FEATURE OF SERRATED YIELDING IN HIGH STRENGTH Al-Zn-Mg-Cu ALLOY
QIAN Kuangwu;LI Xiaoqi;ZHANG Haoguo Fuzhou University
Cite this article: 

QIAN Kuangwu;LI Xiaoqi;ZHANG Haoguo Fuzhou University. FEATURE OF SERRATED YIELDING IN HIGH STRENGTH Al-Zn-Mg-Cu ALLOY. Acta Metall Sin, 1991, 27(5): 77-78.

Download:  PDF(174KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The temperature dependence of critical strain for serrated yielding was found inhigh strength Al-Zn-Mg-Cu alloy. It divides into two temperature regions. Their temperaturecoefficients of critical strain will be negative and positive respectively.
Key words:  serrated yielding      dynamic strain aging      high strength Al a1loy      critical strain     
Received:  18 May 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I5/77

[1] Yahui DENG,Yinhui YANG,Jianchun CAO,Hao QIAN. Research on Dynamic Recrystallization Behavior of 23Cr-2.2Ni-6.3Mn-0.26N Low Nickel TypeDuplex Stainless Steel[J]. 金属学报, 2019, 55(4): 445-456.
[2] LI Junru, GONG Chen, CHEN Lie, ZUO Hui, LIU Yazheng. HOT DEFORMATION BEHAVIOR OF BLADES STEEL 10Cr12Ni3Mo2VN FOR ULTRA- SUPERCRITICAL UNITS[J]. 金属学报, 2014, 50(9): 1063-1070.
[3] GUO Pengcheng, QIAN Lihe, MENG Jiangying, ZHANG Fucheng. MONOTONIC TENSION AND TENSION-COMPRES- SION CYCLIC DEFORMATION BEHAVIORS OF HIGH MANGANESE AUSTENITIC TWIP STEEL[J]. 金属学报, 2014, 50(4): 415-422.
[4] CAI Yulong, FU Shihua, WANG Yuhui, TIAN Chenggang, GAO Yue, CHENG Teng, ZHANG Qingchuan. SERRATED YIELDING OF 5456 ALUMINIUM MAGNE- SIUM ALLOY BASED ON THREE DIMENSIONAL DIGITAL IMAGE CORRELATION[J]. 金属学报, 2014, 50(12): 1491-1497.
[5] HAN Guoming, CUI Chuanyong, GU Yuefeng, HU Zhuangqi, SUN Xiaofeng. INVESTIGATION OF TEMPERATURE DEPENDENCE OF PLC EFFECT IN A NICKEL BASE SUPERALLOY[J]. 金属学报, 2013, 49(10): 1243-1247.
[6] FU Shihua CHENG Teng ZHANG Qingchuan CAO Pengtao HU Qi. STUDY ON TWO CRITICAL MECHANISMS OF PLC EFFECT OF 5456 Al–BASED ALLOY[J]. 金属学报, 2012, 48(12): 1453-1458.
[7] TIAN Chenggang CUI Chuanyong GU Yuefeng SUN Xiaofeng . EFFECT OF SOLUTION TREATMENT ON THE INVERSE DYNAMIC STRAIN AGING OF A Ni–Co BASE SUPERALLOY[J]. 金属学报, 2012, 48(10): 1223-1228.
[8] CAO Yu DI Hongshuang ZHANG Jiecen ZHANG Jingqi MA Tianjun. RESEARCH ON DYNAMIC RECRYSTALLIZATION BEHAVIOR OF INCOLOY 800H[J]. 金属学报, 2012, 48(10): 1175-1185.
[9] CHEN Liqing ZHAO Yang XU Xiangqiu LIU Xianghua. DYNAMIC RECRYSTALLIZATION AND PRECIPITATION BEHAVIORS OF A KIND OF LOW CARBON V–MICROALLYED STEEL[J]. 金属学报, 2010, 46(10): 1215-1222.
[10] JIANG Huifeng CHEN Xuedong FAN Zhichao DONG Jie JIANG Heng LU Shouxiang. EFFECT OF DYNAMIC STRAIN AGING ON FATIGUE--CREEP BEHAVIOR OF 316L AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2009, 45(3): 326-330.
[11] Lu Junyong; Jiang Zhenyu; Zhang Qingchuan. Preliminary Time Series Analysis of Serrated Yielding in Al-4%Cu Alloy[J]. 金属学报, 2006, 42(6): 611-618 .
[12] XIANG Guofu; ZHANG Qingchuan; LIU Haowen; JIANG Huifeng; WU Xiaoping. The Deformation Measurements of Portevin-Le Chatelier Shear Bands in Al-Cu Alloys[J]. 金属学报, 2006, 42(6): 619-623 .
[13] Cong Wang. PORTEVIN-LE CHATELIER EFFECT OF LA41 MAGNESIUM ALLOYS[J]. 金属学报, 2006, 42(2): 191-194 .
[14] . The Effect of Solute Concentration by Solution Treatment on Portevin-Le Chatelier effect in Al-Cu Alloys[J]. 金属学报, 2006, 42(12): 1248-1252 .
[15] JIANG Huifeng; ZHANG Qingchuan; JIANG Zhenyu; WU Xiaoping. Experimental Investigations on the Temporal and Spatial Behaviors of the PLC Effect in Al--Cu Alloys[J]. 金属学报, 2005, 41(7): 727-732 .
No Suggested Reading articles found!