Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (5): 153-155    DOI:
Current Issue | Archive | Adv Search |
TEMPERATURE FIELD THERMOGRAPHY ON FRICTION FACING OF CERTAIN WEAR-RESISTANT ALLOYS
HUANG Yi;BAI Yuankai;XU Jun;LIN Xuerong Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

HUANG Yi;BAI Yuankai;XU Jun;LIN Xuerong Institute of Metal Research; Academia Sinica; Shenyang. TEMPERATURE FIELD THERMOGRAPHY ON FRICTION FACING OF CERTAIN WEAR-RESISTANT ALLOYS. Acta Metall Sin, 1990, 26(5): 153-155.

Download:  PDF(371KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The change of temperature field on the friction facing during contact wearing for3 wear-resistant alloys: Co-Cr-Ni-Si, Co-Cr-Mo and Co-Cr-W has been monitored by theinfrarod sensing thermography. Their flash temperature of the wearing area was measured.
Key words:  Co-base alloy      friction      thermography      flash temperature     
Received:  18 May 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I5/153

1 Bowden F P, Tabor D. The Friction and Lubrication of Solids, Part Ⅱ, Oxford: Clarendon Press, 1964: 31
2 黄毅,林雪荣,徐军.金属学报,1988;24:B207
3 Archard J F. Wear, 1958--59; 2: 43
[1] FENG Li, WANG Guiping, MA Kai, YANG Weijie, AN Guosheng, LI Wensheng. Microstructure and Properties of AlCo x CrFeNiCu High-Entropy Alloy Coating Synthesized by Cold Spraying Assisted Induction Remelting[J]. 金属学报, 2023, 59(5): 703-712.
[2] MIAO Junwei, WANG Mingliang, ZHANG Aijun, LU Yiping, WANG Tongmin, LI Tingju. Tribological Properties and Wear Mechanism of AlCr1.3TiNi2 Eutectic High-Entropy Alloy at Elevated Temperature[J]. 金属学报, 2023, 59(2): 267-276.
[3] LI Huizhao, WANG Caimei, ZHANG Hua, ZHANG Jianjun, HE Peng, SHAO Minghao, ZHU Xiaoteng, FU Yiqin. Research Progress of Friction Stir Additive Manufacturing Technology[J]. 金属学报, 2023, 59(1): 106-124.
[4] CHEN Guo, WANG Xinbo, ZHANG Renxiao, MA Chengyue, YANG Haifeng, ZHOU Li, ZHAO Yunqiang. Effect of Tool Rotation Speed on Microstructure and Properties of Friction Stir Processed 2507 Duplex Stainless Steel[J]. 金属学报, 2021, 57(6): 725-735.
[5] LI Zihan, XIN Jianwen, XIAO Xiao, WANG Huan, HUA Xueming, WU Dongsheng. The Arc Physical Characteristics and Molten Pool Dynamic Behaviors in Conduction Plasma Arc Welding[J]. 金属学报, 2021, 57(5): 693-702.
[6] LI Yanmo, GUO Xiaohui, CHEN Bin, LI Peiyue, GUO Qianying, DING Ran, YU Liming, SU Yu, LI Wenya. Microstructure and Mechanical Properties of Linear Friction Welding Joint of GH4169 Alloy/S31042 Steel[J]. 金属学报, 2021, 57(3): 363-374.
[7] HE Changshu, QIE Mofan, ZHANG Zhiqiang, ZHAO Xiang. Effect of Axial Ultrasonic Vibration on Metal Flow Behavior During Friction Stir Welding[J]. 金属学报, 2021, 57(12): 1614-1626.
[8] LIU Chenxi, MAO Chunliang, CUI Lei, ZHOU Xiaosheng, YU Liming, LIU Yongchang. Recent Progress in Microstructural Control and Solid-State Welding of Reduced Activation Ferritic/Martensitic Steels[J]. 金属学报, 2021, 57(11): 1521-1538.
[9] ZHAO Wanxin, ZHOU Zheng, HUANG Jie, YANG Yange, DU Kaiping, HE Dingyong. Microstructure and Frictional Wear Behavior of FeCrNiMo Alloy Layer Fabricated by Laser Cladding[J]. 金属学报, 2021, 57(10): 1291-1298.
[10] LIU Ming, YAN Fuwen, GAO Chenghui. Effects of Progressive Normal Force on Microscratch Responses of Metallic Materials[J]. 金属学报, 2021, 57(10): 1333-1342.
[11] Suigeng DU,Man GAO,Wanting XU,Xifeng WANG. Study on Interface of Linear Friction Welded Joint Between TC11 and TC17 Titanium Alloy[J]. 金属学报, 2019, 55(7): 885-892.
[12] Mingyu ZHAO,Huijuan ZHEN,Zhihong DONG,Xiuying YANG,Xiao PENG. Preparation and Performance of a Novel Wear-Resistant and High Temperature Oxidation-Resistant NiCrAlSiC Composite Coating[J]. 金属学报, 2019, 55(7): 902-910.
[13] ZHANG Guotao , YIN Yanguo , TONG Baohong , ZHANG Xingquan. Controllable Preparation and Self-Lubricating Mechanism Analysis of Bilayer Porous Iron-Based Powder Metallurgy Materials[J]. 金属学报, 2019, 55(11): 1448-1456.
[14] Chen WANG, Beibei WANG, Peng XUE, Dong WANG, Dingrui NI, Liqing CHEN, Bolü XIAO, Zongyi MA. Fatigue Behavior of Friction Stir Welded SiCp/6092Al Composite[J]. 金属学报, 2019, 55(1): 149-159.
[15] Yanmo LI, Chenxi LIU, Liming YU, Huijun LI, Zumin WANG, Yongchang LIU, Wenya LI. Effect of High-Temperature Ageing on Microstructure and Mechanical Properties of Linear Friction Welded S31042 Steel Joint[J]. 金属学报, 2018, 54(7): 981-990.
No Suggested Reading articles found!