Acta Metall Sin  2019, Vol. 55 Issue (2): 181-190    DOI: 10.11900/0412.1961.2018.00187
Orginal Article Current Issue | Archive | Adv Search |
The Influence of Rolling Process on the Microstructure, Texture and Magnetic Properties of Low Grades Non-Oriented Electrical Steel After Phase Transformation Annealing
Chen GU, Ping YANG(), Weimin MAO
School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China
Cite this article: 

Chen GU, Ping YANG, Weimin MAO. The Influence of Rolling Process on the Microstructure, Texture and Magnetic Properties of Low Grades Non-Oriented Electrical Steel After Phase Transformation Annealing. Acta Metall Sin, 2019, 55(2): 181-190.

Download:  HTML  PDF(6361KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Non-oriented electrical steel sheets are important metallic functional materials for the iron cores in transformers and electrical motors, which require the performance characteristics of low iron loss and high magnetic induction. The magnetic properties of electrical steel critically depend on the microstructure and the occurring texture components. In addition, alloy elements can affect the magnetic properties by altering the electrical resistivity, microstructure and texture. At present, the quality of commercial non-oriented electrical steels are mainly optimized by the control of deformation, recrystallization parameters and chemical composition. And the microstructure, texture and magnetic properties are significantly influenced by the rolling process before recrystallization annealing. The favorite {100} texture in such condition takes at maximum only about 20% in volume fraction. In contrast, phase transformation combined with deformation can lead to nearly 80% volume fraction of {100}-oriented grains. In this work, the influence of rolling process on the microstructure, texture and magnetic properties of low grades non-oriented electrical steel after phase transformation annealing was studied by means of EBSD, XRD and magnetism measuring techniques. The starting material is a columnar-grained industrial low grades electrical steel cast slab. Five different initial microstructures are obtained after different rolling processes, the α→γ→α phase transformation annealing of samples is conducted in a tube furnace under H2 atmosphere. The results show that phase transformation annealing can significantly coarsen grains and reduce the iron loss of non-oriented electrical steels compared with traditional recrystallization annealing. And the phase transformation texture is influenced by texture memory. Compared with hot rolling-cold rolling process, more {100}-oriented grains are obtained and the magnetic properties of non-oriented electrical steels are improved significantly after phase transformation in the directly cold rolling process. The proportion of non-{111} oriented grains increases and more initial {100}-oriented grains are retained after phase transformation in the process with lower hot rolling temperature, which improve the magnetic properties of final sample. In addition, the presence of P and Al elements in commercial electrical steels may affect the microstructure, texture and magnetic properties of non-oriented electrical steels due to segregation and oxidation after phase transformation.

Key words:  non-oriented electrical steel      rolling process      texture memory      phase transformation      chemical element     
Received:  10 May 2018     
ZTFLH:  TG111  
Fund: Supported by National Natural Science Foundation of China (No.51771024)

URL: 

https://www.ams.org.cn/EN/10.11900/0412.1961.2018.00187     OR     https://www.ams.org.cn/EN/Y2019/V55/I2/181

Processing route Hot rolling Cold rolling
A Holding at 1150 ℃ for 30 min, hot rolling by 3 passes and air cooling, 2 mm thickness in hot band, 80% rolling reduction Cold rolling to 0.35 mm (82.5%)
B
Holding at 1150 ℃ for 30 min, hot rolling to 4 mm, then reheating at 1150 ℃ for 5 min followed by 2 passes to 2 mm thickness, air cooling, 50% rolling reduction Cold rolling to 0.35 mm (82.5%)
C The same as route A except heating at 1100 ℃, air cooling, 80% rolling reduction, 2 mm thickness Cold rolling to 0.35 mm (82.5%)
D The same as route C, water cooling Cold rolling to 0.35 mm (82.5%)
E - Direct cold rolling to 0.35 mm (82.5%)
Table 1  The rolling process before final transformation treatment
Fig.1  Macrostructure and EBSD data of the cast slab (φ1, ?, and φ2 are the Euler angles, which form a three-dimensional orientation space; RD, TD and ND represent rolling direction, transverse direction and normal direction of the sheets, respectively)
(a) macrostructure
(b) orientation distribution function (ODF) at φ2=45° section
(c) {200} pole figure
(d) IPF-X (projection of the grain orientations that are parallel to RD in the crystal coordinate system) map (IPF—inverse pole figure)
(e) Kikuchi band quality map
Fig.2  EBSD data of annealed sample for commercial 1300 grade non-oriented electrical steel
(a) IPF-Z (projection of the grain orientations that are parallel to ND in the crystal coordinate system) map for rolling plane
(b) {200} pole figure
(c) ODF at φ2=45° section
Fig.3  IPF-Z maps (a~d) and ODFs at φ2=45° section (e~h) for through-thickness cross section of hot rolling samples in processes A (a, e), B (b, f), C (c, g) and D (d, h), respectively
Fig.4  ODFs at φ2=45° section of texture on the surface of cold rolled samples in the processes A (a), B (b), C (c), D (d) and E (e), respectively
Fig.5  IPF-Z maps (a~e) and ODFs (φ2=45°) (f~j) for through thickness cross section of annealed samples in the rolling processes A (a, f), B (b, g), C (c, h), D (d, i) and E (e, j), respectively
Fig.6  Average grain sizes of annealed samples in different rolling processes
Fig.7  Iron loss (P1.5) (a) and magnetic induction (B50) (b) of transformation annealed samples in different rolling processes
Fig.8  Glow discharge spectrum (GDS) data profiles for the annealed sample in process C
(a) O, Si, Al, P profile after annealing within 2.0 μm from the surface
(b) Al, P profile after annealing within 1.0 μm from the surface
(c) P profiles after annealing within 1.0 μm from the surface
[1] Hou C K.Effect of silicon on the loss separation and permeability of laminated steels[J]. J. Magn. Magn. Mater., 1996, 162: 280
[2] Ghosh P, Chromik R R, Knight A M, et al.Effect of metallurgical factors on the bulk magnetic properties of non-oriented electrical steels[J]. J. Magn. Magn. Mater., 2014, 356: 42
[3] Li H Z, Liu H T, Liu Z Y, et al.Characterization of microstructure, texture and magnetic properties in twin-roll casting high silicon non-oriented electrical steel[J]. Mater. Charact., 2014, 88: 1
[4] Sung J K, Lee D N, Wang D H, et al.Efficient generation of cube-on-face crystallographic texture in iron and its alloys[J]. ISIJ Int., 2011, 51: 284
[5] Sung J K, Koo Y M. Magnetic properties of Fe and Fe-Si alloys with {100} <0vw> texture[J] J. Appl. Phys., 2013, 113: 17A338-1
[6] Tomida T.A new process to develop (100) texture in silicon steel sheets[J]. J. Mater. Eng. Perform., 1996, 5: 316
[7] Xie L, Yang P, Xia D S, et al.Microstructure and texture evolution in a non-oriented electrical steel during γ→α transformation under various atmosphere conditions[J]. J. Magn. Magn. Mater., 2015, 374: 655
[8] Xie L, Yang P, Zhang N, et al.Formation of {100} textured columnar grain structure in a non-oriented electrical steel by phase transformation[J]. J. Magn. Magn. Mater., 2014, 356: 1
[9] Zhang L W, Yang P, Wang J H, et al.Transformation of {100} texture induced by surface effect in ultra-low carbon electrical steel[J]. J. Mater. Sci., 2016, 51: 8087
[10] Zhang L W.Research on the mechanism of {100} transformation texture induced by surface-effect in the electrical steels [D]. Beijing: University of Science and Technology Beijing, 2016(章楼文. 电工钢中表面效应诱发{100}相变织构的机理研究 [D]. 北京: 北京科技大学, 2016)
[11] Fang F, Lu X, Lan M F, et al.Effect of rolling temperature on the microstructure, texture, and magnetic properties of strip-cast grain-oriented 3% Si steel[J]. J. Mater. Sci., 2018, 53: 9217
[12] De Paepe A, Eloot K, Dilewijns J, et al.Effect of hot rolling parameters on the magnetic properties of a low-silicon ultra-low-carbon steel[J]. J. Magn. Magn. Mater., 1996, 160: 129
[13] Sidor J J, Verbeken K, Gomes E, et al.Through process texture evolution and magnetic properties of high Si non-oriented electrical steels[J]. Mater. Charact., 2012, 71: 49
[14] Fischer O,Schneider J.Influence of deformation process on the improvement of non-oriented electrical steel [J]. J. Magn. Magn. Mater., 2003, 254-255: 302
[15] Gutiérrez-Casta?eda E J, Salinas-Rodríguez A. Effect of annealing prior to cold rolling on magnetic and mechanical properties of low carbon non-oriented electrical steels[J]. J. Magn. Magn. Mater., 2011, 323: 2524
[16] Yashiki H, Okamoto A.Effect of hot-band grain size on magnetic properties of non-oriented electrical steels[J]. IEEE Trans. Magn., 1987, 23: 3086
[17] Chang S K, Huang W Y.Effect of normalizing of hot band on magnetic properties and texture in high silicon non-oriented electrical steels[J]. Steel Res. Int., 2007, 78: 340
[18] Zhang N, Yang P, Mao W M.Influence of columnar grains on the cold rolling texture evolution in Fe-3%Si electrical steel[J]. Acta Metall. Sin., 2012, 48: 782(张宁, 杨平, 毛卫民. 柱状晶对Fe-3%Si电工钢冷轧织构演变规律的影响[J]. 金属学报, 2012, 48: 782)
[19] Wang L N, Yang P, Mao W M.Analysis of martensitic transformation during tension of high manganese TRIP steel at high strain rates[J]. Acta Metall. Sin., 2016, 52: 1045(王丽娜, 杨平, 毛卫民. 高锰TRIP钢高速拉伸时的马氏体转变行为分析[J]. 金属学报, 2016, 52: 1045)
[20] Zhang L W, Yang P, Mao W M.Phenomena of Σ3 and orientation gradients in an electrical steel applied α→γ→α transformation[J]. Acta Metall. Sin., 2017, 53: 19(章楼文, 杨平, 毛卫民. 电工钢相变组织中的Σ3和取向梯度现象[J]. 金属学报, 2017, 53: 19)
[21] Tomida T, Wakita M, Yasuyama M, et al.Memory effects of transformation textures in steel and its prediction by the double Kurdjumov-Sachs relation[J]. Acta Mater., 2013, 61: 2828
[22] Lischewski I, Gottstein G.Nucleation and variant selection during the α-γ-α phase transformation in microalloyed steel[J]. Acta Mater., 2011, 59: 1530
[23] Yoshinaga N, Inoue H, Kawasaki K, et al.Factors affecting texture memory appearing through α→γ→α transformation in IF steels[J]. Mater. Trans., 2007, 48: 2036
[24] Sung J K, Lee D N.Evolution of crystallographic texture in pure iron and commercial steels by γ to α transformation [J].Mater. Sci. Forum, 2012, 706-709: 2657
[25] Nakayama T, Honjou N.Effect of aluminum and nitrogen on the magnetic properties of non-oriented semi-processed electrical steel sheet[J]. J. Magn. Magn. Mater., 2000, 213: 87
[26] Hou C K, Hu C T, Lee S.The effect of aluminium on the magnetic properties of lamination steels[J]. IEEE Trans. Magn., 1991, 27: 4305
[27] Park J T, Woo J S, Chang S K.Effect of phosphorus on the magnetic properties of non-oriented electrical steel containing 0.8 wt% silicon[J]. J. Magn. Magn. Mater., 1998, 182: 381
[28] Lee S, De Cooman B C. Effect of phosphorus on the magnetic losses of non-oriented 2% Si steel[J]. ISIJ Int., 2012, 52: 1162
[1] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[2] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[3] WANG Chongyang, HAN Shiwei, XIE Feng, HU Long, DENG Dean. Influence of Solid-State Phase Transformation and Softening Effect on Welding Residual Stress of Ultra-High Strength Steel[J]. 金属学报, 2023, 59(12): 1613-1623.
[4] ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping. Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes[J]. 金属学报, 2023, 59(12): 1633-1643.
[5] LI Sai, YANG Zenan, ZHANG Chi, YANG Zhigang. Phase Field Study of the Diffusional Paths in Pearlite-Austenite Transformation[J]. 金属学报, 2023, 59(10): 1376-1388.
[6] LI Xiaobing, QIAN Kun, SHU Lei, ZHANG Mengshu, ZHANG Jinhu, CHEN Bo, LIU Kui. Effect of W Content on the Phase Transformation Behavior in Ti-42Al-5Mn- xW Alloy[J]. 金属学报, 2023, 59(10): 1401-1410.
[7] CHEN Yuyong, YE Yuan, SUN Jianfei. Present Status for Rolling TiAl Alloy Sheet[J]. 金属学报, 2022, 58(8): 965-978.
[8] LI Xueda, LI Chunyu, CAO Ning, LIN Xueqiang, SUN Jianbo. Crystallography of Reverted Austenite in the Intercritically Reheated Coarse-Grained Heat-Affected Zone of High Strength Pipeline Steel[J]. 金属学报, 2021, 57(8): 967-976.
[9] FENG Miaomiao, ZHANG Hongwei, SHAO Jingxia, LI Tie, LEI Hong, WANG Qiang. Prediction of Macrosegregation of Fe-C Peritectic Alloy Ingot Through Coupling with Thermodynamic Phase Transformation Path[J]. 金属学报, 2021, 57(8): 1057-1072.
[10] LIU Chenxi, MAO Chunliang, CUI Lei, ZHOU Xiaosheng, YU Liming, LIU Yongchang. Recent Progress in Microstructural Control and Solid-State Welding of Reduced Activation Ferritic/Martensitic Steels[J]. 金属学报, 2021, 57(11): 1521-1538.
[11] LI Jinshan, TANG Bin, FAN Jiangkun, WANG Chuanyun, HUA Ke, ZHANG Mengqi, DAI Jinhua, KOU Hongchao. Deformation Mechanism and Microstructure Control of High Strength Metastable β Titanium Alloy[J]. 金属学报, 2021, 57(11): 1438-1454.
[12] CHEN Xiang,CHEN Wei,ZHAO Yang,LU Sheng,JIN Xiaoqing,PENG Xianghe. Assembly Performance Simulation of NiTiNb Shape Memory Alloy Pipe Joint Considering Coupling Effect of Phase Transformation and Plastic Deformation[J]. 金属学报, 2020, 56(3): 361-373.
[13] ZHU Weiqiang, YU Muzhi, TANG Xu, CHEN Xiaoyang, XU Zhengbing, ZENG Jianmin. Effect of Er and Si on Thermal Conductivity and Latent Heat of Phase Transformation of Aluminum-Based Alloy[J]. 金属学报, 2020, 56(11): 1485-1494.
[14] SHI Zhangzhi, ZHANG Min, HUANG Xuefei, LIU Xuefeng, ZHANG Wenzheng. Research Progress in Age-Hardenable Mg-Sn Based Alloys[J]. 金属学报, 2019, 55(10): 1231-1242.
[15] Zhirong HE, Peize WU, Kangkai LIU, Hui FENG, Yuqing DU, Rongyao JI. Microstructure, Phase Transformation and Shape Memory Behavior of Chilled Ti-47Ni Alloy Ribbons[J]. 金属学报, 2018, 54(8): 1157-1164.
No Suggested Reading articles found!