| DETERMINATION OF TEXTURE STATE OF THIN FILM ZrO_2 BY ELECTRON DIFFRACTION PATTERN |
| WANG Yinghua;Department of Materials Science and Engineering.Tsinghua University;Beijing 100084 |
|
Cite this article:
WANG Yinghua;Department of Materials Science and Engineering.Tsinghua University;Beijing 100084. DETERMINATION OF TEXTURE STATE OF THIN FILM ZrO_2 BY ELECTRON DIFFRACTION PATTERN. Acta Metall Sin, 1993, 29(6): 95-96.
|
|
|
Abstract A method for determining thin film texture by electron diffraction pattern ispresented. Using this method, the texture state of the ZrO_2 thin film has been determined.
|
|
Received: 18 June 1993
|
1 Cullity B D. Elements of X-Ray Diffraction. Reading Mass: Addison-Wesley, 1978 2 王英华.X光衍射技术基础.北京:原子能出版社,1987 |
| No Suggested Reading articles found! |
|
|