Shaoming QIANG,Laizhu JIANG,Jin LI,Tianwei LIU,Yanping WU,Yiming JIANG. EVALUATION OF INTERGRANULAR CORROSION SUSCEPTIBILITY OF 11Cr FERRITIC STAINLESS STEEL BY DL-EPR METHOD. Acta Metall Sin, 2015, 51(11): 1349-1355.
Ferritic stainless steel (FSS) containg (11%~13%)Cr with low C and N has excellent comprehensive performances and thus can be widely applied in extensive fields such as automobile exhaust systems, containers, buses and so on. Among them, 409L steel containing 11%Cr has been increasingly used in applications for tail pipes in the cold end parts of automobile exhaust systems because of its good corrosion resistance and moderate price. During the manufacture process for these tail pipes, improper heat treatments and welding operations cause the precipitation of some detrimental phases such as carbides, nitrides, which leads to a reduction on the resistance to intergranular corrosion (IGC) due to the presence of Cr-depleted zone in the grain boundaries. In this work, the precipitates in grain boundaries of 409L steel aged at 600 ℃ were investigated using TEM, EDS and SAED. The double loop-electrochemical potentiokinetic reactivation (DL-EPR) method was extended for evaluating the IGC susceptibility of 409L steel. The operating conditions of the DL-EPR test for 409L steel were optimized by investigating the influences of the main test parameters, such as scanning rate, solution composition, solution temperature. The experimental results showed that the IGC occurred in aged 409L steel due to the precipitation of M23C6 along grain boundaries. The optimized DL-EPR test could evaluate the IGC susceptibility of 409L steel quantitatively with high reproducibility. With the increase of aging time, much more M23C6 precipitated along grain boundaries, which resulted in 409L steel more susceptible to IGC.
Fund: Supported by National Natural Science Foundation of China (Nos.51131008 and 51134010), National Key Technology Support Program (No.2012BAE04B00) and Doctoral Fund of Ministry of Education of China (No.20120071110013)
Fig.1 Volume fraction of phases in 409L steel calculated by Thermo-Calc
Fig.2 TEM image of grain boundary in as-received 409L steel (a), bright-field (b) and dark-field (c) images of grain boundaries in 409L steel after aged at 600 ℃ for 4 h, EDS analysis (d) and SAED pattern (e) of carbides
Fig.3 Effects of KSCN concentration (c) on DL-EPR test for 409L steel in 0.5%H2SO4 solution with scanning rate 1.667 mV/s at 30 ℃ (Ra—intergranular corrosion sensitivity)
Fig.4 Effects of scanning rate on DL-EPR test for 409L steel in 0.5%H2SO4+0.002%KSCN solution at 30 ℃
Fig.5 Effects of solution temperatures on DL-EPR test for 409L steel in 0.5%H2SO4+0.002%KSCN solution with scanning rate 1.667 mV/s
Fig.6 DL-EPR curves at the optimal conditions for 409L steel aged at 600 ℃for different times (ESCE—potential)
Sample
Ia / (mAcm-2)
Ir / (mAcm-2)
Ra / %
As-received
28.40
0
0
Aged for 0.5 h
32.61
2.61
8.00
Aged for 4 h
32.40
6.29
19.41
Aged for 10 h
27.18
8.63
31.75
Table 1 DL-EPR results for 409L steel aged at 600 ℃ for different times at the optimal conditions
Fig.7 OM images of 409L steel after DL-EPR test at the optimal conditions
(a) as-received (b) aged at 600 ℃ for 0.5 h (c) aged at 600 ℃ for 4 h (d) aged at 600 ℃ for 10 h
[1]
Pardo A, Merion M C, Coy A E, Viejo F, Carboneras M, Arrabal R. Acta Mater, 2007; 55: 2239
[2]
Nichol T J, Davis J A. Intergranular Corros Stainless Alloy, 1978; 656: 179
[3]
Devine T M, Drummond B J. Corrosion, 1982; 38: 327
[4]
You X M, Jiang Z H, Li H B, Shen M H, Cao Y. Chin Metall, 2007; (11): 16 (游香米, 姜周华, 李花兵, 申明辉, 曹 阳. 中国冶金, 2007; (11): 16)
[5]
Gate J D, Jago R A. Mater Sci Technol, 1987; 3: 450
[6]
Fritz J D, Franson I A. Mater Perform, 1997; 36(8): 57
[7]
Lakshminarayanan A K, Balasubramanian V. Mater Des, 2010; 31: 4592
[8]
Kim J K, Lee B J, Lee B H, Kim Y H, Kim K Y. Scr Mater, 2009; 61: 1133
[9]
Kim J K, Kim Y H, Lee J S, Kim K Y. Corros Sci, 2010; 52: 1847
[10]
Warren D. Corrosion, 1959; 15(4): 63
[11]
Guarnieri G J, Miller J, Vawter F J. Trans ASM, 1950; 42: 981
[12]
Pohl M, Storz O, Glogowski T. Mater Charact, 2007; 58: 65
[13]
Tseng C C, Shen Y, Thompson S W, Mataya M C, Krauss G. Metall Mater Trans, 1994; 25A: 1147
[14]
Xiao J M. Metallography Issues of Stainless Steels. 2nd Ed., Beijing: Metallurgy Industry Press, 2006: 39; 166; 171 (肖纪美. 不锈钢的金属学问题. 第二版, 北京: 冶金工业出版社, 2006: 39; 166; 171)
[15]
Gui L F,Wu M D,Zhao Y. Handbook of Materials Testing for Mechanical Engineering. Shenyang: Liaoning Science and Technology Press, 2002: 158 (桂立丰,吴民达,赵 源. 机械工程材料测试手册. 沈阳: 辽宁科学技术出版社, 2002: 158)
[16]
Huey W R. Trans Am Soc Steel Treat, 1930; 18: 1126
[17]
Streicher M A. Corros Sci, 1969; 9: 53
[18]
Frangini S, Mignone A. Corrosion, 1992; 48: 75
[19]
Gong J, Jiang Y M, Deng B, Xu J L, Hu J P, Li J. Electrochim Acta, 2010; 55: 5077
[20]
Deng B, Jiang Y M, Xu J L, Sun T, Gao J, Zhang L H, Zhang W, Li J. Corros Sci, 2010; 52: 969
[21]
Gao J, Jiang Y M, Deng B, Zhang W, Zhong C, Li J. Corros Sci, 2009; 54: 5830
[22]
Zhong C, Liu F, Wu Y T, Le J J, Liu L, He M F, Zhu J C, Hu W B. J Alloys Compd, 2012; 520: 11
[23]
Le J J, Liu L, Liu F, Deng Y D, Zhong C, Hu W B. J Alloys Compd, 2014; 610: 173
[24]
Zhong C, He M F, Liu L, Wu Y T, Chen Y J, Deng Y D, Shen B, Hu W B. J Alloys Compd, 2010; 504: 377
[25]
Zhong C, He M F, Liu L, Chen Y J, Shen B, Wu Y T, Deng Y D, Hu W B. Surf Coat Technol, 2010; 205: 2412
[26]
Jin W S, Lang Y P, Rong F, Sun L J. J Chin Soc Corros Prot, 2007; 27: 54 (金维松, 郎宇平, 荣 凡, 孙力军. 中国腐蚀与防护学报, 2007; 27: 54)
[27]
Chen F C, Hu S L. Comput Appl Chem, 2001; 18: 433 (陈范才, 胡石林. 计算机与应用化学, 2001; 18: 433)
[28]
Clarke W L, Cowan R L, Wakler W L. Intergranular Corros Stainless Alloy, 1978; 656: 99
[29]
Cihal V. Corros Sci, 1980; 20: 737
[30]
Mignone A, Borello A, Barbera A L. Corrosion, 1982; 38: 390
[31]
Lee J B. Corrosion, 1986; 42: 106
[32]
Li S S. Corros Sci Technol Prot, 2000; 12: 288 (李神速. 腐蚀科学与防护技术, 2000; 12: 288)
[33]
Kim J K, Kim Y H, Uhm S H, Lee J S, Kim K Y. Corros Sci, 2009; 51: 2716
[34]
Amadou T, Braham C, Sidhom H. Metall Mater Trans, 2004; 35A: 3513
ZHANG Yun;LIU Yulin;ZHAO Hong'en;HU Zhuangqi Institute of Metal Research; Academia Sinica; Shenyang; ZHU Ziyong; WANG Zhengfu Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang. INTERGRANULAR AND EXFOLIATION CORROSION BEHAVIOUR OF 8090Al-Li ALLOY[J]. 金属学报, 1991, 27(4): 127-133.