| Recrystallization Mechanisms in Hot Working Processes of a Nickel-Based Alloy for Ultra-Supercritical Power Plant Application |
Kang WEI, Maicang ZHANG( ), Xishan XIE |
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China |
|
Cite this article:
Kang WEI, Maicang ZHANG, Xishan XIE. Recrystallization Mechanisms in Hot Working Processes of a Nickel-Based Alloy for Ultra-Supercritical Power Plant Application. Acta Metall Sin, 2017, 53(12): 1611-1619.
|
|
|
Abstract Nickel-based alloy is a good choice for materials used in ultra-supercritical power plant, which is subjected to high temperature about 700 ℃ and high pressure in service. In order to meet the requirements above, a nickel-based alloy was designed and the tubes were successfully manufactured. Based on the hot/cold working processes of tube components of the nickel-based alloy, microstructural evolution, especially the recrystallization mechanisms during hot working processes of the alloy were systematically investigated by using a series of hot compression tests, solution annealing tests, OM and TEM analyses. The results showed that dynamic recrystallization was dominated by discontinuous dynamic recrystallization mechanism involving grain boundary bulging, whereas the nucleation mechanism with strain inducing grain boundary migration was the driving force of static recrystallization. In addition, the essence of different forms of step grain boundary producing during dynamic recrystallization and static recrystallization was to make the surface deviate from low index surface, which could ensure more interface to be low energy close-packed surface, so that the energy of grain boundary interface would be reduced. The morphology of step grain boundary depended on the crystallographic relationship of crystal interface and the Burgers vector of grain boundary dislocation. Moreover, the presence of step grain boundary could also promote grain boundary migration and accelerate the recrystallization process. When the recrystallization process was completed, step grain boundaries still remained partially to minimize interfacial energy and continue to promote subsequent grain growth processes.
|
|
Received: 16 January 2017
|
|
|
| [1] | Guo J T.Materials Science and Engineering for Superalloys [M]. Vol.1, Beijing: Science Press, 2008: 1(郭建亭. 高温合金材料学 [M]. 上册, 北京: 科学出版社, 2008: 1) | | [2] | Doherty R D, Hughes D A, Humphreys F J, et al.Current issues in recrystallization: A review[J]. Mater. Sci. Eng., 1997, A238: 219 | | [3] | Humphreys F J, Hatherly M.Recrystallization and Related Annealing Phenomena[M]. 2nd Ed., Amsterdam: Elsevier, 2004: 169 | | [4] | Zahiri S H, Hodgson P D.The static, dynamic and metadynamic recrystallisation of a medium carbon steel[J]. Mater. Sci. Technol., 2004, 20: 458 | | [5] | Sakai T, Belyakov A, Kaibyshev R, et al.Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions[J]. Prog. Mater. Sci., 2014, 60: 130 | | [6] | Singh R P, Hyzak J M, Howson T E, et al.Recrystallization behavior of cold rolled alloy 718 [A]. Superalloys 718, 625 and Various Derivatives[C]. Warrendale, PA: TMS, 1991: 205 | | [7] | Wang L, Wang S A, Liu Y, et al. Dynamic recrystallization behavior of GH4586 superalloy during hot compression [J]. Mater. Sci. Forum, 2010, 638-642: 2357 | | [8] | Liu Y X, Lin Y, Li H B, et al.Study of dynamic recrystallization in a Ni-based superalloy by experiments and cellular automaton model[J]. Mater. Sci. Eng., 2015, A626: 432 | | [9] | Lin Y C, Liu Y X, Chen M S, et al.Study of static recrystallization behavior in hot deformed Ni-based superalloy using cellular automaton model[J]. Mater. Des., 2016, 99: 107 | | [10] | Hirth J P, Pond R C.Steps, dislocations and disconnections as interface defects relating to structure and phase transformations[J]. Acta. Mater., 1996, 44: 4749 | | [11] | Smith W F, Hashemi J.Foundations of Materials Science and Engineering[M]. 5th Ed., New York: McGraw-Hill Education, 2011: 138 | | [12] | Shirdel M, Mirzadeh H, Parsa M H.Abnormal grain growth in AISI 304L stainless steel[J]. Mater. Charact., 2014, 97: 11 | | [13] | Danflou H L, Macia M, Sanders T H, et al.Mechanisms of formation of serrated grain boundaries in nickel base superalloys [A]. Superalloys 1996[C]. Warrendale, PA: TMS, 1996: 119 | | [14] | Kim K J, Ginsztler J, Nam S W.The role of carbon on the occurrence of grain boundary serration in an AISI 316 stainless steel during aging heat treatment[J]. Mater. Lett., 2005, 59: 1439 | | [15] | Kim K J, Hong H U, Nam S W.A study on the mechanism of serrated grain boundary formation in an austenitic stainless steel[J]. Mater. Chem. Phys., 2011, 126: 480 | | [16] | Hong H U, Kim I S, Choi B G, et al.On the mechanism of serrated grain boundary formation in Ni-based superalloys with low γ′ volume fraction [A]. Superalloys 2012[C]. Warrendale, PA: TMS, 2012: 53 | | [17] | Hong H U, Jeong H W, Kim I S, et al.Significant decrease in interfacial energy of grain boundary through serrated grain boundary transition[J]. Philo. Mag., 2012, 92: 2809 | | [18] | Jiang L, Hu R, Kou H C, et al.The effect of M23C6 carbides on the formation of grain boundary serrations in a wrought Ni-based superalloy[J]. Mater. Sci. Eng., 2012, A536: 37 | | [19] | Lim Y S, Kim D J, Hwang S S, et al.M23C6 precipitation behavior and grain boundary serration in Ni-based alloy 690[J]. Mater. Charact., 2014, 96: 28 | | [20] | Wu Y S, Zhang M C, Xie X S.The design and research of a new low cobalt-molybdenum niobium-containing Ni-base superalloy for 700 ℃ advanced ultra-supercritical power plants[J]. Proc. Eng., 2015, 130: 617 | | [21] | Xie X S, Wu Y S, Chi C Y, et al.Superalloys for advanced ultra-super-critical fossil power plant application [A]. Superalloys[M]. Rijeka: InTech, 2015: 51 | | [22] | Li D F, Guo Q M, Guo S L, et al.The microstructure evolution and nucleation mechanisms of dynamic recrystallization in hot-deformed Inconel 625 superalloy[J]. Mater. Des., 2011, 32: 696 | | [23] | Cao Y, Di H S, Zhang J Q, et al.An electron backscattered diffraction study on the dynamic recrystallization behavior of a nickel-chromium alloy (800H) during hot deformation[J]. Mater. Sci. Eng., 2013, A585: 71 | | [24] | Gleiter H.The mechanism of grain boundary migration[J]. Acta Metall., 1969, 17: 565 | | [25] | Gleiter H.Theory of grain boundary migration rate[J]. Acta Metall., 1969, 17: 853 | | [26] | Rae C M F, Smith D A. On the mechanisms of grain boundary migration[J]. Philos. Mag., 1980, 41A: 477 | | [27] | Rajabzadeh A, Legros M, Combe N, et al.Evidence of grain boundary dislocation step motion associated to shear-coupled grain boundary migration[J]. Philos. Mag., 2013, 93: 1299 | | [28] | Bowers M L, Ophus C, Gautam A, et al.Step coalescence by collective motion at an incommensurate grain boundary[J]. Phys. Rev. Lett., 2016, 116: 106102 |
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|