MAGNETIC PROPERTIES AND CRYSTALLIZATION OF RAPIDLY QUENCHED(Fe_(1-x)Ga_x)_(77.5)Nd_4B_(18.5) ALLOYS
YANG Hongying;SHEN Baogen;YANG Linyuan;GUO Huiqun Laboratory of Magnetism; Institute of Physics; Academia Sinica; Beijing
Cite this article: 

YANG Hongying;SHEN Baogen;YANG Linyuan;GUO Huiqun Laboratory of Magnetism; Institute of Physics; Academia Sinica; Beijing. MAGNETIC PROPERTIES AND CRYSTALLIZATION OF RAPIDLY QUENCHED(Fe_(1-x)Ga_x)_(77.5)Nd_4B_(18.5) ALLOYS. Acta Metall Sin, 1992, 28(4): 63-67.

Download:  PDF(427KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The Curie temperature increases but crystallization temperature decreases withthe increase of Ga concentration, x, of amorphous (Fe_(1-x)Ga_x)_(77.5)Nd_4B_(18.5) alloys. The averagemagnetic moment of Fe atom is almost a constant. By X-ray diffraction and thermomagneticmeasurements, the crystalline phases of the alloys, an unknown phase and α-(Fe, Ga) besidesFe_3B as major one, were identified. The room temperature coercive field with related to Ga con-centration was also studied.
Key words:  (Fe      Ga) NdB magnet      amorphous alloy      magnetic property      crystallization     
Received:  18 April 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I4/63

1 Coehoorn R, De Mooij D B, Dchateau J P W B, Buschow K H J. J Phys Colloq, 1988; 49: (C8) : 669
2 Shen Baogen, Yang Linyuan, Zhang Junxian, Gu Benxi, Ning Taishan, Wo Feng, Zhao Jiangao, Guo Huiqun, Zhan Wenshan. Solid State Commun, 1990; 74: 893
3 Shen Baogen, Zhang Junxian, Yang Linyuan, Wo Feng, Ning Taishan. J Magn Magn Mater, 1990; 89: 195
4 Shen Baogen, Zhang Junxian, Yang Linyuan, Wo Feng, Ning Taishan, Zhao Jiangao, Guo Huiqun, Zhan Wenshan. J Less-Common Met, 1990; 167: 339
5 Shen Baogen, Yang Linyuan, Zhang Junxian, Wo Feng, Ning Taishan, Zhao Jiangao, Guo Huiqun, Zhan Wenshan. Phys Status Solidi, 1990; 119a: K63
6 Zhang Junxian, Shen Baogen, Yang Linyuan, Zhan Wenshan. Phys Status Solidi, 1991; 124a: 541
7 Harris R, Plischke M, Zuckermann M J. Phys Rev Lett, 1973; 31: 160
8 Coey J M D, Chappert J, Rebouillat J P, Wang T S. Phys Rev Lett, 1976; 36: 1061
9 Zhao Jiangao, Shen Baogen, Zhan Wenshan. In: Xu G X, Xiao J M eds., Proc Int Conf on Rare Earth Devel. Appl., Beijing: Science Press, 1985: 895
10 Zhang Junxian, Shen Baogen, Yang Linguan, Zhan Wenshan. Phys Status Soildi, 1990; 122a: 651
[1] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[2] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[3] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[4] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[5] LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature[J]. 金属学报, 2023, 59(11): 1439-1447.
[6] WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo. Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy[J]. 金属学报, 2022, 58(7): 932-942.
[7] GUO Lu, ZHU Qianke, CHEN Zhe, ZHANG Kewei, JIANG Yong. Non-Isothermal Crystallization Kinetics of Fe76Ga5Ge5B6P7Cu1 Alloy[J]. 金属学报, 2022, 58(6): 799-806.
[8] LIU Shuaishuai, HOU Chaonan, WANG Engang, JIA Peng. Plastic Rheological Behaviors of Zr61Cu25Al12Ti2 and Zr52.5Cu17.9Ni14.6Al10Ti5 Amorphous Alloys in the Supercooled Liquid Region[J]. 金属学报, 2022, 58(6): 807-815.
[9] LI Jinfu, LI Wei. Structure and Glass-Forming Ability of Al-Based Amorphous Alloys[J]. 金属学报, 2022, 58(4): 457-472.
[10] REN Shaofei, ZHANG Jianyang, ZHANG Xinfang, SUN Mingyue, XU Bin, CUI Chuanyong. Evolution of Interfacial Microstructure of Ni-Co Base Superalloy During Plastic Deformation Bonding and Its Bonding Mechanism[J]. 金属学报, 2022, 58(2): 129-140.
[11] ZHANG Jinyong, ZHAO Congcong, WU Yijin, CHEN Changjiu, CHEN Zheng, SHEN Baolong. Structural Characteristic and Crystallization Behavior of the (Fe0.33Co0.33Ni0.33)84 -x Cr8Mn8B x High-Entropy-Amorphous Alloy Ribbons[J]. 金属学报, 2022, 58(2): 215-224.
[12] JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge. Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. 金属学报, 2022, 58(12): 1545-1556.
[13] HU Chen, PAN Shuai, HUANG Mingxin. Strong and Tough Heterogeneous TWIP Steel Fabricated by Warm Rolling[J]. 金属学报, 2022, 58(11): 1519-1526.
[14] HAN Luhui, KE Haibo, ZHANG Pei, SANG Ge, HUANG Huogen. Kinetic Crystallization Behavior of Amorphous U60Fe27.5Al12.5 Alloy[J]. 金属学报, 2022, 58(10): 1316-1324.
[15] XIANG Zhaolong, ZHANG Lin, XIN Yan, AN Bailing, NIU Rongmei, LU Jun, MARDANI Masoud, HAN Ke, WANG Engang. Effect of Cr Content on Microstructure of Spinodal Decomposition and Properties in FeCrCoSi Permanent Magnet Alloy[J]. 金属学报, 2022, 58(1): 103-113.
No Suggested Reading articles found!