MAGNETIC MOMENT AND CURIE TEMPERATURE OF (Fe_(80)Ni_(20))_(78)Si_(22-x)B_x AMORPHOUS ALLOYS
GUAN Kehong;PU Xiaodong Northeast University of Technology; ShenyangDept. Mater. Sci.; Northeast University of Technology;Shenyang
Cite this article: 

GUAN Kehong;PU Xiaodong Northeast University of Technology; ShenyangDept. Mater. Sci.; Northeast University of Technology;Shenyang. MAGNETIC MOMENT AND CURIE TEMPERATURE OF (Fe_(80)Ni_(20))_(78)Si_(22-x)B_x AMORPHOUS ALLOYS. Acta Metall Sin, 1988, 24(3): 296-298.

Download:  PDF(183KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In the amorphous alloys (Fe_(80)Ni_(20))_(78)Si_(22-x)B_x, the magnetic moment and the curietemperature were found to increase slowly with increasing boron and relatively decreasing silicon.This phenomenon has been explained qualitatively in terms of the electron transition model andthe molecular field approtimation theory.
Key words:  Fe-Ni-Si-B alloys      magnetic moment      Curie temperature     
Received:  18 March 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I3/296

1 Ward K D, Crangle J, Davies H A. In: Masumoto T et al. eds. The Magnetic Moments on Fe, Co and Ni Atoms in Amorphous Alloys Containing Boron, Proc 4th Int Conf on Rapidly Quenched Metal, Sendai. Aug 24--28, 1981, Japan: The Japan Institute of Metals, 1982: 1141--1144
2 Kaneyoshi T. In: Hasegawa R ed., Magnetic Chemical and Structural Properties in Glass Metallic Alloys, Cleveland, Ohio: Chemical Rubber Co., 1981: 38--409
[1] MAO Fei, LU Hao, TANG Fawei, GUO Kai, LIU Dong, SONG Xiaoyan. First-Principle Calculation on the Effect of Mn and In on the Structural Stability and Magnetic Moment of SmCo7 Alloys[J]. 金属学报, 2021, 57(7): 948-958.
[2] WANG Dongmei SONG Lin WANG Yaohui ZHANG Wei Bilige Tegus O. MAGNETOCALORIC EFFECT IN MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03) COMPOUNDS[J]. 金属学报, 2011, 47(3): 344-348.
[3] Gao-Feng WANG; Lin SONG. Magnetocaloric effect on low field in non-stoichiometric MnFe(P,Si,Ge) alloys[J]. 金属学报, 2007, 43(8): 889-892 .
[4] YIN Xiaoying;WANG Yingang;TANG Ning;YANG Fuming(State Key Laboratory of Magnetism; Institute of Physics; Chinese Academy of Sciences; Beijing 100080)(Chinese People's Public Security University; Beijing 100038). CRYSTAL STRUCTURE AND MAGNETIC PROPERTIES OF Y_2Fe_(17-x)Mn_x[J]. 金属学报, 1997, 33(5): 539-542.
[5] WANG Zhi;HE Kaiyuan;ZHANG Luo (Northeastern University; Shenyang 110006)(Tianjin Institute of Technology; Tianjin 300191)(Shanghai Iron and Steel Research Institute; Shanghai 200940). MAGNETOTHERMAL ANALYSIS OF Fe_(72.7)Cu_1Nb_2V_(1.8)Si_(13.5)B_9 ALLOY[J]. 金属学报, 1997, 33(12): 1289-1294.
[6] YANG Wangyue; SHENG Lizhen;SUN Zuqing; HUANG Yuanding; MAO Weimin (University of Science and Technology Beijing; Beijing 100083); ZHANG Baisheng; YE Chuntang (China Institute of Atomic Energy; Beijing 102413)(Manuscript received 1995-11-10; in revised form 1996-04-05). NEUTRON DIFFRACTION STUDY ON SITE OCCUPATION OF SUBSTITUTIONAL ELEMENTS AT SUBLATTICE IN Fe_3Al INTERMETALLICS[J]. 金属学报, 1996, 32(8): 799-804.
[7] LU Zhichao; XIANYU Ze (Department of Physics; Northeastern University;Shenyang)SHEN Baogen((Institute of Physics; Chinese Academy of Scicnces;Beijing)LU Manqi(Institute of Metal Research; Chinese Academy of Sciences;Shenyang). THERMAL EXPANSION AND MAGNETIC PROPERTIES OF NANOCRYSTALLINE Fe-Zr-B ALLOYS[J]. 金属学报, 1994, 30(18): 265-269.
[8] YANG Jilian;ZHANG Baisheng;DING Yongfan;YANG Yingchang;ZHANG Xiaodong;PAN Shuming China Institute of Atomic Energy; Beijing Department of Physics; Peking University; Beijing General Research Institute for Non-Ferrous Metals; Beijing associate professor; P.O. Box 275; Branch No.30; Beijing 102413. NEUTRON DIFFRACTION STUDY ON R_2Fe_(17)N_χ(R=Y, Dy, Nd)[J]. 金属学报, 1993, 29(3): 84-87.
[9] CAO Lei; SHEN Baogen; YANG Linyuan; ZHAO Jiangao (State Key Laboratory of Magnetism; Institute of Physics; Academia Sinica; Beijing). MAGNETIC PROPERTIES AND CRYSTALLIZATION OF AMORPHOUS Nd_4Fe_(77.5)(B_(1-x)C_x)_(18.5) ALLOYS[J]. 金属学报, 1992, 28(11): 70-74.
[10] SHEN Baogen;ZHANG Zhiying;GUO Huiqun;ZHAO Jiangao;GU Benxi Institute of Physics; Academia Sinica; Beijing Department of Physics; Nanjing University research assistant. MAGNETIC MOMENT, CURIE TEMPERATURE AND SPIN WAVE EXCITATION FOR AMORPHOUS Fe_(90-x) Si_x Zr_(10) ALLOYS[J]. 金属学报, 1990, 26(4): 119-124.
[11] YANG Jilian;ZHANG Baisheng;JIN Lan;DING Yongfan;YE Chuntang;YANG Yingchang;KONG Linshu China Academy of Atomic Energy; Beijing Depattment of Physics; Peking University; Beijing Associate Professor P. O. Box 275-80; Beijing 102413. NEUTRON DIFFRACTION STUDY OF Nd_2(Fe_(0.9)Si_(0.1))_(14)B[J]. 金属学报, 1990, 26(1): 69-71.
[12] GUAN Kehong;WANG Jun Northeast University of Technology; Shenyang GUAN Kekong; associate professor; Department of Material Science and Engineering;Northeast University of Technology; 110006 Shenyang. INTRINSIC MAGNETISM AND MAGNETIC ANISOTROPY OF AMORPHOUS ALLOYS Fe_(1-x)(Si, B)_x[J]. 金属学报, 1989, 25(5): 111-114.
[13] XING Feng;JIANG Chao;HO Wenwang Department of Physics; Peking University. MAGNETIC PROPERTIES OF Nd_2(Fe_(1-x)M_x)_(14)B(M=C, Si) ALLOYS[J]. 金属学报, 1988, 24(5): 420-424.
No Suggested Reading articles found!