| X-RAY DIFFRACTION DETERMINATION OF STRESS RELAX IN LASER MELTED AREA OF STAINLESS STEEL |
| XU Jingyang;VAN BRUSSEL;B J;NOORDHUIS J;BRONSVELD P M;DE HOSSON J Th M Shanghai Institute of Metallurgy; Academia Sinica Department of Applied Physics; Materials Science Center; University of Groningen; The Netherlands |
|
Cite this article:
XU Jingyang;VAN BRUSSEL;B J;NOORDHUIS J;BRONSVELD P M;DE HOSSON J Th M Shanghai Institute of Metallurgy; Academia Sinica Department of Applied Physics; Materials Science Center; University of Groningen; The Netherlands. X-RAY DIFFRACTION DETERMINATION OF STRESS RELAX IN LASER MELTED AREA OF STAINLESS STEEL. Acta Metall Sin, 1993, 29(9): 92-96.
|
|
|
Abstract Laser surface melting of AISI 304 stainless steel has frequently beneficial effecton surface modification due to the high quench rate by self conduction of heat as quenching,and has a disadvantage that a considerable amount of tensile stress was introduced.It could berelaxed by neon implantation. Principle and method for measuring the stress relax in 0.1 μmthick surface layer were explained in detail for showing the Ne effect on it.
|
|
Received: 18 September 1993
|
1 De Beurs H, Hovius J A, De Hosson J Th M. Acta Metall, 1988; 36: 3123 2 Xu J Y(徐景阳), Van Brussel B J, Bronsveld P M, De Hosson J Th M. Surf Coat Technol. 1991; 45: 43 3 Perry A J, Chollet L. J Vac Sci Technol, 1986; 4A: 2801 4 徐景阳, Van Brussel B J, Noordhuis J, Bronsveld P M, De Hosson J Th M. 金属学报, 1993; 29: B88 5 Simmons R O, Balluffi R W. Phys Rev, 1962; 125: 862 6 Gaber A, Ehrhart P. Radiat Eff 1983; 78: 213 7 Xu J Y(徐景阳), Van Brussel B J, Noodhuis J, Bronsveld P M, De Hosson J Th M. Proc Surf Eng Conf Toronto, 1990: 167 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|