| CRYOGENIC MECHANICAL BEHAVIOUR OF MARAGING STEEL CONTAINING HYDROGEN |
| LIU Zhonghao;CHEN Lian Institute of Metal Research; Academia Sinica; Shenyang research assistant;Institute of Metal Research;Academia Sinica; Shenyang 110015 |
|
Cite this article:
LIU Zhonghao;CHEN Lian Institute of Metal Research; Academia Sinica; Shenyang research assistant;Institute of Metal Research;Academia Sinica; Shenyang 110015. CRYOGENIC MECHANICAL BEHAVIOUR OF MARAGING STEEL CONTAINING HYDROGEN. Acta Metall Sin, 1990, 26(4): 54-61.
|
|
|
Abstract Within the range of 77 to 295 K, the strength and plasticity of 18Nimaraging steel containing hydrogen increase with the decreasing temperature anddecrease with the increasing hydrogen content. The susceptibility to hydrogen em-brittlement of the maraged specimens is superior to solid solution treated ones evendown to 77K. The dislocations after plastically deformed will be tangled into cellswhich reduce themself in size as decreasing temperature and coarsen as increasinghydrogen concentration. No cryogenic deformation twin was found. The tensile frac-ture surfaces of the solution and maraged specimens containing 5.90 ppm hydrogenunder 295--223 K are revealed as quasi-cleavage and intergranular features respec-tively and as transgranular one at all under other experimental conditions. Theinfluence of hydrogen on the mechanical behaviour of steel and the mechanism ifhydrogen induced deformation and fracture were also discussed.
|
|
Received: 18 April 1990
|
1 Salmon P H, Birkle A J, Reisdorf B G, Pellissier G E. ASM Trans. 1967; 60: 125 2 河部義邦,金尾正雄,中沢兴三,宗木政一.铁钢,1974;60:269 3 浅山行昭.日本金属学会志,1980;44:963 4 Patterson R L, Wayman C M. Actu Metall, 1966; 14: 347 5 Ellina Lunaska. In: Oriani R A, Hirth J P, Smialowski M eds., Hydrogen Degradation of Ferrous Alloys, The Metallurgical Society of AIME, 1985: 321 6 Oriani R A. Ann Rev Mater Sci, 1978; 8: 327 7 Stroh A N. Philos Mag, 1958; 3: 597 8 Cottrell A H. Trans Am Soc, AIME, 1958; 212: 192 9 冯端,王业宁,丘第荣.金属物理(上),北京:科学出版社,1963:341 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|