Research Progress in High-Performance Ultrahigh-Pressure Treated Magnesium Alloys
FU Hui1, SUN Yong2, ZOU Guodong2, ZHANG Fan1, YANG Xusheng3, ZHANG Tao1, PENG Qiuming2()
1 School of Physics and Materials Science, Guangzhou University, Guangzhou 510006, China 2 State Key Laboratory of Metastable Materials Science and Technology, Yanshan University, Qinhuangdao 066004, China 3 Department of Industrial and Systems Engineering, The Hong Kong Polytechnic University, Hong Kong 999077, China
Cite this article:
FU Hui, SUN Yong, ZOU Guodong, ZHANG Fan, YANG Xusheng, ZHANG Tao, PENG Qiuming. Research Progress in High-Performance Ultrahigh-Pressure Treated Magnesium Alloys. Acta Metall Sin, 2025, 61(3): 475-487.
Magnesium alloys are the lightest metallic structural materials. The density of magnesium alloys is ~1.7 g/cm3, which is ~2/3 of the aluminum alloy, ~2/5 of titanium alloys, and ~1/4 of steel. Magnesium alloys possess high specific strength, excellent casting performance, excellent biocompatibility, good electromagnetic shielding performance, remarkable damping performance, and ease of recovery. They have broad application potential in aerospace, defense, automobile transportation, biomedical, electronic 3C, construction, and energy fields. China has substantial Mg resources. The development of low-cost and high-performance magnesium alloys in the lightweight field can transform resource advantages into industrial benefits while promoting energy conservation and emission reduction in production and daily life. This is strategically significant for the enhancement of the country's technology industry and the achievement of the objectives of “carbon peak and carbon neutrality”. However, commercial magnesium alloys currently possess relatively low strength, poor ductility, and corrosion resistance compared with common metallic structural materials like steel and aluminum alloys, significantly hindering the large-scale industrial application of magnesium alloys as structural materials. Many methods exist to enhance the comprehensive mechanical properties of magnesium alloys. Conventionally, the microstructure of magnesium alloys can be modified by adding alloying elements, plastic deformation, and heat treatment. The strength of magnesium alloys can be improved through grain refinement, work hardening, solid solution strengthening, and precipitation strengthening. Nevertheless, magnesium alloys prepared through these traditional methods can achieve excellent strength but at the expense of ductility, leading to the strength-ductility tradeoff in the magnesium alloy. At present, ultrahigh-pressure (UHP) treatment technology can achieve novel phases and modified microstructures that cannot be prepared under atmospheric pressure. The pressure significantly impacts the thermodynamics and dynamic parameters of metallic materials, such as the equilibrium temperature, critical radius for nucleation, interfacial free energy, chemical potential, entropy, enthalpy and heat capacity, and nucleation rate. Thus, the solid solubility, grain size, morphologies, dislocation density and types, twin types and morphologies, as well as the distribution and morphologies of the intermetallic phases of the magnesium alloys, can be modified using UHP treatment combined with temperature. It offers significant potential for altering the microstructure of magnesium alloys, providing new paths to break the bottlenecks between the comprehensive properties. This paper summarizes the progress of the research on the UHP treatment of high-performance magnesium alloys, the fabrication technology, and the technical characteristics of the UHP treatment. Moreover, the effects of UHP treatment on the mechanical properties, corrosion resistance, and hydrogen storage properties of magnesium alloys by modifying the microstructures of magnesium alloys are emphasized. Finally, the future development directions of the UHP magnesium alloys are explored.
Fund: Ministry of Education Yangtze River Scholar Professor Program(T2020124);National Natural Science Foundation of China(52371104);National Natural Science Foundation of China(52171126);National Natural Science Foundation of China(52202374);National Natural Science Foundation of China(52331003);Guangdong Basic and Applied Basic Research Foundation(2024A1515013052);Guangzhou Basic and Applied Basic Research Special Project(2024A04J4289);HK PolyU grant(1-YXB4)
Corresponding Authors:
PENG Qiuming, professor, Tel: (0335)8057047, E-mail: pengqiuming@ysu.edu.cn
Fig.1 Schematics of the common ultrahigh-pressure (UHP) treatment equipments
Fig.2 OM images of Mg-30Al samples under different states[9] (A—snowflake-like Mg matrix, B—eutectic phase, SHP—super-high pressure. 800, 950, 1050, and 1150 represent 800, 950, 1050 and 1150 oC, respectively) (a) as-cast (b) SHP-2 GPa-800 (c) SHP-2 GPa-950 (d) SHP-4 GPa-1050 (e) SHP-4 GPa-1150
Fig.3 Phase fraction of β-Li phase (a) and typical TEM (b) and scanning transmission electron microscopy (STEM) (c) images of dual-phase Mg-8Li alloys treated at 1000 oC under 6 GPa[6] (LAGB—low angle grain boundary, MTB—macrotwin boundary, NTB—nanotwin boundary)
Fig.4 Comparisons of the yield strength and fracture ductility of UHPed Mg-Li-x alloys[6,26,28,29]
Fig.5 Summary of effects of the UHP on the microstructure of the Mg-Al, Mg-Li, and Mg-RE alloys
Fig.6 Near-in-situ SEM images of surfaces of 4 GPa-900 Mg-13Li sample immersed in 3.5%NaCl (mass fraction) solution for 5 min (a), 15 min (b), 30 min (c), 60 min (d), 90 min (e), and 120 min (f)[12]
Fig.7 OM (a, c, e, f) and SEM (b, d) images of Mg-5Ni alloys with different states (1100, 1400, and 1600 represent 1100, 1400, and 1600 oC, respectively)[54] (a, b) as-cast sample (c, d) 6 GPa-1100 (e) 6 GPa-1400 (f) 6 GPa-1600
1
Peng L M, Deng Q C, Wu Y J, et al. Additive manufacturing of magnesium alloys by selective laser melting technology: A review [J]. Acta Metall. Sin., 2023, 59: 31
doi: 10.11900/0412.1961.2022.00166
Peng X, Liu W C, Wu G H. Strengthening-toughening methods and mechanisms of Mg-Li alloy: A review [J]. Rare Met., 2022, 41: 1176
3
Nie J F, Shin K S, Zeng Z R. Microstructure, deformation, and property of wrought magnesium alloys [J]. Metall. Mater. Trans., 2020, 51A: 6045
4
Yue Y H, Gao Y F, Hu W T, et al. Hierarchically structured diamond composite with exceptional toughness [J]. Nature, 2020, 582: 370
5
Ge B C, Fu H, Deng K K, et al. Unique strengthening mechanisms of ultrahigh pressure Mg alloys [J]. Bioact. Mater., 2018, 3: 250
doi: 10.1016/j.bioactmat.2017.11.009
pmid: 29744464
6
Fu H, Ge B C, Xin Y C, et al. Achieving high strength and ductility in magnesium alloys via densely hierarchical double contraction nanotwins [J]. Nano Lett., 2017, 17: 6117
doi: 10.1021/acs.nanolett.7b02641
pmid: 28857573
7
Wang L, Lin X P, Xu C, et al. The microstructure and the mechanical property of AZ91D solidified under GPa-grade high-pressure [J]. Mater. Sci. Technol., 2019, 35: 1690
8
Peng Q M, Sun Y, Wang J, et al. Structural characteristics of $\left\{ 10\bar{1}1 \right\}$ contraction twin-twin interaction in magnesium [J]. Acta Mater., 2020, 192: 60
9
Zhao S S, Peng Q M, Li H, et al. Effects of super-high pressure on microstructures, nano-mechanical behaviors and corrosion properties of Mg-Al alloys [J]. J. Alloys Compd., 2014, 584: 56
10
Fu H, Peng Q M, Guo J X, et al. High-pressure synthesis of a nanoscale YB12 strengthening precipitate in Mg-Y alloys [J]. Scr. Mater., 2014, 76: 33
11
Feng J W, Li H N, Deng K K, et al. Unique corrosion resistance of ultrahigh pressure Mg-25Al binary alloys [J]. Corros. Sci., 2018, 143: 229
12
Feng J W, Zhang H, Zhang L, et al. Microstructure and corrosion properties for ultrahigh-pressure Mg-Li alloys [J]. Corros. Sci., 2022, 206: 110519
13
Yang H, Ding Z, Li Y T, et al. Recent advances in kinetic and thermodynamic regulation of magnesium hydride for hydrogen storage [J]. Rare Met., 2023, 42: 2906
14
Ouyang L Z, Liu F, Wang H, et al. Magnesium-based hydrogen storage compounds: A review [J]. J. Alloys Compd., 2020, 832: 154865
15
Wu C, Yang S Q, Li Y, et al. Microstructural evolution and electrochemical properties of the ultra-high pressure treated La0.70Mg0.30Ni3.3 hydrogen storage alloy [J]. J. Alloys Compd., 2016, 665: 231
16
Pimenta Martins L G, Comin R, Matos M J S, et al. High-pressure studies of atomically thin van der Waals materials [J]. Appl. Phys. Rev., 2023, 10: 011313
17
Tang Y, Wang H K, Ouyang X P, et al. Overcoming strength-ductility tradeoff with high pressure thermal treatment [J]. Nat. Commun., 2024, 15: 3932
doi: 10.1038/s41467-024-48435-6
pmid: 38729936
18
Bridgman P W. Recent work in the field of high pressures [J]. Rev. Mod. Phys., 1946, 18: 1
19
Schilling J S. The use of high pressure in basic and materials science [J]. J. Phys. Chem. Solids, 1998, 59: 553
20
Wu B L, Chen B, Wang C W, et al. Corrosion behavior of a novel Mg-13Li-X alloy with different grain sizes by rapid solidification rate [J]. Rare Met., 2022, 41: 3197
21
Sobczak J J, Drenchev L, Asthana R. Effect of pressure on solidification of metallic materials [J]. Int. J. Cast Met. Res., 2012, 25: 1
22
Nie J F. Precipitation and hardening in magnesium alloys [J]. Metall. Mater. Trans., 2012, 43A: 3891
23
Lin X P, Dai P L, Xu C, et al. Solute redistribution and mechanism of structure refinement of Mg-Al alloy during solidification under high pressure [J]. J. Alloys Compd., 2022, 910: 164777
24
Peng X, Liu W C, Wu G H, et al. Plastic deformation and heat treatment of Mg-Li alloys: A review [J]. J. Mater. Sci. Technol., 2022, 99: 193
doi: 10.1016/j.jmst.2021.04.072
25
Ge B C, Yang M, Zu Q, et al. Lithium cluster segregation in coherent contraction twin boundaries of magnesium alloys [J]. Acta Mater., 2020, 201: 477
26
Peng Q M, Ge B C, Fu H, et al. Nanoscale coherent interface strengthening of Mg alloys [J]. Nanoscale, 2018, 10: 18028
doi: 10.1039/c8nr04805c
pmid: 30229782
27
Peng Q M, Sun Y, Ge B C, et al. Interactive contraction nanotwins-stacking faults strengthening mechanism of Mg alloys [J]. Acta Mater., 2019, 169: 36
28
Zhang S, Sun Y, Wu R Z, et al. Coherent interface strengthening of ultrahigh pressure heat-treated Mg-Li-Y alloys [J]. J. Mater. Sci. Technol., 2020, 51: 79
doi: 10.1016/j.jmst.2020.02.039
29
Wang D, Huang P Z, Wu R Z, et al. Synergistically improved strength and damping capacity of Mg-Li-Y-Er-Zn-Zr alloy by ultra-high pressure treatment [J]. Mater. Sci. Eng, 2024, A915: 147205
30
Meier J M, Caris J, Luo A A. Towards high strength cast Mg-RE based alloys: Phase diagrams and strengthening mechanisms [J]. J. Magnes. Alloy., 2022, 10: 1401
31
Zhao H G, Pan J L, Li H, et al. Spherical strengthening precipitate in a Mg-10wt%Y alloy with superhigh pressure aging [J]. Mater. Lett., 2013, 96: 16
32
Fu H, Li H, Fang D Q, et al. High ductility of a bi-modal Mg-7wt.%Y alloy at low temperature prepared by high pressure boriding and semi-solid extrusion [J]. Mater. Des., 2016, 92: 240
33
Fu H, Liu N, Zhang Z W, et al. Effect of super-high pressure on microstructure and mechanical properties of Mg97Zn1Y2 alloys [J]. J. Magnes. Alloy., 2016, 4: 302
34
Matsushita M, Masuda K, Waki R, et al. Ultrafine spherulite Mg alloy with high yield strength [J]. J. Alloys Compd., 2019, 784: 1284
35
Matsushita M, Sakata Y, Senzaki T, et al. Phase relations among D03, α-Mg, and long-period stacking orders in Mg85Zn6Y9 alloy under 3 GPa [J]. Mater. Trans., 2015, 56: 910
36
Matsushita M, Yamamoto S, Nishiyama N, et al. D03 + hcp mixed phase with nanostructures in Mg85Zn6Y9 alloy obtained by high-pressure and high-temperature treatments [J]. Mater. Lett., 2015, 155: 11
37
Haque N, Cochrane R F, Mullis A M. Rapid solidification morphologies in Ni3Ge: Spherulites, dendrites and dense-branched fractal structures [J]. Intermetallics, 2016, 76: 70
38
Zhou L T, Niu T T, Zou G D, et al. High-strong-ductile magnesium alloys by interactions of nanoscale quasi-long period stacking order unit with twin [J]. J. Magnes. Alloy., 2024, 12: 4953
39
Atrens A, Shi Z M, Mehreen S U, et al. Review of Mg alloy corrosion rates [J]. J. Magnes. Alloy., 2020, 8: 989
40
Feng J W, Pan Y K, Yang M, et al. A lactoglobulin-composite self-healing coating for Mg alloys [J]. ACS Appl. Bio Mater., 2021, 4: 6843
doi: 10.1021/acsabm.1c00560
pmid: 35006984
41
Zhu Q C, Li Y X, Cao F Y, et al. Towards development of a high-strength stainless Mg alloy with Al-assisted growth of passive film [J]. Nat. Commun., 2022, 13: 5838
doi: 10.1038/s41467-022-33480-w
pmid: 36192418
42
Peng Q M, Zhao S S, Li H, et al. High pressure solidification: An effective approach to improve the corrosion properties of Mg-Y based implants [J]. Int. J. Electrochem. Sci., 2012, 7: 5581
43
Yang M, Feng J W, Hu H D, et al. Microstructure and corrosion resistance of ultrahigh pressure Mg-8Li based alloys [J]. J. Alloys Compd., 2023, 966: 171543
44
Deng M, Wang L Q, Höche D, et al. Approaching “stainless magnesium” by Ca micro-alloying [J]. Mater. Horiz., 2021, 8: 589
doi: 10.1039/d0mh01380c
pmid: 34821275
45
Xu W Q, Birbilis N, Sha G, et al. A high-specific-strength and corrosion-resistant magnesium alloy [J]. Nat. Mater., 2015, 14: 1229
doi: 10.1038/nmat4435
pmid: 26480229
46
Shang Y Y, Pistidda C, Gizer G, et al. Mg-based materials for hydrogen storage [J]. J. Magnes. Alloy., 2021, 9: 1837
47
Chen J, Sakai T, Kitamura N, et al. High-pressure synthesis of amorphous MgNi1.02H2.2 [J]. J. Am. Chem. Soc., 2001, 123: 6193
pmid: 11414860
48
Takamura H, Kakuta H, Kamegawa A, et al. Crystal structure of novel hydrides in a Mg-Ni-H system prepared under an ultra high pressure [J]. J. Alloys Compd., 2002, 330-332: 157
49
Kataoka R, Goto Y, Kamegawa A, et al. High-pressure synthesis of novel hydride in Mg-Ni-H and Mg-Ni-Cu-H systems [J]. J. Alloys Compd., 2007, 446-447: 142
50
Kataoka R, Kamegawa A, Takamura H, et al. High pressure synthesis of novel Mg (Ni1 - x Cu x )2 hydrides (x = 0-0.2) [J]. Mater. Trans., 2009, 50: 1179
51
Kataoka R, Goto Y, Kamegawa A, et al. High-pressure synthesis of novel hydride in Mg-Ni(-H) system [J]. Mater. Trans., 2006, 47: 1957
52
Kamata Y, Kuriiwa T, Kamegawa A, et al. Effect of Cu or Ti substitution in MgNi on crystal structure and hydrogen absorption-desorption properties [J]. Mater. Trans., 2009, 50: 2064
53
Peng X Y, Liu B Z, Zhao X, et al. Effects of ultra-high pressure on phase compositions, phase configurations and hydrogen storage properties of LaMg4Ni alloys [J]. Int. J. Hydrogen Energy, 2013, 38: 14661
54
Fu H, Wu W S, Dou Y, et al. Hydrogen diffusion kinetics and structural integrity of superhigh pressure Mg-5wt%Ni alloys with dendrite interface [J]. J. Power Sources, 2016, 320: 212
55
Sun Y, Wang D B, Wang J M, et al. Hydrogen storage properties of ultrahigh pressure Mg12NiY alloys with a superfine LPSO structure [J]. Int. J. Hydrogen Energy, 2019, 44: 23179
56
Torres B, Martínez-Lope M J, Alonso J A, et al. Short communication: High-pressure synthesis and crystal structure of a novel Mg3CuH x ternary hydride [J]. Int. J. Hydrogen Energy, 2013, 38: 15264
57
Kyoi D, Sato T, Rönnebro E, et al. A novel magnesium-vanadium hydride synthesized by a gigapascal-high-pressure technique [J]. J. Alloys Compd., 2004, 375: 253
58
Moser D, Bull D J, Sato T, et al. Structure and stability of high pressure synthesized Mg-TM hydrides (TM = Ti, Zr, Hf, V, Nb and Ta) as possible new hydrogen rich hydrides for hydrogen storage [J]. J. Mater. Chem., 2009, 19: 8150
59
Goto Y, Kakuta H, Kamegawa A, et al. High-pressure synthesis of novel hydride in Mg-M systems (M = Li, Pd) [J]. J. Alloys Compd., 2005, 404-406: 448
60
Retuerto M, Sánchez-Benítez J, Rodríguez-Cañas E, et al. High-pressure synthesis of Mg2FeH6 complex hydride [J]. Int. J. Hydrogen Energy, 2010, 35: 7835
61
Goto Y, Kamegawa A, Takamura H, et al. Synthesis of new hydrides in Mg-Y systems by using high pressure [J]. Mater. Trans., 2002, 43: 2717