| EMBRITTLEMENT OF σ PHASE IN STAINLESS STEEL FOR PRIMARY COOLANT PIPES OF NUCLEAR POWER PLANT |
Yongqiang WANG1( ),Bin YANG2,Na LI3,Suhua LIN3,Li SUN3 |
1 School of Materials Science and Engineering, Anhui University of Technology, Maanshan 243002, China 2 State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083, China 3 School of Metallurgical Engineering, Anhui University of Technology, Maanshan 243002, China |
|
Cite this article:
Yongqiang WANG,Bin YANG,Na LI,Suhua LIN,Li SUN. EMBRITTLEMENT OF σ PHASE IN STAINLESS STEEL FOR PRIMARY COOLANT PIPES OF NUCLEAR POWER PLANT. Acta Metall Sin, 2016, 52(1): 17-24.
|
|
|
|
Abstract Cast austenite stainless steel (CASS) possesses excellent mechanical properties, good workability and high resistance to localized corrosion in chloride environments due to the dual phase microstructure in which the island a-ferrite phase distributes in the g-austenite matrix. So they are widely used in the primary coolant pipes of nuclear power plants. However, undesirable s phase can precipitate in these steels when they are welded or heat treated and it severely decreases the toughness of stainless steels. Although some works have been done to investigate the effect of s phase on mechanical properties of CASS, the mechanism of embrittlement was still lacking. In this work, the effect of s phase on toughness of Z3CN20.09M CASS was investigated, and the embrittlement mechanism of s phase in CASS was discussed by using in situ tensile test, microhardness technology and fracture analysis. It was found that the impact energy of specimens aged at 750 ℃ decreased severely due to the presence of s phases. The (s+g2) structure formed by the eutectoid decomposition of a phase is very hard and its hardness is much higher than that of austenite. This makes the deformation between (s+g2) structure and austenite incoordinate in aged specimens. The precipitation of s phase brought more s/g2 and a/s/g2 high energy non-coherent boundaries. These boundaries hindered dislocation movements and brought stress concentrations. So cracks initiated at the s/g2 or a/s/g2 boundaries preferentially and propagated rapidly when the aged specimen bearded impact stress. The much potential cracking sites (s/g2 and a/s/g2 boundaries) in the (s+g2) structure is the main reason of embrittlement of aged Z3CN20.09M CASS with low toughness.
|
|
Received: 31 March 2015
|
| Fund: Supported by National Natural Science Foundation of China (No.51501001), National High Technology Research and Development Program of China (No.2012AA03A507) and Natural Science Foundation of Anhui Province (No.1508085QE102) |
| [1] | Yamada T, Okano S, Kuwano H. J Nucl Mater, 2006; 350: 47 | | [2] | Xue F, Wang Z X, Shu G G, Yu W W, Shi H J, Ti W X. Nucl Eng Des, 2009; 239: 2217 | | [3] | Li S L, Wang X T, Wang Y L, Li S X. Acta Metall Sin, 2011; 47: 751 | | [3] | (李时磊, 王西涛, 王艳丽, 李树肖. 金属学报, 2011; 47: 751) | | [4] | Kawaguchi S, Sakamoto N, Takano G, Fukuhisa M, Kikuchi Y, Mráz L U. Nucl Eng Des, 1997; 174: 273 | | [5] | Sedriks A J. Corrosion of Stainless Steels. New York: Wiley, 1979: 9 | | [6] | Gunn R N. Duplex Stainless Steels: Microstructure, Properties and Applications. Cambridge: Abington Publishing, 1997: 175 | | [7] | Li S L, Wang Y L, Li S X, Wang X T. Acta Metall Sin, 2010; 46: 1186 | | [7] | (李时磊, 王艳丽, 李树肖, 王西涛. 金属学报, 2010; 46: 1186) | | [8] | Wang Y Q, Han J, Wu H C, Yang B, Wang X T. Nucl Eng Des, 2013; 259: 1 | | [9] | Wang Y Q, Han J, Yang B, Wu H C, Wang X T. Acta Metall Sin, 2013; 49: 415 | | [9] | (王永强, 韩 军, 杨 滨, 武焕春, 王西涛. 金属学报, 2013; 49: 415) | | [10] | Ohmura T, Tsuzaki K, Sawada K, Kimura K. J Mater Res, 2006; 21: 1229 | | [11] | Lo K H, Shek C H, Lai J K L. Mater Sci Eng, 2009; R65: 39 | | [12] | Ibrahim O H, Ibrahim I S, Khalifa T A F. J Mater Sci Technol, 2010; 26: 810 | | [13] | Chen T H, Weng K L, Yang J R. Mater Sci Eng, 2002; A338: 259 | | [14] | Fargas G, Mestra A, Mateo A. Wear, 2013; 303: 584 | | [15] | Shek C H, Wong K W, Lai J K L, Li D J. Mater Sci Eng, 1997; A231: 42 | | [16] | Shek C H, Li D J, Wong K W, Lai J K L. Mater Sci Eng, 1999; A266: 30 | | [17] | Han Y S, Hong S H. Scr Mater, 1997; 36: 557 | | [18] | Li D J, Gao Y, Tan J L, Wang F G, Zhang J S. Scr Metall, 1989; 23: 1319 | | [19] | Lai J K L, Wickens A. Acta Metall, 1979; 27: 217 | | [20] | Pohl M, Storz O, Glogowski T. Mater Charact, 2007; 58: 65 | | [21] | Maehara Y, Ohmori Y, Kunitake T. Met Technol, 1983; 10: 296 | | [22] | Wang Y Q, Han J, Yang B, Wang X T. Mater Charact, 2013; 84: 120 | | [23] | Wang Y Q. PhD Dissertation, University of Science and Technology Beijing, 2013 | | [23] | (王永强. 北京科技大学博士学位论文, 2013) | | [24] | Nilsson J O. Mater Sci Technol, 1992; 8: 685 | | [25] | Chen T H, Yang J R. Mater Sci Eng, 2001; A311: 28 | | [26] | Dai Q X. Metal Materials Science. 2nd Ed., Beijing: Chemical Industry Press, 2013: 130 | | [26] | (戴启勋. 金属材料学. 第二版, 北京: 化学工业出版社, 2013: 130) |
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |