Evolution and Healing Mechanism of 1Cr22Mn16N High Nitrogen Austenitic Stainless Steel Interface Microstructure During Plastic Deformation Bonding
YANG Ruize1,2,3, ZHAI Ruzong1,2, REN Shaofei1,2, SUN Mingyue1,2(), XU Bin1,2, QIAO Yanxin3(), YANG Lanlan3
1 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
2 CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
3 School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003, China
Cite this article: 

YANG Ruize, ZHAI Ruzong, REN Shaofei, SUN Mingyue, XU Bin, QIAO Yanxin, YANG Lanlan. Evolution and Healing Mechanism of 1Cr22Mn16N High Nitrogen Austenitic Stainless Steel Interface Microstructure During Plastic Deformation Bonding. Acta Metall Sin, 2024, 60(7): 915-925.

Download:  HTML  PDF(4134KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

High nitrogen austenitic stainless steels (HNASSs) are widely used for their good wear resistance and high strength, plasticity, and corrosion resistance. Among these steels, 1Cr22Mn16N HNASS improves the cost effectiveness because of the incorporation of a N element in place of the expensive Ni element. In addition, the overall mechanical properties of the steel are further improved because of the solid solution-strengthening effect of the N element. However, the traditional welding methods such as arc welding, tungsten gas shielded welding, and friction stir welding are not suitable for 1Cr22Mn16N HNASS welding because of the different solubility of N in the liquid and solid phases. N easily spills out during the welding process, which considerably degrades the mechanical properties of the welded joints. Therefore, a new welding method needs to be explored to solve the problems in 1Cr22Mn16N welding. In this work, the bonding technology of plastic deformation was introduced to solve the poor performance problems of 1Cr22Mn16N HNASS welded joints. The experiments were conducted through the Glebble 3500 thermomechanical simulation in the temperature range of 1050-1250oC and a strain range of 10%-40% with a strain rate of 0.1 s-1. The microstructure evolution of the bonding interface was characterized and investigated using OM, EBSD, and TEM; the interface healing mechanism was discussed, and the bonding strength of the joint was evaluated by tensile test. The results show that the bonding level of the interface substantially increases with the increase in deformation and temperature. When the deformation temperature reached 1200oC and the strain reached 40%, the mechanical properties of the bonding interface reached up to the same level as the matrix. During the process of deformation, discontinuous dynamic recrystallization (DDRX) occurred at the interface because of thermomechanical coupling; meanwhile, dislocations accumulated and entanglement occurred under the action of stress, forming a large number of subgrain boundaries within the original grain boundaries near the interface, which, lead to continuous dynamic recrystallization (CDRX). The healing of the interface was achieved by the synergistic effect of CDRX and DDRX.

Key words:  high-nitrogen austenitic stainless steel      plastic deformation bonding      dynamic recrystallization     
Received:  09 January 2023     
ZTFLH:  TG406  
Fund: National Key Research and Development Program of China(2018YFA0702900);National Natural Science Foundation of China(52173305);National Natural Science Foundation of China(52101061);National Natural Science Foundation of China(52233017);National Natural Science Foundation of China(52203384)
Corresponding Authors:  SUN Mingyue, professor, Tel: (024)83971018, E-mail: mysun@imr.ac.cn;

URL: 

https://www.ams.org.cn/EN/10.11900/0412.1961.2023.00015     OR     https://www.ams.org.cn/EN/Y2024/V60/I7/915

Fig.1  Schematics of the experimental method and sample size (unit: mm)
(a) experimental method of plastic deformation bonding (b) samples before and after deformation
(c) experimental method of tensile butt-joint (The top schematic shows a butt-joint specimen; the bottom schematic shows the sample of the base material)
(d) tensile sample before compression
Fig.2  Inverse pole figure (IPF) of microstructure of 1Cr22Mn16N high nitrogen austenitic stainless steel (HNASS)
Fig.3  OM images of interface in 1Cr22Mn16N HNASS at different deformation temperatures with 0.1 s-1 strain rate and 20% strain
Fig.4  OM images of interface in 1Cr22Mn16N HNASS at 1200oC and deformations of 10% (a), 20% (b), 30% (c), and 40% (d); and average grain size diagram (e)
Fig.5  Room temperature tensile curves of the bonding joints (BJs) and base materials (BMs) with deformations of 20% and 40%
Fig.6  Tensile fracture morphologies of BJs (a, c) and BMs (b, d) at deformations of 20% (a, b) and 40% (c, d) (Insets show the macrostructures of fracture)
Fig.7  IPFs (a, d, g, j),geometrically necessary dislocation (GND) maps (b, e, h, k), and grain orientation spread (GOS) maps (c, f, i, l) of interface microstructures under deformations of 10% (a-c), 20% (d-f), 30% (g-i), and 40% (j-l) at 1200oC (CDRX—continuous dynamic recrystallization, DDRX—discontinuous dynamic recrystallization, LAGB—low angle grain boundary, MAGB—middle angle grain boundary, HAGB—high angle grain boundary)
Fig.8  Misorientation angle distributions of samples under different deformations at 1200oC (Inset shows the magnified MAGB occupancy)
Fig.9  TEM images of interface structure at 1200oC and 20% strain
(a) DRX grain (b) subgrain boundary
Fig.10  Schematics of healing mechanism of bonding interface during plastic deformation bonding
(a) deformation (b) grain boundary bow (c) dislocation accumulation
(d) increased dynamic recrystallization (DRX) (e) interface bonding
1 Zhang X Y, Zhou Q, Wang K H., et al. Study on microstructure and tensile properties of high nitrogen Cr-Mn steel processed by CMT wire and arc additive manufacturing [J]. Mater. Des., 2019, 166: 107611
2 Gavriljuk V G, Berns H. High Nitrogen Steels [M]. Berlin: Springer, 1999: 135
3 Lang Y P, Zhou Y, Rong F, et al. Hot working of high nitrogen austenitic stainless steel [J]. J. Iron Steel Res. Int., 2010, 17: 45
4 Bott A H, Pickering F B, Butterworth G J. Development of high manganese high nitrogen low activation austenitic stainless steels [J]. J. Nucl. Mater., 1986, 141-143: 1088
5 Simmons J W. Overview: High-nitrogen alloying of stainless steels [J]. Mater. Sci. Eng., 1996, A207: 159
6 Harzenmoser M. Welding of high nitrogen steels [J]. Mater. Manuf. Processes, 2004, 19: 75
7 Du Toit M, Pistorius P C. Nitrogen control during autogenous arc welding of stainless steel—Part 1: Experimental observations [J]. Trans. Weld. J.., 2003, 82:219
8 Mohammed R, Reddy G M, Rao K S. Welding of nickel free high nitrogen stainless steel: Microstructure and mechanical properties [J]. Def. Technol., 2017, 13: 59
doi: 10.1016/j.dt.2016.06.003
9 Zhao L, Tian Z L, Peng Y, et al. Laser welding of high nitrogen steel 1Cr22Mn16N Ⅲ. Microstructure and mechanical properties of welding heat-affected zone [J]. Trans. China Weld. Inst., 2007, 28(12): 26
赵 琳, 田志凌, 彭 云 等. 1Cr22Mn16N高氮钢的激光焊接Ⅲ.焊接热影响区组织和性能 [J]. 焊接学报, 2007, 28(12): 26
10 Kamiya O, Chen Z W, Kikuchi Y. Microporosity formation in partially melted zone during welding of high nitrogen austenitic stainless steels [J]. J. Mater. Sci., 2002, 37: 2475
11 Qiang W, Wang K H. Shielding gas effects on double-sided synchronous autogenous GTA weldability of high nitrogen austenitic stainless steel [J]. J. Mater. Process. Technol., 2017, 250: 169
12 Zhang H, Wan D, Xue P, et al. Research advances on homogenization manufacturing of heavy components by metal additive forging [J]. J. Mater. Sci. Technol., 2018, 34: 2183e8
doi: 10.1016/j.jmst.2018.03.014
13 Sun M Y, Xu B, Xie B J, et al. Research progress of homogenized construction and forming of heavy forgings [J]. Chin. Sci. Bull., 2020, 65: 3043
孙明月, 徐 斌, 谢碧君 等. 大锻件均质化构筑成形研究进展 [J]. 科学通报, 2020, 65: 3043
14 Zhang J Y, Xu B, Tariq N H, et al. Microstructure evolutions and interfacial bonding behavior of Ni-based superalloys during solid state plastic deformation bonding [J]. J. Mater. Sci. Technol., 2020, 46: 1
doi: 10.1016/j.jmst.2019.11.015
15 Zhou L Y, Feng S B, Sun M Y, et al. Interfacial microstructure evolution and bonding mechanisms of 14YWT alloys produced by hot compression bonding [J]. J. Mater. Sci. Technol., 2019, 35: 1671
doi: 10.1016/j.jmst.2019.04.005
16 Xie B J, Sun M Y, Xu B, et al. Dissolution and evolution of interfacial oxides improving the mechanical properties of solid state bonding joints [J]. Mater. Des., 2018, 157: 437
17 Xie B J, Sun M Y, Xu B, et al. Oxidation of stainless steel in vacuum and evolution of surface oxide scales during hot-compression bonding [J]. Corros. Sci., 2019, 147: 41
18 Zhang J Y, Sun M Y, Xu B, et al. Evolution of the interfacial microstructure during the plastic deformation bonding of copper [J]. Mater. Sci. Eng., 2019, A746 : 1
19 Jiang H Y, Sun M Y, Wu M F, et al. Microstructure and properties of 7075 aluminum alloy hot compress bonding joint [J]. Heat Treat. Met., 2020, 45(2): 46
江海洋, 孙明月, 吴铭方 等. 7075铝合金热变形连接接头的组织与性能 [J]. 金属热处理, 2020, 45(2): 46
doi: 10.13251/j.issn.0254-6051.2020.02.009
20 Ren S F, Zhang J Y, Zhang X F, et al. Evolution of interfacial microstructure of Ni-Co base superalloy during plastic deformation bonding and its bonding mechanism [J]. Acta Metall. Sin., 2022, 58: 129
doi: 10.11900/0412.1961.2020.00493
任少飞, 张健杨, 张新房 等. 新型Ni-Co基高温合金塑性变形连接中界面组织演化及愈合机制 [J]. 金属学报, 2022, 58: 129
doi: 10.11900/0412.1961.2020.00493
21 Miura H, Ozama M, Mogawa R, et al. Strain-rate effect on dynamic recrystallization at grain boundary in Cu alloy bicrystal [J]. Scr. Mater., 2003, 48: 1501
22 Wang Y, Shao W Z, Zhen L, et al. Flow behavior and microstructures of superalloy 718 during high temperature deformation[J]. Mater. Sci. Eng., 2008, A497: 479
23 Mandal S, Jayalakshmi M, Bhaduri A K, et al. Effect of strain rate on the dynamic recrystallization behavior in a nitrogen-enhanced 316L(N) [J]. Metall. Mater. Trans., 2014, 45A: 5645
24 Wang X Y, Wang D K, Jin J S, et al. Effects of strain rates and twins evolution on dynamic recrystallization mechanisms of austenite stainless steel [J]. Mater. Sci. Eng., 2019, A761: 138044
25 Humphrey F J, Hatherly M. Recrystallization and Related Annealing Phenomena [M]. 2nd Ed., Amsterdam: Elsevier, 2004: 427
26 Sakai T, Belyakov A, Kaibyshev R, et al. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions [J]. Prog. Mater. Sci., 2014, 60: 130
27 Sakai T, Jonas J J. Overview no.35 Dynamic recrystallization: Mechanical and microstructural considerations [J]. Acta Metall., 1984, 32: 189
28 Jonas J J, Sellars C M, Tegart W J M. Strength and structure under hot-working conditions [J]. Metall. Rev., 1969, 14: 1
29 Doherty R D, Hughes D A, Humphreys F J, et al. Current issues in recrystallization: A review [J]. Mater. Sci. Eng., 1997, A238: 219
30 Huang K, Logé R E. A review of dynamic recrystallization phenomena in metallic materials [J]. Mater. Des., 2016, 111: 548
31 Hu G D, Wang P, Li D Z, et al. Effects of nitrogen on precipitation and tensile behaviors of 25Cr 20Ni austenitic stainless steels at elevated temperatures [J]. Mater. Sci. Eng., 2019, A752: 93
32 Zhong X T, Wang L, Liu F. Study on formation mechanism of necklace structure in discontinuous dynamic recrystallization of Incoloy 028 [J]. Acta Metall. Sin., 2018, 54: 969
doi: 10.11900/0412.1961.2017.00461
钟茜婷, 王 磊, 刘 峰. Incoloy 028合金不连续动态再结晶中链状组织形成机理研究 [J]. 金属学报, 2018, 54: 969
doi: 10.11900/0412.1961.2017.00461
33 Souza R C, Silva E S, Jorge A M, et al. Dynamic recovery and dynamic recrystallization competition on a Nb- and N-bearing austenitic stainless steel biomaterial: Influence of strain rate and temperature [J]. Mater. Sci. Eng., 2013, A582: 96
34 Sakai T. Dynamic recrystallization microstructures under hot working conditions [J]. J. Mater. Process. Technol., 1995, 53: 349
35 Hu G X, Cai X, Rong Y H. Fundamentals of Materials Science [M]. 3rd Ed., Shanghai: Shanghai Jiao Tong University Press, 2010: 5
胡赓祥, 蔡 珣, 戎咏华. 材料科学基础 [M]. 第 3版, 上海: 上海交通大学出版社, 2010: 5
36 Paggi A, Angella G, Donnini R. Strain induced grain boundary migration effects on grain growth of an austenitic stainless steel during static and metadynamic recrystallization [J]. Mater. Charact, 2015, 107: 174
37 Dudova N, Belyakov A, Sakai T, et al. Dynamic recrystallization mechanisms operating in a Ni-20%Cr alloy under hot-to-warm working [J]. Acta Mater., 2010, 58: 3624
38 Xie B C, Yu H, Sheng T, et al. DDRX and CDRX of an as-cast nickel-based superalloy during hot compression at γ′ sub-/super-solvus temperatures [J]. J. Alloys Compd., 2019, 803: 16
39 Kubota M, Ushioda K, Miyamoto G, et al. Analysis of recrystallization behavior of hot-deformed austenite reconstructed from electron backscattering diffraction orientation maps of lath martensite [J]. Scr. Mater., 2016, 112: 92
40 Kim J M, Kim S J, Kang J H. Effects of short-range ordering and stacking fault energy on tensile behavior of nitrogen-containing austenitic stainless steels [J]. Mater. Sci. Eng., 2022, A836: 142730
41 Kumar S, Samantaray D, Aashranth B, et al. Dependency of rate sensitive DRX behaviour on interstitial content of a Fe-Cr-Ni-Mo alloy [J]. Mater. Sci. Eng., 2019, A743: 148
[1] CHEN Shenghu, WANG Qiyu, JIANG Haichang, RONG Lijian. Effect of δ-Ferrite on Hot Deformation and Recrystallization of 316KD Austenitic Stainless Steel for Sodium-Cooled Fast Reactor Application[J]. 金属学报, 2024, 60(3): 367-376.
[2] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[3] LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature[J]. 金属学报, 2023, 59(11): 1439-1447.
[4] WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo. Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy[J]. 金属学报, 2022, 58(7): 932-942.
[5] REN Shaofei, ZHANG Jianyang, ZHANG Xinfang, SUN Mingyue, XU Bin, CUI Chuanyong. Evolution of Interfacial Microstructure of Ni-Co Base Superalloy During Plastic Deformation Bonding and Its Bonding Mechanism[J]. 金属学报, 2022, 58(2): 129-140.
[6] JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge. Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. 金属学报, 2022, 58(12): 1545-1556.
[7] NI Ke, YANG Yinhui, CAO Jianchun, WANG Liuhang, LIU Zehui, QIAN Hao. Softening Behavior of 18.7Cr-1.0Ni-5.8Mn-0.2N Low Nickel-Type Duplex Stainless Steel During Hot Compression Deformation Under Large Strain[J]. 金属学报, 2021, 57(2): 224-236.
[8] CHEN Wenxiong, HU Baojia, JIA Chunni, ZHENG Chengwu, LI Dianzhong. Post-Dynamic Softening of Austenite in a Ni-30%Fe Model Alloy After Hot Deformation[J]. 金属学报, 2020, 56(6): 874-884.
[9] ZHANG Yang, SHAO Jianbo, CHEN Tao, LIU Chuming, CHEN Zhiyong. Deformation Mechanism and Dynamic Recrystallization of Mg-5.6Gd-0.8Zn Alloy During Multi-Directional Forging[J]. 金属学报, 2020, 56(5): 723-735.
[10] ZHANG Yong, LI Xinxu, WEI Kang, WAN Zhipeng, JIA Chonglin, WANG Tao, LI Zhao, SUN Yu, LIANG Hongyan. Hot Deformation Characteristics of Novel Wrought Superalloy GH4975 Extruded Rod Used for 850 ℃ Turbine Disc[J]. 金属学报, 2020, 56(10): 1401-1410.
[11] WU Huajian, CHENG Renshan, LI Jingren, XIE Dongsheng, SONG Kai, PAN Hucheng, QIN Gaowu. Effect of Al Content on Microstructure and Mechanical Properties of Mg-Sn-Ca Alloy[J]. 金属学报, 2020, 56(10): 1423-1432.
[12] Xu LI,Qingbo YANG,Xiangze FAN,Yonglin GUO,Lin LIN,Zhiqing ZHANG. Influence of Deformation Parameters on Dynamic Recrystallization of 2195 Al-Li Alloy[J]. 金属学报, 2019, 55(6): 709-719.
[13] Yahui DENG,Yinhui YANG,Jianchun CAO,Hao QIAN. Research on Dynamic Recrystallization Behavior of 23Cr-2.2Ni-6.3Mn-0.26N Low Nickel TypeDuplex Stainless Steel[J]. 金属学报, 2019, 55(4): 445-456.
[14] Xiting ZHONG, Lei WANG, Feng LIU. Study on Formation Mechanism of Necklace Structure in Discontinuous Dynamic Recrystallization of Incoloy 028[J]. 金属学报, 2018, 54(7): 969-980.
[15] Yusen SU, Yinhui YANG, Jianchun CAO, Yuliang BAI. Research on Hot Working Behavior of Low-NickelDuplex Stainless Steel 2101[J]. 金属学报, 2018, 54(4): 485-493.
No Suggested Reading articles found!