TEMPERATURE FIELD THERMOGRAPHY ON FRICTION FACING OF CERTAIN WEAR-RESISTANT ALLOYS
HUANG Yi;BAI Yuankai;XU Jun;LIN Xuerong Institute of Metal Research; Academia Sinica; Shenyang
Cite this article:
HUANG Yi;BAI Yuankai;XU Jun;LIN Xuerong Institute of Metal Research; Academia Sinica; Shenyang. TEMPERATURE FIELD THERMOGRAPHY ON FRICTION FACING OF CERTAIN WEAR-RESISTANT ALLOYS. Acta Metall Sin, 1990, 26(5): 153-155.
Abstract The change of temperature field on the friction facing during contact wearing for3 wear-resistant alloys: Co-Cr-Ni-Si, Co-Cr-Mo and Co-Cr-W has been monitored by theinfrarod sensing thermography. Their flash temperature of the wearing area was measured.
1 Bowden F P, Tabor D. The Friction and Lubrication of Solids, Part Ⅱ, Oxford: Clarendon Press, 1964: 31 2 黄毅,林雪荣,徐军.金属学报,1988;24:B207 3 Archard J F. Wear, 1958--59; 2: 43