					Cite this article:
						|  |  
    					|  |  
    					| Effect of Heat Treatment on Microstructure and Mechanical Properties of Consecutive Point-Mode Forging and Laser Rapid Forming GH4169 Alloy |  
						| Mingzhe XI(  ),Wei ZHOU,Junying SHANG,Chao LV,Zhenhao WU,Shiyou GAO |  
						| Key Laboratory of Advanced Forging & Stamping Technology and Science, Ministry of Education, Yanshan University, Qinhuangdao 066004, China |  
						|  |  
					
			      Mingzhe XI,Wei ZHOU,Junying SHANG,Chao LV,Zhenhao WU,Shiyou GAO. Effect of Heat Treatment on Microstructure and Mechanical Properties of Consecutive Point-Mode Forging and Laser Rapid Forming GH4169 Alloy. Acta Metall Sin, 2017, 53(2): 239-247.	
				 
					
						| 
								
									|  
          
          
            
              
				
												  
													
													    |  |  
														| Abstract To transform the columnar grain in the as-deposited GH4169 alloy to the exquiaxed grain and get better mechanical properties, a block sample of GH4169 alloy has been formed by using a technology of consecutive point-mode forging and laser rapid forming (CPF-LRF). During the process of CPF-LRF, GH4169 alloy was deposited by laser rapid forming firstly and then the deposited GH4169 alloy was deformed by consecutive point-mode forging. Both consecutive point-mode forging and laser rapid forming were alternately carried out until the completion of the forming of an objective part. The effects of heat treatment on the microstructures and mechanical properties of CPF-LRF GH4169 alloy have been investigated. The result shows that 980STA heat treatment fails to lead to recrystallization of CPF-LRF GH4169 alloy, and the tensile properties of 980STAed CPF-LRF GH4169 alloy can't meet the wrought standards. After the 1020STA heat treatment, the average recrystal grain size of GH4169 alloy is about 12.8 μm, and Laves phase can not be dissolved completely. The tensile properties of the 1020STAed CPF-LRF GH4169 alloy is superior to the wrought standards. Compared to the 1020STAed CPF-LRF GH4169 alloy, the tensile strength of 1050STAed CPF-LRF GH4169 alloy drops and its ductility increases due to complete dissolution of Laves phase and grain size increasing to 25.3 μm. The average grain size of the 1080STAed CPF-LRF GH4169 alloy is about 123.6 μm. Compared to 1020STAed and 1050STAed CPF-LRF GH4169, the tensile properties of 1080STAed CPF-LRF GH4169 has fallen substantially, which just satisfy the wrought standards. |  
															| Received:  02 August 2016 |  
															| Fund: Supported by National Natural Science Foundation of China (Nos.51375426 and 51375245) |  
            
									            
									               
																												  
															| | [1] | Mei Y P, Liu Y C, Liu C X, et al.Effects of cold rolling on the precipitation kinetics and the morphology evolution of intermediate phases in Inconel 718 alloy[J]. J. Alloys Compd., 2015, 649: 949 |  | [2] | Chang L T, Sun W R, Cui Y Y, et al.Effect of heat treatment on microstructure and mechanical properties of the hot-isostatic-pressed Inconel 718 powder compact[J]. J. Alloys Compd., 2014, 590: 227 |  | [3] | Lambarrin J, Leunda J, Navas V G, et al.Microstructural and tensile characterization of Inconel 718 laser coatings for aeronautic components[J]. Opt. Laser. Eng., 2013, 51: 813 |  | [4] | Zhang Q L, Yao J H, Mazumder J.Laser direct metal deposition technology and microstructure and composition segregation of Inconel 718 superalloy[J]. J. Iron Steel Res. Int., 2011, 18: 73 |  | [5] | Chang L T, Sun W R, Cu Y Y, et al.Influences of hot-isostatic-pressing temperature on microstructure, tensile properties and tensile fracture mode of Inconel 718 powder compact[J]. Mater. Sci. Eng., 2014, A599: 186 |  | [6] | Mei Y P, Liu Y C, Liu C X, et al.Effects of cold rolling on the precipitation kinetics and the morphology evolution of intermediate phases in Inconel 718 alloy[J]. J. Alloys Compd., 2015, 649: 949 |  | [7] | Rao G A, Srinivas M, Sarma D S.Effect of thermomechanical working on the microstructure and mechanical properties of hot isostatically pressed superalloy Inconel 718[J]. Mater. Sci. Eng., 2004, A383: 201 |  | [8] | Wang Y D, Tang H B, Fang Y L, et al.Effect of heat treatment on microstructure and mechanical properties of laser melting deposited 1Cr12Ni2WMoVNb steel[J]. Mater. Sci. Eng., 2010, A528: 474 |  | [9] | Zhang Q, Chen J, Lin X, et al.Grain morphology control and texture characterization of laser solid Formed Ti6Al2Sn2Zr3Mo1.5Cr2Nb titanium alloy[J]. J. Mater. Process. Technol., 2016, 238: 202 |  | [10] | Wang Y D, Tang H B, Fang Y L, et al.Microstructure and mechanical properties of laser melting deposited 1Cr12Ni2WMoVNb steel[J]. Mater. Sci. Eng., 2010, A527: 4804 |  | [11] | Zhu Y Y, Liu D, Tian X J, et al.Characterization of microstructure and mechanical properties of laser melting deposited Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy[J]. Mater. Des., 2014, 56: 445 |  | [12] | Zhu Y Y, Li J, Tian X J, et al.Microstructure and mechanical properties of hybrid fabricated Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy by laser additive manufacturing[J]. Mater. Sci. Eng., 2014, A607: 427 |  | [13] | Liu C M, Wang H M, Tian X J, et al.Microstructure and tensile properties of laser melting deposited Ti-5Al-5Mo-5V-1Cr-1Fe near β titanium alloy[J]. Mater. Sci. Eng., 2013, A586: 323 |  | [14] | Liu F C, Lin X, Huang C P, et al.The effect of laser scanning path on microstructures and mechanical properties of laser solid formed nickel-base superalloy Inconel 718[J]. J. Alloys Compd., 2011, 509: 4505 |  | [15] | Liu F C, Lin X, Yang G L, et al.Microstructure and residual stress of laser rapid formed Inconel 718 nickel-base superalloy[J]. Opt. Laser Technol., 2011, 43: 208 |  | [16] | Liu F C, Lin X, Zhao W W, et al.Effects of solution treatment temperature on microstructures and properties of laser solid forming GH4169 superalloy[J]. Rare Met. Mater. Eng., 2010, 39: 1519 |  | [17] | Liu F C, Lin X, Yang G L, et al.Microstructures and mechanical properties of laser solid formed nickle base superalloy Inconel 718 prepared in different atmospheres[J]. Acta Metall. Sin., 2010, 46: 1047 |  | [17] | (刘奋成, 林鑫, 杨高林等. 不同气氛激光立体成形镍基高温合金Inconel 718的显微组织和力学性能[J]. 金属学报, 2010, 46: 1047) |  | [18] | Zhao W W, Lin X, Liu F C, et al.Effect of heat treatment on microstructure and mechanical properties of laser solid forming Inconel 718 superalloy[J]. Chin. J. Lasers, 2009, 36: 3220 |  | [18] | (赵卫卫, 林鑫, 刘奋成等. 热处理对激光立体成形Inconel 718高温合金组织和力学性能的影响[J]. 中国激光, 2009, 36: 3220) |  | [19] | Zhao X M, Chen J, Lin X, et al.Study on microstructure and mechanical properties of laser rapid forming Inconel 718[J]. Mater. Sci. Eng., 2008, A478: 119 |  | [20] | Song K, Yu K, Lin X, et al.Microstructure and mechanical properties of heat treatment laser solid forming superalloy Inconel 718[J]. Acta Metall. Sin., 2015, 51: 935 |  | [20] | (宋衎, 喻凯, 林鑫等. 热处理态激光立体成形Inconel 718高温合金的组织及力学性能[J]. 金属学报, 2015, 51: 935) |  | [21] | Zhang D Y, Niu W, Cao X Y, et al.Effect of standard heat treatment on the microstructure and mechanical properties of selective laser melting manufactured Inconel 718 superalloy[J]. Mater. Sci. Eng., 2015, A644: 32 |  | [22] | Wang Z M, Guan K, Gao M, et al.The microstructure and mechanical properties of deposited-IN718 by selective laser melting[J]. J. Alloys Compd., 2012, 513: 518 |  | [23] | Xi M Z, Liu J B, Zhao Y, et al.Microstructures of heat treatment and properties of TA15 titanium alloy formed by technology of laser rapid forming combined with continuous point forging[J]. Chin. J. Lasers, 2016, 43: 203001 |  | [23] | (席明哲, 刘静波, 赵毅等. 连续点式锻压激光快速成形TA15钛合金热处理组织与性能[J]. 中国激光, 2016, 43: 203001) |  | [24] | Rao G A, Kumar M, Srinivas M, et al.Effect of standard heat treatment on the microstructure and mechanical properties of hot isostatically pressed superalloy Inconel 718[J]. Mater. Sci. Eng., 2003, A355: 114 |  | [25] | Ram G D J, Reddy A V, Rao K P, et al. Microstructure and tensile properties of Inconel 718 pulsed Nd-YAG laser welds[J]. J. Mater. Process. Technol., 2005, 167: 73 | 
 |  
             
								                
															
																| 
																																																																									
																				| No Suggested Reading articles found! |  |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |