| BEHAVIOUR OF BORON SEGREGATION TO GRAIN BOUNDARIES IN BCC Fe-3%Si ALLOY |
| HE Xinlai;CHU Youyi;KE Jun University of Science and Technology BeijingZHANG Sanhong;Department of Materials Physics;University of Science and Technology Beijing;Beijing 100083 |
|
Cite this article:
HE Xinlai;CHU Youyi;KE Jun University of Science and Technology BeijingZHANG Sanhong;Department of Materials Physics;University of Science and Technology Beijing;Beijing 100083. BEHAVIOUR OF BORON SEGREGATION TO GRAIN BOUNDARIES IN BCC Fe-3%Si ALLOY. Acta Metall Sin, 1993, 29(6): 1-7.
|
|
|
Abstract Behaviour of B segregation to grain boundaries in Fe-3% Si alloy has beenstudied by means of particle tracking autoradiography. Results indicate that B tends to equi-librium segregation to grain boundaries in Fe-3% Si higher than in austenitic alloys. No ob-servable nonequilibrium segregation of B to grain boundaries was revealed in Fe-3% Si alloyduring cooling and isothermal holding. The binding energy between B atoms and grainboundaries is 55.7±1.7 kJ/mol. Based on the complex mechanism of quenching-induce-nonequilibrium segregation, different behaviours of B segregation in γ-Fe and b.c.c.Fe-3% Si alloy were discussed.
|
|
Received: 18 June 1993
|
1 Guttmann M, McLean D. Interfacial Segregation, ASM, 1977 2 He X L, Chu Y Y. J phys, D: Appl phys, 1983; 16: 1145 3 He X L, Chu Y Y, Jonas J J. Acta Metall, 1989; 37: 2905 4 He X L, Chu Y Y, Jonas J J. Acta Metall, 1989: 37: 147 5 Karlsson L, Norden H, Odelias H. Acta Metall, 1988; 36: 13 6 McLean D. Grain Boundaries in Metals. Oxford, 1957: 101 7 褚幼义,章三红,贺信莱,柯俊.金属学报,1989;25:A275 8 Williams T M, Stoneham A M, Harries D R. J Met Sci. 1976; 10: 14 9 章三红.北京科技大学博士论文,1991 10 Busby P E, Wells C. Trans AIME, 1954; 198: 972 11 Peterson N L, Siegel R W. Properties of Atomic Defects in Metals, 1978: 63 12 Cahn R W,钢铁学院金属物理教研室译.物理金属学,中册,北京:科学出版社,1985:453 |