| MAGNETIC PROPERTIES AND CRYSTALLIZATION OF RAPIDLY QUENCHED(Fe_(1-x)Ga_x)_(77.5)Nd_4B_(18.5) ALLOYS |
| YANG Hongying;SHEN Baogen;YANG Linyuan;GUO Huiqun Laboratory of Magnetism; Institute of Physics; Academia Sinica; Beijing |
|
Cite this article:
YANG Hongying;SHEN Baogen;YANG Linyuan;GUO Huiqun Laboratory of Magnetism; Institute of Physics; Academia Sinica; Beijing. MAGNETIC PROPERTIES AND CRYSTALLIZATION OF RAPIDLY QUENCHED(Fe_(1-x)Ga_x)_(77.5)Nd_4B_(18.5) ALLOYS. Acta Metall Sin, 1992, 28(4): 63-67.
|
|
|
Abstract The Curie temperature increases but crystallization temperature decreases withthe increase of Ga concentration, x, of amorphous (Fe_(1-x)Ga_x)_(77.5)Nd_4B_(18.5) alloys. The averagemagnetic moment of Fe atom is almost a constant. By X-ray diffraction and thermomagneticmeasurements, the crystalline phases of the alloys, an unknown phase and α-(Fe, Ga) besidesFe_3B as major one, were identified. The room temperature coercive field with related to Ga con-centration was also studied.
|
|
Received: 18 April 1992
|
1 Coehoorn R, De Mooij D B, Dchateau J P W B, Buschow K H J. J Phys Colloq, 1988; 49: (C8) : 669 2 Shen Baogen, Yang Linyuan, Zhang Junxian, Gu Benxi, Ning Taishan, Wo Feng, Zhao Jiangao, Guo Huiqun, Zhan Wenshan. Solid State Commun, 1990; 74: 893 3 Shen Baogen, Zhang Junxian, Yang Linyuan, Wo Feng, Ning Taishan. J Magn Magn Mater, 1990; 89: 195 4 Shen Baogen, Zhang Junxian, Yang Linyuan, Wo Feng, Ning Taishan, Zhao Jiangao, Guo Huiqun, Zhan Wenshan. J Less-Common Met, 1990; 167: 339 5 Shen Baogen, Yang Linyuan, Zhang Junxian, Wo Feng, Ning Taishan, Zhao Jiangao, Guo Huiqun, Zhan Wenshan. Phys Status Solidi, 1990; 119a: K63 6 Zhang Junxian, Shen Baogen, Yang Linyuan, Zhan Wenshan. Phys Status Solidi, 1991; 124a: 541 7 Harris R, Plischke M, Zuckermann M J. Phys Rev Lett, 1973; 31: 160 8 Coey J M D, Chappert J, Rebouillat J P, Wang T S. Phys Rev Lett, 1976; 36: 1061 9 Zhao Jiangao, Shen Baogen, Zhan Wenshan. In: Xu G X, Xiao J M eds., Proc Int Conf on Rare Earth Devel. Appl., Beijing: Science Press, 1985: 895 10 Zhang Junxian, Shen Baogen, Yang Linguan, Zhan Wenshan. Phys Status Soildi, 1990; 122a: 651 |