Acta Metall Sin  1993, Vol. 29 Issue (6): 8-12    DOI:
Current Issue | Archive | Adv Search |
STRUCTURE AND MAGNETIC PROPERTIES OF METASTABLE COMPOUND Ce_2Fe_(23)B3
CAO Lei;GONG Huayang;YANG Linyuan;KONG Linshu;GUO Huiqun Stale Key Laboratory of Magnetism; Institute of Physics; Academia Sinica; BeijingSHEN Baogen;assoeiate professor.Institute of Physies Academia Sinica;Beijing 100080
Cite this article: 

CAO Lei;GONG Huayang;YANG Linyuan;KONG Linshu;GUO Huiqun Stale Key Laboratory of Magnetism; Institute of Physics; Academia Sinica; BeijingSHEN Baogen;assoeiate professor.Institute of Physies Academia Sinica;Beijing 100080. STRUCTURE AND MAGNETIC PROPERTIES OF METASTABLE COMPOUND Ce_2Fe_(23)B3. Acta Metall Sin, 1993, 29(6): 8-12.

Download:  PDF(321KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Crystallization of amorphous Ce_2Fe_(23)B_3 alloys as well as structure and mag-netic properties of metastable compound Ce_2Fe_(23)B_3 were studied. X-ray diffraction analysisconfirmed that the crystal structure of Ce_2Fe_(23)B_3 compound is body-centered cubic, its lat-tice constant α=1.417 nm. Measurement of room temperature hyperfine field ofCe_2Fe_(23)B_3 observeed that the size of Fe magnetic moment in different Fe site is orderlyμ_(Fe)(48e_1)>μ_(Fe)(48e_2)>μ_(Fe)(48e_3)>μ_(Fe)(16c)>μ_(Fe)(24d). Average magnetic moments per Fe atomand per Ce atom are 1.94 and 0.85μ_B respectively.
Key words:  metastable compound      structure      magnetic property     
Received:  18 June 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I6/8

1 De Mooij D B, Buschow K H J. Philips J Res, 1986; 41: 400
2 Shen B G, Yang L Y, Cao L, Yang H Y, Zhao J G, Yang F M. J Magn Magn Mater, 1992; 104--107: 1281
3 沈保根,杨林原,曹蕾,袁俭,郭慧群.科学通报,1992;37:1358
4 Gau C, Cheng Z X, Chen D F, Niu S W, Yan O W, Zhang P L, Shen B G, Yang L Y. J Magn Magn Mater, 1993; in Press.
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[3] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[4] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[5] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[6] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[7] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[8] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[9] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[10] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[11] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[12] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[13] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[14] LI Qian, LIU Kai, ZHAO Tianliang. Rust Formation Behavior and Mechanism of Q235 Carbon Steel in 5%NaCl Salt Spray Under Elastic Tensile Stress[J]. 金属学报, 2023, 59(6): 829-840.
[15] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
No Suggested Reading articles found!