| EFFECTS OF PASSIVATION POTENTIAL AND POST-TREATMENT ON COMPOSITION OF SURFACE FILM FORMED ON STEEL 304 AND ITS STABILITY |
| SONG Guangling; CAO Chunan; XIA Bangjie; LIN Haichao (Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang) |
|
Cite this article:
SONG Guangling; CAO Chunan; XIA Bangjie; LIN Haichao (Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang). EFFECTS OF PASSIVATION POTENTIAL AND POST-TREATMENT ON COMPOSITION OF SURFACE FILM FORMED ON STEEL 304 AND ITS STABILITY. Acta Metall Sin, 1992, 28(8): 84-90.
|
|
|
Abstract The measurements of the activation time and the breakdown potential of surface films formed on stainless steel 304 in passive or transpassive potential range, followed by post-treatment in Na_2MoO_4 containing solution or not treated, were carried out. The results show that the resistance of transpassive film against the activation dissolution in acidic solution is much higher than that of passive film, and the breakdown potential of transpassive film can be strikingly enhanced by post-treatment. In addition, the effects of potential and post-treatment on the composition of surface film were investigated by means of AES and XPS analysis, and the relationship between the composition and stability of film was discussed too.
|
|
Received: 18 August 1992
|
1 吕玉成,Clayton C R.中国腐蚀与防护学报,1988;8:29 2 姜晓霞,王景韫.合金相电化学.上海:上海科学技术出版社,1984:17 3 Landolt D. In: Frankenthal P, Kruger J eds., Passivity of Metals, Proc 4th Int Symp. on Passivity, Warrenton, October 17-21, 1977, The Electrochemical Society, 1978:484 4 宋光铃,曹楚南,王友,林海潮.中国腐蚀与防护学报,1991;11:319 5 宋光铃,曹楚南,林海潮.中国腐蚀与防护学报,1992;12:76 6 宋光铃,曹楚南,林海潮.应用化学学报,1992;9:79 7 Clayton C R, Lu Y C. J Electrochem Soc, 1986; 133: 2465 8 McIntyre N S. In: Briggs D, Seah M P eds., Practical Surface Analysis by Auger and X-ray Photoelectron Spectroscopy, New York: Wiley, 1983: 411 9 Hoppe H-W, Strehblow H-H. Surf Interface Anal, 1989; 14:121 10 Brooks A R, Clayton C R, Doss K, Lu Y C. J Electrochem Soc, 1986;133:2459 11 Bloom M C, Goldenberg L. Corros Sci, 1965; 5:623< |