| THERMAL FATIGUE CRACK IN 5CrMnMo STEEL |
| HE Shiyu;LI Ying;LIU Jianhong Harbin Institute of Technology Faculty of Metal;Harbin Institute of Technology; Harbin |
|
Cite this article:
HE Shiyu;LI Ying;LIU Jianhong Harbin Institute of Technology Faculty of Metal;Harbin Institute of Technology; Harbin. THERMAL FATIGUE CRACK IN 5CrMnMo STEEL. Acta Metall Sin, 1990, 26(4): 62-65.
|
|
|
Abstract The thermal fatigue behaviour of 5CrMnMo steel after various heattreatments has been examined by means of Coffin-model and self-strained thermalfatigue testing machines, The thermal fatigue crack initiation and propagation havebeen observed under SEM and TEM. The majority of thermal fatigue crack was in-itiated through the grain boundaries for the quenched steel and through the breakof interface between carbide and matrix or crack of grain boundary for quenchedand tempered one. The thermal fatigue crack propagated mainly through the break-age of the interface of carbide and grain boundaries for either quenched or quen-ched and tempered steel.
|
|
Received: 18 April 1990
|
1 平修二.热应力热疲劳,东京:日刊工业新闻社,1974:6 2 Malm S. Norstroem L-A. Met Sci, 1979; 13: 545 3 Young R M, Moore A A, Gibbons C L II. Ind Heat, 1981; 48(7) : 24 4 Yamada Y, Yoshimura N, Sakurai T. Int J Mech Sci, 1968; 10: 343 5 张静华,唐亚俊,于洋,张济山,胡壮麒.金属学报,1988;24:A254 6 Coffin L F Jr. Trans ASME, 1954; 76: 931L |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|