Ni-based single crystal superalloys during heat treatment [J]. Acta Metall. Sin., 2010, 46: 897
[11] (陈晶阳, 赵 宾, 冯 强等. Ru和Cr对镍基单晶高温合金γ/γ'热处理组织演变的影响 [J]. 金属学报, 2010, 46: 897)
[12] Nganbe M, Heilmaier M. Modelling of particle strengthening in the γ' and oxide dispersion strengthened nickel-base superalloy PM3030 [J]. Mater. Sci. Eng., 2004, A387-389: 609
[13] Wang K G, Li J R, Liu S Z, et al. Study on creep properties of single crystal superalloy DD6 at 760 ℃ [J]. J. Mater. Eng., 2004, (5): 7
[13] (王开国, 李嘉荣, 刘世忠等. DD6单晶高温合金760 ℃的蠕变性能研究 [J]. 材料工程, 2004, (5): 7)
[14] Murakumo T, Kobayashi T, Koizumi Y, et al. Creep behaviour of Ni-base single-crystal superalloys with various γ' volume fraction [J]. Acta Mater., 2004, 52: 3737
[15] Shi Z X, Li J R, Liu S Z, et al. Transverse tensile properties and fracture behaviour of DD6 single crystal superalloy [J]. J. Aeronaut. Mater., 2009, 29(2): 101
[15] (史振学, 李嘉荣, 刘世忠等. DD6单晶高温合金横向拉伸性能及其断裂行为 [J]. 航空材料学报, 2009, 29(2): 101)
[16] Shi Z X, Liu S Z, Xiong J C, et al. Microstructure evolution behavior of DD6 single crystal superalloy at different using temperatures [J]. Chin. J. Nonferrous Met., 2015, 25: 3077
[16] (史振学, 刘世忠, 熊继春等. 不同使用温度下DD6单晶高温合金的组织演变行为 [J]. 中国有色金属学报, 2015, 25: 3077)
[17] Wang J J, Guo W G, Li P H, et al. Dynamic tensile properties of a single crystal nickel-base superalloy at high temperatures measured with an improved SHTB technique [J]. Mater. Sci. Eng., 2016, A670: 1
[18] Zhao J Q, Li J R, Liu S Z, et al. Effects of low angle grain boundaries on stress rupture properties of single crystal superalloy DD6 [J]. J. Aeronaut. Mater., 2007, 27(6): 6
[18] (赵金乾, 李嘉荣, 刘世忠等. 小角度晶界对单晶高温合金DD6持久性能的影响 [J]. 航空材料学报, 2007, 27(6): 6)
[19] Qin J C, Cui R J, Huang Z H, et al. Effect of low angle grain boundaries on mechanical properties of DD5 single crystal Ni-base superalloy [J]. J. Aeronaut. Mater., 2017, 37(3): 24
[19] (秦健朝, 崔仁杰, 黄朝晖等. 小角度晶界对DD5镍基单晶高温合金力学性能的影响 [J]. 航空材料学报, 2017, 37(3): 24)
[20] Hemmersmeier U, Feller-Kniepmeier M. Element distribution in the macro- and microstructure of nickel base superalloy CMSX-4 [J]. Mater. Sci. Eng., 1998, A248: 87
[21] Zhang S M, Yu J G, Huang Z Y, et al. Directional migration behavior of alloying elements in the rafting process of the single crystal superalloy DD6 [J]. Rare Met. Mater. Eng., 2016, 45: 1147
[22] Wheeler J M, Armstrong D E J, Heinz W, et al. High temperature nanoindentation: The state of the art and future challenges [J]. Curr. Opin. Solid State Mater. Sci., 2015, 19: 354
[23] Zhang W J, Song X Y, Hui S X, et al. In-situ SEM observations of fracture behavior of BT25y alloy during tensile process at different temperature [J]. Mater. Des., 2017, 116: 638
[24] Wang J, Zhang Y F, Ma J Y, et al. Microcrack nucleation and propagation investigation of Inconel 740H alloy under in situ high temperature tensile test [J]. Acta Metall. Sin., 2017, 53: 1627
[24] (王 晋, 张跃飞, 马晋遥等. Inconel740H合金原位高温拉伸微裂纹萌生扩展研究 [J]. 金属学报, 2017, 53: 1627)
[25] Liang J C, Wang Z, Xie H F, et al. In situ scanning electron microscopy-based high-temperature deformation measurement of nickel-based single crystal superalloy up to 800 ℃ [J]. Opt. Lasers Eng., 2018, 108: 1
[26] Bokstein B S, Epishin A I, Link T, et al. Model for the porosity growth in single-crystal nickel-base superalloys during homogenization [J]. Scr. Mater., 2007, 57: 801
[27] Chen Q Z, Kong Y H, Jones C N, et al. Porosity reduction by minor additions in RR2086 superalloy [J]. Scr. Mater., 2004, 51: 155
[28] Wang G L, Liu J L, Liu J D, et al. Temperature dependence of tensile behavior and deformation microstructure of a Re-containing Ni-base single crystal superalloy [J]. Mater. Des., 2017, 130: 131
[29] Luo Z P, Wu Z T, Miller D J. The dislocation microstructure of a nickel-base single-crystal superalloy after tensile fracture [J]. Mater. Sci. Eng., 2003, A354: 358
[30] Zhang L, Zhao L G, Roy A, et al. In-situ SEM study of slip-controlled short-crack growth in single-crystal nickel superalloy [J]. Mater. Sci. Eng., 2019, A742: 564
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[3] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[5] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[6] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[7] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[8] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[9] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[10] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[11] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[12] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[13] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[14] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[15] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
No Suggested Reading articles found!