Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (6): 257-263    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF HYDROGENATION ON MICROSTRUCTURE OF SUPER-α_2
YANG Ke;LIAO Bo;LI Yiyi(Key Laboratory for Materials and Hydrogen of Liaoning Province;Institute of Metal Research;Chinese Academy of Sciences;Shenyang)(Manuscript received 27 October;1993;in revised form 8 December;1993)
Cite this article: 

YANG Ke;LIAO Bo;LI Yiyi(Key Laboratory for Materials and Hydrogen of Liaoning Province;Institute of Metal Research;Chinese Academy of Sciences;Shenyang)(Manuscript received 27 October;1993;in revised form 8 December;1993). EFFECT OF HYDROGENATION ON MICROSTRUCTURE OF SUPER-α_2. Acta Metall Sin, 1994, 30(6): 257-263.

Download:  PDF(748KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Hydrogenation of a Ti3Al-based intermetallic(Super-α_2) was carried out to systematically investigate the microstructural variations of this compound.The experimental results showed that evident variations have taken place in microstructures of Super-α2 due to the hydrogenations.Acicular or Widmanstatten α2 was found to form in the hydrogenated microstructure under continuously cooling with slower rate,instead of nearly equiaxed α2 under the normal treatment.The precipitations in the hydrogenated microstructures undergoing ageing treatment showed more regular and homogeneous in morphology and distribution. Furthermore,the formation of O-phase in the microstructure was found to be promoted by the hydrogenation.The essential reason for these microstructural variations of Super-α2 caused by hydrogenation can be explained by the fact that hydrogen,as a strongβ-stabilising element,can significantly lower the α2/βtransition temperature of the compound and thus strongly affect,thermodynamically and dynamically,the transformation process of β→α2(or O-phase).
Key words:  hydrogen      hydrogenation      Ti_3Al-based intermetallic      microstructure     
Received:  18 June 1994     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I6/257

1WeykampHT,BakerDR,PaxtonDM,KanfmanMJ.ScriptaMetall,1990:24:4452PatersJA,BassiC.ScriptaMetall.,1990;24:9153GogiaAK,BanerjeeD,NandyTK.MetallTrans,1990;21A:6094ChenZ,SimcaF,CopeMT.MaterSci&Tech,1992;8:7295SaqibM,ApgarLS,EylonD,WeissI.SeventhWorldConferenceonTitanium,June28-July2,1992,SanDiego,USA6ChuWY,ThompsonAW.In:MoodyNRetal.eds.,HydrogenEffectsonMaterialBehaviorTMSWarrendale,1990;2857FroesFH,EylonD.In:MoodyNRetal.eds.,HydrogenEffectsonMaterialBehaviorTMSWarrendale,1990;2618KerrWK.MetallTrans,1985;16A:10779MassalskiTBetaleds.,BinaryAlloyPhaseDiagrams,Vol.2ASM,1990;206810BlackburnMJ,SmithMP.TechnicalReport,AFWAL-TR-4086,Daytou,OH198211BaselackⅢWA,BroderickT.ScriptaMetall,1990;24:61712WardCH,WilliamsJC,ThompsonAW.ScriptaMetall,1990;24:61713.ChoW,ThompsonAW,WilliamsJC.MetallTrans,1990;21A:64114YangK,GuoZX,EdmondsDV.ScriptaMelall,1992;27:1021f
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[3] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[4] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[5] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[6] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[11] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[12] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[13] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[14] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[15] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
No Suggested Reading articles found!