1 Wedge Central South Research Institute, Shenzhen 518045, China 2 Foundry Institute, RWTH Aachen University, Aachen 52072, Germany 3 Energy Conversion R&D Center, Central Academy, Dongfang Electric Co., Chengdu 611731, China 4 State Key Laborotory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China |
|
Cite this article:
Dexin MA, Fu WANG, Xuhui WEN, Dejian SUN, Lin LIU. Influence of MC Carbides on the Formation of γ/γ′ Eutectics in Single Crystal Superalloy CM247LC. Acta Metall Sin, 2017, 53(12): 1603-1610.
|
Abstract The structure formation of superalloys is very complicated because of their multicomponent composition and multiphase transition processing. Duo to the limitation of some pre-conditions, the structure formation can not be accurately determined by thermodynamic calculation method. Knowledge about the structure is critical for the design of the following heat treatment process. In this work, a single crystal (SC) sample of superalloy CM247LC was directional solidified in a labor Bridgman furnace with a pulling rate of 0.2 mm/min and then water quenched, to investigate the solidification sequence including MC carbide and γ/γ′-eutectic. It was observed that the γ-phase is firstly formed in the form of dendrites; it is then followed by the homogeneously precipitation of MC carbides from the liquid behind dendrite tips. Near the end of solidification the interdendritic residual liquid transits into γ/γ′-eutectics. It is interesting to found that the γ/γ′ eutectics do not nucleate on the existing γ -phase, but preferably on the MC carbides which have completely different chemical composition and crystal structure. The result of EBSD examination indicates that the γ/γ′ eutectics formed on the MC substrates have random crystal orientations compared to the SC γ -matrix, exhibiting the misoriented multi-crystal microstructure in the so called "single crystal" superalloy casting.
|
Received: 05 April 2017
|
|
Fund: Supported by National Natural Science Foundation of China (Nos.51331005, 51690163 and 51631008), National Key Research and Development Program (No.2016YFB0701405) and Science and Technology Innovation Commission of Shenzhen Municipality (No.JSGG20150731142227736) |
[1] | Yukawa N, Murata Y, Noda T.Analysis of solidification behavior and alloy design of a nickel-base superalloy, IN-100 [A]. Superalloys 1984[C]. Warrendale: TMS, 1984: 83 | [2] | He L Z, Zheng Q, Sun X F, et al.Effect of carbides on the creep properties of a Ni-base superalloy M963[J]. Mater. Sci. Eng., 2005, A397: 297 | [3] | Yang J X, Zheng Q, Sun X F, et al.Topologically close-packed phase precipitation in a nickel-base superalloy during thermal exposure[J]. Mater. Sci. Eng., 2007, A465: 100 | [4] | Harris K, Erickson G L. Single crystal (single grain) alloy [P]. US Pat, 4582548, 1986 | [5] | Ross E W, Wukusick C S, King W T. Nickel-based superalloys for producing single crystal articles having improved tolerance to low angle grain boundaries [P]. US Pat, 5399313, 1995 | [6] | Wasson A J, Fuchs G E.Microstructural evolution of a carbon modified single crystal Ni-base superalloy[J]. Mater. Charact., 2012, 74: 11 | [7] | Mihalisin J R, Corrigan J, Baker R J, et al. Clean single crystal nickel base superalloy [P]. US Pat, 5549765, 1996 | [8] | Tin S, Pollock T M, Murphy W.Stabilization of thermosolutal convective instabilities in Ni-based single-crystal superalloys: Carbon additions and freckle formation[J]. Metall. Mater. Trans., 2001, 32A: 1743 | [9] | Cutler E R, Wasson A J, Fuch G E.Effect of minor alloying additions on the solidification of single-crystal Ni-base superalloys[J]. J. Cryst. Growth, 2009, 311: 3753 | [10] | Tin S, Pollock T M, King W T.Carbon additions and grain defect formation in high refractory nickel-base single crystal superalloy [A]. Superalloys 2000[C]. Warrendale: TMS, 2000: 201 | [11] | Tin S, Pollock T M.Stabilization of thermosolutal convective instabilities in Ni-based single-crystal superalloys: Carbide precipitation and Rayleigh numbers[J]. Metall. Mater. Trans., 2003, 34A: 1953 | [12] | Liu L, Fu H Z, Shi Z X.Relationship between primary morphology and crystal structure of carbides growing in superalloys[J]. Acta Metall. Sin.(Engl. Ed.), 1990, 3: 46 | [13] | Liu L, Sommer F, Fu H Z.Effect of solidification conditions on MC carbides in a Nickel-base superalloy in IN 738-LC[J]. Scr. Metall. Mater., 1994, 30: 587 | [14] | Chen J, Lee J H, Jo C Y, et al.MC carbide formation in directionally solidified MAR-M247 LC superalloy[J]. Mater. Sci. Eng., 1998, A247: 113 | [15] | Sun W R, Lee J H, Seo S M, et al.The eutectic characteristic of MC-type carbide precipitation in a DS nickel-base superalloy[J]. Mater. Sci. Eng., 1999, A271: 143 | [16] | Chen J, Huang B Y, Lee J H, et al.Carbide formation process in directionally solidified MAR-M247 LC superalloy[J]. J. Mater. Sci. Technol., 1999, 15: 48 | [17] | Huang H E, Koo C H.Characteristics and mechanical properties of polycrystalline CM 247 LC superalloy casting[J]. Mater. Trans., 2004, 45: 562 | [18] | Szczotok A, Rodak K.Microstructural studies of carbides in MAR-M247 nickel-based superalloy[J]. IOP Conf. Ser.: Mater. Sci. Eng., 2012, 35: 012006 | [19] | D'Souza N, Dong H B. Solidification path in third-generation Ni-based superalloys, with an emphasis on last stage solidification[J]. Scr. Mater., 2007, 56: 41 | [20] | Liang Y J, Li J, Li A, et al.Solidification path of single-crystal nickel-base superalloys with minor carbon additions under laser rapid directional solidification conditions[J]. Scr. Mater., 2017, 127: 58 | [21] | Durand-Charre M, translated by Davidson J H. The Microstructure of Superalloys[M]. Amsterdam: Gordon and Breach Science Publishers, 1997: 30 | [22] | Zou J, Wang H P, Doherty R, et al.Solidification behavior and microstructure formation in a cast Nickel based superalloy: Experiment and modeling [A]. Superalloys 1992[C]. Warrendale: TMS, 1992: 165 | [23] | D'Souza N D, Dong H B. An analysis of solidification path in the Ni-base superalloy, CMSX10K [A]. Superalloys 2008[C]. Warrendale: TMS, 2008: 261 | [24] | Zou J, Wang H P, Doherty R, et al.Solidification behavior and microstructure formation in a cast nickel based superalloy: Experiment and modeling [A]. Superalloys 1992[C]. Warrendale: TMS, 1992: 165 | [25] | Warnken N, Ma D, Mathes M, et al. Investigation of eutectic island formation in SX superalloys [J]. Mater. Sci. Eng., 2005, A413-414: 267 |
|
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|