Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (5): 120-124    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF Nb ADDITION ON MICROSTRUCTURE OF (Nd,Dy)-(Fe,Co)-B MAGNETS
SONG Xiaoping;WANG Xiaotian;HUANG Qihua;LIU Junhai;YAO Yinliang Xi'an Jiaotong University
Cite this article: 

SONG Xiaoping;WANG Xiaotian;HUANG Qihua;LIU Junhai;YAO Yinliang Xi'an Jiaotong University. EFFECT OF Nb ADDITION ON MICROSTRUCTURE OF (Nd,Dy)-(Fe,Co)-B MAGNETS. Acta Metall Sin, 1991, 27(5): 120-124.

Download:  PDF(1368KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An addition of Nb up to 2 at.-% into (Nd, Dy)-(Fe, Co)-B alloy causes to form the primary lath Fe_2Nb crystallization and to precipitate the hard magnetic grain. Both increases with the increasing Nb content. During sintering, part of Fe_2Nb dissolves within the 2:14:1 phase, and the Fe_2Nb along grain boundary hinders the growth of 2:14:1 grain. In annealing processing, the dissolved Nb in φ phase precipitates out, and this nearby the grain boundary diffuses into Nd-rich phase to form new Nb-containing grain and to increase the Nb content in Nd-rich phase.
Key words:  NdFeB      rare earth permanent magnet      microstructure     
Received:  18 May 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I5/120

1 Kim A S. J Appl Phys, 1988; 63: 3975
2 Xiao Y, Strnat K J, Mildrum H F, Ray A E. In: Herget C, Poerschke R eds., Proc 9th Int Workshop on Rare Earth Magnets and their Applications and 5th Int Symposium on Magnetic Anisotropy and Coercivity in Rare Earth-Transition Metal Alloys, Vol.Ⅰ, 31, Aug. 3 Sep., 1987, Bad Soden, FRG, Bad Honnef 1, FRG: DPG-GmbH, 1987: 467
3 Tokunaga M., Kogure H, Endoh M, Harada H IEEE Trans Magn, 1987; 23: 2287
4 Rodewald W, Wall B. J Magn Magn Mater, 1989; 80: 57
5 Parker S F H, Grundy P J, Fidler J. J Magn Magn Mater, 1987; 66: 74
6 Ishikawa T, Hamada Y, Ohmort K. IEEE Trans Magn, 1989; 25: 3434
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[3] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[4] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[5] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[6] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[7] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[11] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[12] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[13] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[14] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[15] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
No Suggested Reading articles found!