| MICROSTRUCTURAL INSTABILITY OF ULTRAFINE--GRAINED COPPER UNDER ANNEALING AND HIGH--TEMPERATURE DEFORMING |
| JIANG Qingwei1; LIU Yin1; WANG Yao1; CHAO Yuesheng1; LI Xiaowu1;2 |
1) Institute of Materials Physics and Chemistry; College of Sciences; Northeastern University; Shenyang 110004
2) Key Laboratory for Anisotropy and Texture of Materials; Ministry of Education; Northeastern University; Shenyang 110004 |
|
Cite this article:
JIANG Qingwei LIU Yin WANG Yao CHAO Yuesheng LI Xiaowu . MICROSTRUCTURAL INSTABILITY OF ULTRAFINE--GRAINED COPPER UNDER ANNEALING AND HIGH--TEMPERATURE DEFORMING. Acta Metall Sin, 2009, 45(7): 873-879.
|
|
|
Abstract The thermal stability and hardness behavior of ultrafine--grained (UFG) copper produced by equal channel angular pressing (ECAP) under the condition of annealing were studied by differential scanning calorimeter (DSC) and micro--hardness tests, and the microstructural changes of this material under uniaxial compression or cyclic deformation at temperatures ranging from room temperature to 300 ℃ were examined by electron channeling contrast (ECC) technique in scanning electron microscopy (SEM) and by transmission electron microscopy (TEM). It was found that under annealing even at a certain temperature below recrystallization temperature, UFG copper would exhibit a structural evolution, i.e., recrystallization and grain coarsening, the process of which may happen gradually at a low developing rate, so that the DSC response curve as a functional of annealing time cannot detect such a process. The grain coarsening behavior of UFG copper under high--temperature compression is related to the strain rate, i.e., the higher the strain rate, more remarkable the localization of grain coarsening becomes; the lower the strain rate, many more grains become coarsened integrally. Comparatively speaking, the grain coarsening induced by high--temperature cyclic deformation takes place more notably and uniformly, and some typical dislocation arrangements, like dislocation walls and dislocation cells etc., can be observed in some coarsened grains. Also, the inhomogeneity of grain coarsening under high--temperature deformation was quantitatively discussed in terms of a ratio V of maximum grain size (Dmax) to average grain size (Daver), which is available for the coarsened grains.
|
|
Received: 24 September 2009
|
|
|
| Fund: Supported by National Natural Science Foundation of China (No.50671023) and the Program for New Century Excellent Talents in University, Ministry of Education (No.NCET--07--0162) |
| [1] Segal V M. Mater Sci Eng, 1995; A197: 157
[2] Iwahashi Y, Horita Z, Nemoto M, Langdon T G. Acta Mater, 1998; 46: 3317
[3] Valiev R Z, Islamgaliev R K, Alexandrov I V. Prog Mater Sci, 2000; 45: 103
[4] Vinogradov A, Kaneko Y, Kitagawa K, Hashimato S, Stolyarov Y, Valiev R. Scr Mater, 1997; 36: 1345
[5] Agnew S R, Weertman J R. Mater Sci Eng, 1998; A244: 145
[6] Wu S D, Wang Z G, Jiang C B, Li G Y. Philos Mag Lett, 2002; 82: 559
[7] Wu S D,Wang Z G, Jiang C B, Li G Y, Alexandrov I V, Valiev R Z. Scr Mater, 2003; 48: 1605
[8] Vinogradov A Y, Stolyarov V V, Hashimoto S, Valiev R Z. Mater Sci Eng, 2001; A318: 163
[9] Mughrabi H, H¨oppel H W, Kautz M. Scr Mater, 2004; 51: 807
[10] Molodova X, Gottstein G, Winning M, Hellmig R J. Mater Sci Eng, 2007; A460–461: 204
[11] Li X W, Umakoshi Y, Wu S D, Wang Z G, Alexandrov I V, Valiev R Z. Phys Stat Sol, 2004; A201: 119
[12] Li X W, Wu S D, Wu Y, Yasuda H Y, Umakoushi Y. Adv Eng Mater, 2005; 7: 829
[13] Furukawa M, Iwahashi Y, Hotita Z, Nemoto M, Langdon T G. Mater Sci Eng, 1998; A257: 328
[14] Amouyal Y, Divinski S, Klinger L, Rabkin E. Acta Mater, 2008; 56: 5500
[15] Li X W, Zhang Z F, Wang Z G, Li S X, Umakoshi Y. Defect Diffus Forum, 2001; 188–190: 153
[16] Mughrabi H, Wang R. In: Hansen N, Horsewell A, Leffers T, Lilholt H eds., Proc 2nd Risφ Int Symp on Metallurgy and Materials Science, Roskilde: Risφ National Laboratory, 1981: 87
[17] Zhang J S. High–Temperature Deformation and Fracture of Materials. Beijing: Science Press, 2007: 29
(张俊善著. 材料的高温变形与断裂. 北京: 科学出版社, 2007: 29) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|