INFLUENCE OF Ce IMPLANTATION ON OXIDATION BEHAVIOUR OF Ni20Cr ALLOY |
LI Meishuan; PENG Hiao;MA Hinqing;LI Tiefan(Corrosion Science Laboratory;Institute of Corrosion and Protection of Metals;Chinese Academy of Sciences)(Manuscript received 10 May;1993) |
|
Cite this article:
LI Meishuan; PENG Hiao;MA Hinqing;LI Tiefan(Corrosion Science Laboratory;Institute of Corrosion and Protection of Metals;Chinese Academy of Sciences)(Manuscript received 10 May;1993). INFLUENCE OF Ce IMPLANTATION ON OXIDATION BEHAVIOUR OF Ni20Cr ALLOY. Acta Metall Sin, 1994, 30(16): 169-174.
|
Abstract Implantation of 2×1016,5×1016,1×1017Ce+/cm2 into Ni20Cr alloy can significantly decrease the oxidation rate at 1000 and 1100℃,and improve the adhesion of oxide scales.The changes of binding energy of alloy in elements in alloy surface after Ce implanting and in oxide scale formed at 1100℃ were measured using ion microperobe mass analyzer.The decrement of binding energy of Cr+on the alloy surface accelerate rapidly the formation of protective Cr2O3,however these of Cr+and Ni+ in the oxide scale increase,the outward diffusion of Cr3+and Ni2+through the scale are delayed.This seems to be the main reason for Ce implantation to decrease the oxidation rate of Ni20Cr at 1100℃.The oxide scales of Ce-implanted Ni20Cr alloy are dense,intact and well adhesive with the alloy.The oxide scales spall partially after 270 time during the cyclic oxidation at 1000℃,but the effect of Ce on the improvement of the oxide scale adherence is still obvious.Correspondent:LI Meishuan,assistant professor,(Institute of Corrosion and Protection of Metals,Chinese Academy of Sciences,Shenyang 110015)
|
|
1HindamH,WhittleDP.OxidMet,1982;18:2452MoonDP.MaterSciTechnol,1989;5:7543StringerJ.MaterSciEng,1989,A120:1294StootFH,PunniJS,WoodGC,DearnaleyG.IonImplantationIntoMetals.PergamonPress,1982:2455PrzybylskiK,Garratt-ReedAJ,YurekGJ.JElectrochemSoc,1988;135:5096CotellCM,YurekGJ,HusseyRJ,MitchchellDF,GrahamMJ.OxidMet,1990;34:173,2017万晓景,杨柯,曹名洲.金属学报,1986;22:A1898陈廉,刘树望,邹军军,邵玉霞,李裕光.质谱学报,1988:9:329GaoPeiyu.8thInternationalCongressonMetallicCorrosion,Vol.1,Mainz,Germany,InternationalCorrosionCouncil,EuropeanFederationofCorrosion,DechemaDeutscheGesellsehaftfurChemischesApparatewesene.V.Frankfurt//Main,1981:40610AbderrazikGB,MoulinG,HuntzAM,OxidMet,1990;33:191p |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|