Abstract The Nd_(14)Fe_(73)Co_6B_7 magnetic powder with high coercivity was effectively made of its ingot by hydrogenizing-disproportionating-dehydrogenizing, so called HDD process, under H_2 atmosphere. The high coercivity of the powder was found to be dependent on the decomposition of Nd_2Fe(Co)_4B phase during hydrogenation and consequent upon recrystallization during dehydrogenation. And the contrast of grain size in between original ingot powder and recrystallized one, from 10—50 down to 0.3--1μm, may be the principal cause for this improvement.
|
|
Received: 18 August 1992
|
1 Lee R W, Appl Phys Lett, 1985; 46:790 2 Takeslita T, Nakayama R. Proc 10th Int Workshop on Rare Earth Permanent Magnets and their Applications,551-557 3 Xiao Y, Zhang Z, Proc 11th Int Workshop on Rare Earth Permanent Magnets and their Applications.531-537T |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|