LUO Yang;ZHANG Ning Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; BeijingSenior Engineer;Dept. of precision Alloys Central Iron and Steel Research Institute;Ministry of Metallurgical Industry;Beijing. VARIATION OF YOUNG'S MODULUS WITH TEMPERATURE IN Nd-Fe-B MAGNET. Acta Metall Sin, 1988, 24(3): 293-295.
|
|
|
Abstract Young's modulus of Nd-Fe-B magnet within temperature range from 25 to 800℃was measured by means of ultrasonic resonance. E_∥ measured along c-axis is always smaller thanE_⊥, measured perpendicular to c-axis. The relative difference of Young's modulus (E_⊥-E_∥)/E_⊥=2.2% at room temperature remains almost the same till 500℃, whereas increases very sharplywhen T>500℃. Taking the value of aboat 12% at 600℃, i.e. 5 times more than the value atroom temperature. There is a step following a steep fall of both E_∥ and B_⊥ within the tempera-ture range of 550--600℃, which may be attributed to the melting of Nd-rich phase in the mag-net. Since Young's modulus reflects mainly the strength of bonding between atoms, i. e. thestiffness of the materials, the obtained results imply that the anisotropy of stiffness for Nd-Fe-Bmagnets becomes much higher at temperature above 600℃. Both the high anisotropy of stiff-ness and the remarkable softening at T>600℃ provide evidences for the mechanism of inducedtexture due to hot pressing.
|
|
Received: 18 March 1988
|
1 罗阳,张宁.金属学报,1987;23(1) :A95 2 高占武.高温弹性模量测量新技术,1983;未发表 3 Luo Yang, Ning Zhang. Graham C D Jr. J Appl Phys, 1987; 61(8) : 3442 4 Glvord D, Li H S, Morean J M, Tenaud P. J Magn Magn Mater, 1986; 54--57: 445 5 Lee R W, Schaffel N, Brewer E G. IEEE Trans Magn, 1985; MAG-21: 195 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|