| TECHNOLOGICAL STUDIES ON EQUIAXED GRAIN REFINEMENT IN TC11 Ti ALLOY BAR |
| SU Zuwu;MENG Guowen;GUO Hongzhen;LIU Jianchao;YAO Zekun Northwestern Polytechnical University; Xi'an; YANG Zhaosu;HU Zongshi Baoji Non Ferrous Metals Mill |
|
Cite this article:
SU Zuwu;MENG Guowen;GUO Hongzhen;LIU Jianchao;YAO Zekun Northwestern Polytechnical University; Xi'an; YANG Zhaosu;HU Zongshi Baoji Non Ferrous Metals Mill. TECHNOLOGICAL STUDIES ON EQUIAXED GRAIN REFINEMENT IN TC11 Ti ALLOY BAR. Acta Metall Sin, 1991, 27(5): 79-82.
|
|
|
Abstract The formation reason and elimination method of non-uniform microstructure defects in TC11 Ti alloy bar have been studied. The coagulating and coarsening into block of the part of grain boundary α and secondary α seem to be caused by the ingot cogging and initial forging temperature in the β region as well as no more enough deformation and uneven distribution. The grain α, elongated α and blocky α may be finally eliminated by adopting the technique of (α+β) thermomechanical processing+β processing, W. Q.+recrystallization annealing, A. C., thus the size of uniform and fine equiaxed α structure is believed to be reduced to 1.9258μm.
|
|
Received: 18 May 1991
|
1 Weiss I, Froes F H, Eylon D, Welsch G E. Metall Trans, 1986; 17A: 1935--1946 2 Борисова Е А,陈石卿译.钛合金金相学,北京:国防工业出版社,1986:41 |